摘要:
Impact-resistant thermoplastic polyester molding materials are prepared by thoroughly mixingA. from 52 to 99 parts by weight of a melt of one or more polyalkylene terephthalates withB. from 1 to 48 parts by weight of one or more elastomeric graft polymers prepared by emulsion polymerization and composed of1. from 70 to 90% by weight of a grafting base consisting of elastomeric polymers having a gel content of not less than 80% and a glass transition temperature Tg of less than -20.degree. C. and2. from 10 to 30% by weight of a grafted shell consisting of one or more polymers having a glass transition temperature Tg greater than 40.degree. C.,in the form of an aqueous dispersion in which not less than 80% of the particles of graft polymer B have a size of from 0.05 to 0.15 .mu.m, with simultaneous removal of the water which vaporizes.
摘要:
A curable epoxy resin mixture containing an adduct of an epoxy resin with a bifunctional phenol or a bifunctional aromatic carboxylic acid of the formula ##STR1## where A=SO.sub.2 or CO, Ar is ##STR2## and X is OH or COOH, and an aromatic amine as a curing agent.
摘要翻译:一种可固化的环氧树脂混合物,其包含环氧树脂与双官能酚或式(II)的双官能芳族羧酸的加合物,其中A = SO 2或CO,Ar为X,并且X为OH或COOH,芳族 胺作为固化剂。
摘要:
Thermoplastic molding materials containing a mixture ofA. a heat-stable polymer, e.g. a polyether sulfone or polysulfone, which does not contain any reactive groups, andB. a heat-stable polymer which contains reactive groups, preferably nitrile or thioaryl groups and/or sulfur bridges,can be processed to moldings, which can be crosslinked, for example by being heated at above 200.degree. C., so that the plastic matrix becomes virtually insoluble.
摘要:
A platinum alloy catalyst on an electrically conductive carbon support which contains an alloy of 40 to 60 atom-% of platinum, 10 to 20 atom-% of rhodium and 20 to 50 atom-% of iron in the form of finely divided alloy particles. The catalyst is characterised in that the average particle size of the alloy particles is less than 10 nm.
摘要:
High molecular weight polyaryletherketones are prepared by nucleophilic polycondensation of a bisphenol with a mixture of a difluoroaromatic and a dichloroaromatic by a process in which, in a first stage, the total amount of bisphenol and dichloroaromatic is added and, in a second stage, the difluoroaromatic is added. The resulting polyaryletherketones have a reduced viscosity of not less than 0.65 and contain from 0.003 to 0.03% by weight of organically bonded chlorine and from 0.003 to 0.03% by weight of organically bonded fluorine.
摘要:
A polymeric molding composition contains(a) 20-70% by weight of a thermotropic, liquid-crystalline polymer(b) 10-50% by weight of a polycarbonate(c) 10-50% by weight of a polyester, the weight percentages (a), (b) and (c) adding up to 100, and(d) up to 60% by weight, based on the total amount of proportions (a), (b) and (c), of further polymers, fillers, reinforcing agents, processing aids or other additives, and is used for producing moldings, fibers, films or coatings.
摘要:
Thermoplastic polyester molding materials having low-temperature impact strength essentially consist of(A) from 20 to 79 parts by weight of one or more aliphatic polyesters of an aromatic dicarboxylic acid having a relative viscosity of from 1.2 to 1.8,(B) from 20 to 79 parts by weight of one or more aromatic polycarbonates having a relative viscosity of from 1.2 to 1.5,(C) from 1 to 40 parts by weight of an elastomer blend consisting of1. from 5 to 95% by weight of an ethylene copolymer composed of(a) from 40 to 99% by weight of ethylene and(b) from 1 to 60% by weight of one or more comonomers containing carboxyl groups and/or derivatives of carboxyl groups, and2. from 5 to 95% by weight of an elastomeric graft polymer which is prepared by emulsion polymerization and composed of(a) from 70 to 95% by weight of a substantially crosslinked grafting base having a glass transition temperature T.sub.g below -20.degree. C. and(b) from 5 to 30% by weight of a graft shell consisting of one or more polymers having a glass transition temperature T.sub.g higher than 20.degree. C., the amounts of components (A) to (C) summing to 100 parts by weight, and the amounts of components (1a) and (1b) and (2a) and (b) each summing to 100% by weight, and(D) if required, conventional additives in effective amounts.
摘要:
Impact-resistant thermoplastic molding compositions having a hard component comprising a styrene/acrylonitrile copolymer and a soft component comprising a graft copolymer of styrene and acrylonitrile on a rubbery polymer containing butadiene. The rubbery polymer serving as base for the graft copolymer is produced by polymerization or the monomer of monomers forming said polymer in aqueous emulsion and in the presence of a small amount of an alkanol of from 1 to 4 carbon atoms. The compositions have improved color and color stability and may be processed by conventional methods to form shaped articles.
摘要:
Disclosed herein is a system comprising an air reactor; where the air reactor is operative to oxidize metal oxide particles with oxygen from air to form oxidized metal oxide particles; a fuel reactor; where the fuel reactor is operative to release the oxygen from the oxidized metal oxide particles and to react this oxygen with fuel and steam to form syngas; a water gas shift reactor located downstream of the fuel reactor; where the water gas shift reactor is operative to convert syngas to a mixture of carbon and hydrogen; a combustor; and a gas turbine; the combustor being operative to combust the hydrogen and discharge flue gases derived from the combustion of hydrogen to drive the turbine; where the exhaust from the turbine is carbon free.
摘要:
A catalyst for use in a fuel cell containing a platinum-aluminum alloy on a conductive carbon carrier, wherein the atomic ratio of platinum to aluminum is from 80:20 to 60:40 and the alloy is present on the carbon carrier in carbidized form with the structure of platinum-aluminum carbide Pt.sub.3 AlC.sub.0.5. Also disclosed are multimetallic alloy catalysts for use as electrode catalysts in fuel cells. Catalysts with high activity and stability are obtained on the basis of carbidized platinum-aluminum alloy catalysts by adding alloying elements of the groups VIB, VIIB, VIII and IB of the Periodic Table of Elements.