摘要:
An information processing apparatus that determines a position of a touch input received at a display of the information processing apparatus, controls the display to display a string of candidate characters for input at a position on the display corresponding to the position of the touch input, detects selection of a desired character from the string of candidate characters, and controls the display to display the desired character in a character input field on the display.
摘要:
A process for producing a mixed powder for powder metallurgy in which graphite segregation can be prevented and which has satisfactory flowability and brings about satisfactory lubricating properties, the process comprising: selecting an organic binder which, when the solubility of an organic lubricant in a given organic solvent at a given temperature is taken as 1, has a solubility in the same solvent at the same temperature of 2 or higher; mixing the organic lubricant and the organic binder with the given organic solvent together with an iron powder to prepare an iron-powder slurry in which the organic lubricant and the organic binder have been dissolved in the organic solvent; and removing the organic solvent from the iron-powder slurry by vaporization to precipitate the organic lubricant and the organic binder in this order.
摘要:
A dielectric ceramic material is composed of a perovskite compound represented by ABO3 as a main component. In the case where ABO3 is, for example, BaTiO3, the crystal grains include BaTiO3 crystal grains composed of the main component and, as secondary phases, Mg—Ni—Ti-containing crystalline grains composed of a crystalline oxide containing at least Mg, Ni, and Ti and Ba—Si-containing crystalline grains composed of a crystalline oxide containing at least Ba and Si.
摘要:
In an information terminal 10 of the present invention, a read unit 34 reads image data to be displayed from a storage device (20, 50). A display 12 displays an image based on the read image data. An image transformation unit 44 applies image transformation to the displayed image. A background image acquisition unit 60 acquires the image data on the image transformed by the image transformation unit 44 and displayed on the display 12, as background image data to be pasted to the background of the display 12.
摘要:
A storage in a wireless communication terminal stores at least one data file. A data file selector selects a data file from among the data files stored in the storage, in accordance with an instruction from a user acknowledged in an acknowledging unit. A search unit searches for a wireless communication terminal originating a download request signal requesting a download of a data file. A transmission destination selector selects a transmission destination wireless communication terminal from among the wireless communication terminals identified through the search, in accordance with an instruction from a user acknowledged in the acknowledging unit. A transmitter transmits the selected data file to the transmission destination wireless communication terminal.
摘要:
A lubricant for powder metallurgy which includes a polyhydroxycarboxylic acid amide. The lubricant improves both flowability and lubricity, irrespective of a presence or absence of any complicated pretreatment step.
摘要:
A strength member, for vehicle use, extending in the vehicle width direction inside an instrument panel of a vehicle has a reinforcing bar in which a closed space is formed, and the reinforcing bar has a driver's seat side region, a central region and an assistant driver's seat side region, the reinforcing bar being composed of a metallic member arranged in the driver's seat side region and a resin member or a resin and metallic member arranged in the central region and the assistant driver's seat side region.
摘要:
A current/voltage non-linear resistor comprises a sintered body having a main component of ZnO, an electrode applied to a surface of the sintered body and an insulation material applied to another surface of the sintered body. The main component containing, as auxiliary components, Bi, Co, Mn, Sb, Ni and Al, and the contents of the auxiliary components are respectively expressed as Bi2O3, Co2O3, MnO, Sb2O3, NiO and Al3+, of Bi2O3: 0.3 to 2 mol %, Co2O3: 0.3 to 1.5 mol %, MnO: 0.4 to 6 mol %, Sb2O3: 0.8 to 7 mol %, NiO: 0.5 to 5 mol % and Al3+: 0.001 to 0.02 mol %; a Bi2O3 crystalline phase in the sintered body including an &agr;-Bi2O3 phase representing at least 80% of the total Bi2O3 phase.
摘要翻译:电流/电压非线性电阻器包括具有ZnO的主要成分的烧结体,施加到烧结体的表面的电极和施加到烧结体的另一个表面的绝缘材料。 作为辅助成分的Bi,Co,Mn,Sb,Ni和Al的主成分以及辅助成分的含量分别表示为Bi 2 O 3,Co 2 O 3,MnO,Sb 2 O 3,NiO和Al 3+,Bi 2 O 3 :0.3〜2摩尔%,Co 2 O 3:0.3〜1.5摩尔%,MnO:0.4〜6摩尔%,Sb2O3:0.8〜7摩尔%,NiO:0.5〜5摩尔%,Al 3+:0.001〜0.02摩尔% ; 所述烧结体中的Bi 2 O 3结晶相包括表示总Bi 2 O 3相的至少80%的α-Bi 2 O 3相。
摘要:
Alumina cement mortar is used as a source material for a kneaded cement cured body for joining hardware onto an insulator body, whereby the insulator can maintain high initial and long term mechanical strength and high electrical strength over a long period of time, and the curing time for forming the cured body is shortened to reduce the cost of producing the insulator. The alumina cement mortar is formed by kneading a mixture of alumina cement particles having a specific surface area of at least 3500 cm2/g, a polymer-steric-hindrance type water reducing agent, an aggregate, and water, or an alumina cement mortar is obtained by kneading a mixture of alumina cement particles having an amorphous phase on an outer peripheral surface of particles and having a specific surface area of at least 3500 cm2/g, a water reducing agent, an aggregate, and water.
摘要:
A nonlinear resistor is formed by forming side surface insulating layer 2 on a sintered body 1 which contains zinc oxide as a main component and providing a pair of electrodes 3 on upper and lower surfaces of the sintered body 1. The electrodes 3 are formed by plasma thermal spraying of less than 10 kW in an atmosphere in which an oxygen concentration is set to 22 volume % or less. The electrodes 3 are formed of aluminum, copper, zinc, nickel, silver, or their alloy whose average particle size is within 5 .mu.m to 50 .mu.m. Preferably porosity is less than 15%, weight percentage of metal oxide is less than 25%, average film thickness is within 5 .mu.m to 500 .mu.m, average surface roughness is less than 8 .mu.m, and resistivity is less than 15 .mu..OMEGA..multidot.cm. Accordingly, the nonlinear resistor having the excellent discharge withstand can be provided.