PROCESS FOR THE PREPARATION OF CATALYST COMPONENTS FOR THE POLYMERIZATION OF OLEFINS

    公开(公告)号:US20200231716A1

    公开(公告)日:2020-07-23

    申请号:US16647766

    申请日:2018-09-07

    Abstract: A process for the preparation of a solid catalyst component for the polymerization of CH2═CHR olefins, wherein R is hydrogen or hydrocarbyl radical with 1-12 carbon atoms, made from or containing a Ti compound on a Mg chloride based support, including the steps of (a) reacting a Mg based compound with a liquid medium made from or containing a Ti compound, at a temperature ranging from 0 to 150° C., thereby yielding solid particles; and (b) suspending the solid particles coming from step (a) in a liquid medium made from or containing hydrocarbons at a temperature ranging from 10 to 100° C., wherein step (a) or (b) is carried out in the presence of 0.2 to 20.0% by weight, with respect to the amount of Mg compound, of particles of a solid compound containing more than 50% by weight of SiO2 units and having average particle size from 1 to 100 μm.

    PROCESS FOR GAS-PHASE POLYMERIZATION OF OLEFINS

    公开(公告)号:US20200216588A1

    公开(公告)日:2020-07-09

    申请号:US16649044

    申请日:2018-09-13

    Abstract: A process for the polymerization of olefins in gas phase carried out in a reactor having two interconnected polymerization zones, a first zone (riser) and a second zone (downcomer), wherein growing polymer particles: a) flow through the riser under fast fluidization conditions established by feeding a mixture of gas and liquid; b) leave the riser and enter the downcomer, through which the growing polymer particles flow downward in a densified form; and c) leave the downcomer and are reintroduced into the riser, thereby establishing a circulation of polymer between the riser and the downcomer; the reactor is operated at a temperature between 0° C. and 5° C. above the dew point of the riser gas at the operating pressure, and in the riser, besides the growing polymer particles and gas flow, an amount of liquid is present.

    Film for stretch hood applications
    363.
    发明授权

    公开(公告)号:US10661540B2

    公开(公告)日:2020-05-26

    申请号:US16301799

    申请日:2017-05-09

    Abstract: The disclosure provides a multilayer blown film for stretch hood made from or containing a layer made from or containing a first polyolefin composition made from or containing from 20 wt % to 80 wt %, based upon the total weight of the first polyolefin composition, of Component A) and from 20 wt % to 80 wt %, based upon the total weight of the first polyolefin composition, of Component B); wherein Component A) is an ethylene copolymer and Component B) is a polyolefin composition made from or containing: (i) 5-35% by weight, based upon the total weight of Component B, of a propylene homopolymer or a propylene ethylene copolymer (ii) 20-50% by weight, based upon the total weight of Component B, of a copolymer of ethylene and a C3-C8 alpha-olefin; and (iii) 30-60% by weight, based upon the total weight of Component B, of a copolymer of ethylene and propylene.

    PROPYLENE BASED POLYMER COMPOSITION
    364.
    发明申请

    公开(公告)号:US20200087499A1

    公开(公告)日:2020-03-19

    申请号:US16610332

    申请日:2018-04-12

    Abstract: A propylene polymer composition made from or containing: a) from 35 wt % to 65 wt %, based upon the total weight of the propylene polymer composition, of a propylene 1-hexene copolymer containing from 10.2 to 13.0% by weight, based upon the weight of the propylene 1-hexene copolymer, of 1-hexene derived units and having a Melt Flow Rate (MFR, measured according to ASTM D 1238, 230° C./2.16 kg, (at 230° C., with a load of 2.16 kg)) from 3.5 to 12.0 g/10 min; b) from 35 wt % to 65 wt %, based upon the total weight of the propylene polymer composition, of a propylene ethylene copolymer containing from 1.5 wt % to 6.5 wt %, based upon the weight of the propylene ethylene copolymer, of ethylene derived units and having a Melt Flow Rate (MFR, measured according to ASTM D 1238, 230° C./2.16 kg, (at 230° C., with a load of 2.16 kg)) from 3.5 to 12.0 g/10 min.

    MASTERBATCH COMPOSITION
    366.
    发明申请

    公开(公告)号:US20200024434A1

    公开(公告)日:2020-01-23

    申请号:US16471986

    申请日:2017-12-18

    Abstract: A masterbatch composition made from or containing: 65 to 85 wt % of a propylene homopolymer or copolymer as component (1) containing 0 to 3 wt % of ethylene or one or more C4-C10-α-olefin-derived units; and 15 to 35 wt % of a propylene-ethylene copolymer as component (2) containing 25 to 35 wt % of ethylene-derived units, wherein the masterbatch composition has: 1) a melt flow rate (230° C., load: 21.18 N) of 5 to 30 g/10 minutes; 2) xylene insolubles with an Mw of 10×104 to 30×104 and an Mw/Mn of 6 to 20 as measured by GPC; and 3) xylene solubles with an intrinsic viscosity of 5.5 to 9.0 dl/g.

    BUTENE-1 POLYMER COMPOSITION HAVING A HIGH MELT FLOW RATE

    公开(公告)号:US20190322779A1

    公开(公告)日:2019-10-24

    申请号:US16312474

    申请日:2017-07-03

    Abstract: A butene-1 polymer composition having MFR values of from 400 to 2000 g/10 min, measured according to ISO 1133 at 190° C. with a load of 2.16 kg, made from or containing A) a butene-1 homopolymer or a copolymer of butene-1 with a comonomer selected from the group consisting of ethylene and higher alpha-olefins, having a copolymerized comonomer content of up to 5% by mole; B) a copolymer of butene-1 with a comonomer selected from the group consisting of ethylene and higher alpha-olefins, having a copolymerized comonomer content of from 6% to 20% by mole; wherein the composition having a total copolymerized comonomer content from 4% to 15% by mole, referred to the sum of A) and B), and a content of fraction soluble in xylene at 0° C. of 60% by weight or less, determined on the total weight of A) and B).