METHOD FOR MAKING A FILM COMPRISING MFC
    46.
    发明申请

    公开(公告)号:US20190276621A1

    公开(公告)日:2019-09-12

    申请号:US16461897

    申请日:2017-11-16

    Applicant: Stora Enso OYJ

    Abstract: Method for making a film that comprises microfibrillated cellulose, wherein the film has low OTR values and especially suitable for a tropical environment. The method comprising the steps of providing a suspension comprising microfibrillated cellulose (MFC), forming a film from said suspension, wherein the film having a solid content above 40%, preferably above 50%, treating the film with flame or plasma treatment, such that a surface activation takes place on the film, and cooling the film, wherein the surface of the film having a decreased OTR value and a high moisture resistance.

    Method of manufacturing a film having low oxygen transmission rate values

    公开(公告)号:US11555275B2

    公开(公告)日:2023-01-17

    申请号:US16614164

    申请日:2018-05-17

    Applicant: Stora Enso OYJ

    Abstract: A method of manufacturing a film having an oxygen transmission rate (OTR) value in the range of 0.1 to 200 cc/m2*24 h at 23° C., 50% relative humidity (RH), and an OTR value in the range of 0.1 to 2000 cc/m2*24 h at 38° C. at 85% RH, comprising at least 60% by weight nanocellulose based on the weight of the total amount of fibers in the film, wherein the method comprises the steps of, providing an aqueous suspension comprising said nanocellulose; forming a web from said aqueous suspension; calendering said web at a line load of at least 40 kN/m, and at a temperature of at least 60° C. wherein said film is formed and said web has an OTR value in the range of 50 to 10 000 cc/m2*24 h at 23° C., 50% RH before said calendering step, or more preferably in the range of 500 to 5000 cc/m2*24 h at 23° C., 50% RH before said calendering step.

Patent Agency Ranking