摘要:
The present invention provides a moulding composition, which includes: a plurality of bead polymers dispersed in at least one matrix polymer; wherein the bead polymers: have an average particle size of 5 to 40 &mgr;m, and have a refractive index nD at 20° C. which is different from a refractive index nD at 20° C. of said matrix polymer; and wherein the bead polymers are prepared by a process, which includes: contacting: at least one polymerizable mix which includes at least 50% by weight of at least one (meth)acrylate monomer, at least one aluminum compound, and an aqueous phase, to prepare a mixture; dispersing the mixture at a shear rate ≧103 s−1 to form a dispersion, wherein the dispersion is stabilized by the aluminum compound; and polymerizing to produce the bead polymers having an average particle size of 5 to 40 &mgr;m.
摘要翻译:本发明提供了一种模塑组合物,其包括:分散在至少一种基质聚合物中的多个珠粒聚合物;其中所述珠粒聚合物的平均粒度为5至40μm,并且在20℃具有折射率nD。 其与所述基质聚合物在20℃的折射率nD不同;并且其中所述珠粒聚合物通过一种方法制备,所述方法包括:使至少一种可聚合的混合物至少包含至少50重量% 一种(甲基)丙烯酸酯单体,至少一种铝化合物和水相,以制备混合物;将混合物在剪切速率> 10 3 s -1下分散以形成分散体,其中分散体稳定 由铝化合物; 并且聚合以产生平均粒径为5至40μm的珠粒聚合物。
摘要:
Injection molded parts having a scratch resistant surface are produced by applying a liquid mixture of at least one monomer susceptible of free radical polymerization and having more than one polymerizable double bond and of at least one free radical forming initiator to the forming surface of an injection mold, polymerizing the mixture at least partially, and then injecting a thermoplastic or duroplastic molding composition into the closed mold.
摘要:
The invention relates to a molding composition modified for impact resistance, in particular to impact-resistant PMMA with improved optical properties at elevated temperatures, to molded items obtainable therefrom, and also to the use of the molding composition and of the molded items.
摘要:
A molding compound comprises a copolymer (I)a), produced by polymerization of 90-100% by weight methylmethacrylate, styrene and malic acid anhydride, and optionally 0-10% by weight additional monomers which can be copolymerized with methylmethacrylate, a (co)polymer (II)b), produced by polymerization of 80-100% by weight methylmethacrylate and optionally 0-20% by weight additional monomers which can be copolymerized with methylmethacrylate, and has a solution viscosity in chloroform at 25° C. (ISO 1628 Part 6) of 50 to 55 ml/g, as well as c) optional conventional additives, auxiliary agents and/or fillers. The molding compound is characterized in that the copolymer (I) has a solution viscosity in chloroform at 25° C. (ISO 1628 Part) of 55 ml/g or less. Also disclosed are moldings produced by thermoplastic processing of the molding compound and their uses.
摘要:
The invention relates to a new adhesive composition and to sheets produced from it, for producing laminates, more particularly for bonding plastic with glass components, to a method for producing such laminates, and to the laminates produced accordingly.
摘要:
Provided is a molding composition comprising, based on the total weight of the composition, (A) 50.0% by weight to 99.5% by weight of at least one (co)polymer which is a homopolymer or copolymer of at least 80% by weight of methyl methacrylate, (B) 0.5% by weight to 50.0% by weight of at least one copolymer obtained by polymerization of a monomer, and (C) at least one low molecular weight (meth)acrylate (co)polymer having a solution viscosity in chloroform at 25° C. (ISO 1628—part 6) of less than or equal to 55 ml/g.
摘要:
A moulding compound comprises a copolymer (I)a), produced by polymerisation of 90-100% by weight methylmethacrylate, styrene and malic acid anhydride, and optionally 0-10% by weight additional monomers which can be copolymerised with methylmethacrylate, a (co)polymer (II)b), produced by polymerisation of 80-100% by weight methylmethacrylate and optionally 0-20% by weight additional monomers which can be copolymerised with methylmethacrylate, and has a solution viscosity in chloroform at 25° C. (ISO 1628 Part 6) of 50 to 55 ml/g, as well as c) optional conventional additives, auxiliary agents and/or fillers. The moulding compound is characterised in that the copolymer (I) has a solution viscosity in chloroform at 25° C. (ISO 1628 Part) of 55 ml/g or less. Also disclosed are mouldings produced by thermoplastic processing of the moulding compound and their uses.
摘要:
(EN) The invention concerns a method for producing a thermoplastic molding material or element, said material or element containing nanometric inorganic particles. In molten state, the thermoplastic is mixed with the nanometric inorganic particles and with a solubilizing agent in a conveyor screw extruder, the pressures and temperatures being adjusted so that the plastic is in melt form and the solubilizing agent in supercritical state. The invention is characterized in that at the output of the extruder, the mixture passes through a slot with a passage less than 20 $g(m)m to penetrate into an expansion zone and the molten material, wherein are incorporated the nanometric inorganic particles, is evacuated, reduced into molding material after cooling or transferred into a molding tool to be molded. The invention also concerns the molding material and the molding elements obtained by this method, as well as the uses thereof.
摘要:
The invention relates to an injection moulding method for the production of a complex, high optical quality light-diffusing moulded item. The moulding material used comprises a matrix made of polymethyl(meth)acrylate and spherical plastic particles whose particle size ranges from 1-24 μm and the concentration thereof ranges from 0.05-30 wt.-% in relation to the weight of the polymethyl(meth)acrylate. The spherical particles exhibit a refractive index differential in relation to the polymethyl(meth)acrylate matrix of 0.01 0.2.
摘要:
The present invention relates to a core-shell particle which has a core, a first shell and, where appropriate, a second shell, where: i) the core encompasses, based on its total weight, at least 75.0% by weight of (meth)acrylate repeat units; ii) the first shell has a glass transition temperature below 30° C.; iii) the second shell present where appropriate encompassed, based on its total weight, at lest 75.0% by weight of (meth)acrylate repeat units; iv) the first shell encompasses, based on its total weight, the following constituents; E) from 92.0 to 98.0% by weight of (meth)acrylate repeat units and F) from 2.0 to 8.0% by weight of styrenic repeat units of the general formula (I) where the radicals R1 to R6 are defined according to the Description and the percentages by weight of E) and F) give a total of 100.0% by weight, v) the radius of the core-shell particle inclusive of any second shell present, measured by the Coulter method, is in the range from above 160.0 to 240.0 nm. The present invention further relates to a process for preparing core-shell particles, to a moulding composition comprising core-shell particles, and to the use thereof.