Abstract:
The present disclosure relates to a polypropylene composition for the production of molded articles, such as finished parts for the automotive industry, has melt flow rate (230° C., 2.16 kg) of at least 25 g/10 min and comprising: (A) 50-95% of a composition having an intrinsic viscosity of the fraction soluble in xylene at 25° C. of 3.0-5.0 dl/g; and (A1) 70-95% of a propylene homopolymer having a polydispersity index (PI) of 4.3-10, a fraction insoluble in xylene at 25° C. higher than 90% and an MFR (230° C., 2.16 kg) of 100-250 g/10 min; (A2) 5-30% of a copolymer of propylene with 36-44% of ethylene-derived units; (B) optionally up to 45% of a heterophasic propylene polymer, having an MFR (230° C., 2.16 kg) of 10-25 g/10 min, a flexural modulus higher than 1400 MPa, comprising 5-20% of a copolymer rubber component and 80-95% of a matrix propylene polymer component; (C) 2-10% of an ethylene based elastoplastic copolymer; and (D) optionally up to 20% of talc.
Abstract:
A copolymer of propylene with hexene-1 containing from 5 to 9% by weight of recurring units derived from hexene-1, having a melting temperature from 125 to 140 and Melt Flow Rate (ASTM D1238, 230/2.16 Kg) from 0.1 to 3 g/10 min., is used to produce blown films having valuable mechanical and optical properties.
Abstract:
A solid catalyst component for the (co)polymerization of olefins CH2═CHR, in which R is a hydrocarbyl radical with 1-12 carbon atoms, optionally in mixture with ethylene, comprising Ti, Mg, Cu, Cl, and an electron donor compound characterized by the fact that the Cu/Ti weight ratio is lower than 0.5.
Abstract:
A pre-polymerized catalyst component for the polymerization of olefins endowed with high activity and morphological stability comprises a non-stereospecific solid catalyst component containing Ti, Mg and a halogen, and an amount of an ethylene/alpha-olefin block (co)polymer ranging from 0.1 up to 5 g per g of said solid catalyst component, said prepolymerized catalyst component being characterized by a mercury porosity, due to pores having radius up to 1 μm, ranging from 0.15 to 0.5 cm3/g and by the fact that at least 55% of said porosity is due to pores having pore radius up to 0.2 μm.
Abstract:
The present invention relates to a new polypropylene composition for molded articles, such as finished parts for the automotive industry. A composition comprising: (A) from 40 to 85% by weight of a first propylene-based component being selected from propylene homopolymers, propylene copolymers and heterophasic propylene polymer, such first propylene-based component having a flexural modulus higher than 800 MPa; (B) from 5 to 20% by weight of a second propylene-based component being a heterophasic propylene polymer comprising: (B1) from 20 to 90% by weight of a crystalline polypropylene, and (B2) from 10 to 80% by weight of a copolymer of ethylene and at least one C3-C10 alpha-olefin, such copolymer containing from 10 to 70% by weight of ethylene, being soluble in xylene at room temperature, and having an intrinsic viscosity in tetrahydronaphtalene at 135° C. of higher than 3.5 dl/g; and (C) from 10 to 40% by weight of glass fibers.
Abstract:
A polyolefin composition comprising: A) from 65 wt % to 85 wt %, of a propylene/ethylene/1-butene terpolymer wherein: i) the content of ethylene derived units ranges from 0.6 wt % to 2.5 wt; ii) the content of 1-butene derived units ranges from 6 wt % to 12 wt %; iii) the fraction soluble in xylene at 25° C. ranges from 3.5 wt % to 20 wt %; B) from 15 wt % to 35 wt % of a propylene/ethylene copolymer having a content of ethylene derived units ranging from 10 wt % to 40 wt %; the copolymer optionally can contains 1-butene derived units in an amount less than 1 wt %; the sum A)+B) being 100.
Abstract:
A masterbatch composition comprising: 70-90% wt of a component (A) being a propylene homopolymer or copolymer of propylene with ethylene or C4-C10 alpha olefins, having a MFRA according to ISO 1133 (230° C./2.16 Kg) ranging from 15 to 70 g/10 min; and 10-30% wt of a component B) being a propylene-ethylene copolymer comprising 25-45% wt of ethylene derived units and having a value of the intrinsic viscosity [η] of the fraction soluble in xylene at room temperature ranging from 5 to 9 dl/g, said masterbatch composition having a total MFR higher than 4 g/10 min, and a value of the flexural modulus measured according to ISO method 178 ranging from 950 to 2000 MPa.
Abstract:
The present technology relates to films or sheets comprising a layer of a heterophasic propylene copolymer containing up to 7.0% by weight of ethylene-derived units and comprising: (a) 80%-92% by weight of a matrix phase comprising a propylene homopolymer or a propylene copolymer containing up to 5% by weight of units derived from ethylene and/or an alpha-olefin; and (b) 8%-20% by weight of a rubber phase comprising an ethylene-propylene copolymer containing 20%-60% by weight of ethylene-derived units.
Abstract:
The present technology relates to articles for use in healthcare or medical applications, such as blow-fill-seal applications, made of a propylene-ethylene random copolymer that demonstrate good optical properties after heat sterilization.
Abstract:
Multilayer film (BOPP) structure comprising at least: A) a skin (outer) layer substantially consisting of a crystalline low seal Initiation temperature propylene copolymer; B) a tie layer substantially consisting of a butene-1 copolymer having flexural modulus (MEF) of 75 MPa or less; C) a core layer substantially consisting of one or more polypropylene homopolymers designed for BOPP.