-
公开(公告)号:US10967621B2
公开(公告)日:2021-04-06
申请号:US14644062
申请日:2015-03-10
Applicant: COI CERAMICS, INC.
Inventor: James A. Riedell
IPC: B32B37/00 , B32B37/18 , B32B38/18 , B32B18/00 , B32B3/20 , B32B3/10 , C04B35/64 , C04B35/634 , C04B35/645 , C04B37/00 , F16J15/00 , F16J15/10
Abstract: Methods of forming ceramic matrix composite structures include joining at least two lamina together to form a flexible ceramic matrix composite structure. Ceramic matrix composite structures include at least one region of reduced inter-laminar bonding at a selected location between lamina thereof. Thermal protection systems include at least one seal comprising a ceramic matrix composite material and have at least one region of reduced inter-laminar bonding at a selected location between lamina used to form the seal. Methods of forming thermal protection systems include providing one or more such seals between adjacent panels of a thermal protection system.
-
公开(公告)号:US20210061717A1
公开(公告)日:2021-03-04
申请号:US17010486
申请日:2020-09-02
Applicant: TOSOH CORPORATION
Inventor: Takeshi ITO , Yuji MATSUMURA , Isao YAMASHITA
Abstract: A zirconia sintered body that includes a transparent zirconia portion and an opaque zirconia portion has a biaxial bending strength of 300 MPa or more. In addition, the opaque zirconia portion is configured by an opaque zirconia sintered body that is any one of a dark-colored zirconia sintered body, a medium-light-colored zirconia sintered body, and a light-colored zirconia sintered body.
-
43.
公开(公告)号:US10920318B2
公开(公告)日:2021-02-16
申请号:US15771525
申请日:2016-10-27
Applicant: KYOCERA CORPORATION
Inventor: Yukio Noguchi , Yuuji Kawase , Hiromasa Matsufuji , Kouji Teramoto
IPC: C23C16/455 , C04B37/00 , C04B35/626 , B28B11/12 , C04B35/111 , B28B11/24 , C04B35/117 , C04B35/64 , H01L21/67
Abstract: A shower plate according to the present disclosure includes a ceramic sintered body, the ceramic sintered body comprising a first surface, a second surface facing the first surface, and a through hole positioned between the first surface and the second surface. An inner surface of the through hole includes a protruding crystal grain which protrudes more than an exposed part of a grain boundary phase existing between crystal grains. In addition, a semiconductor manufacturing apparatus according to the present disclosure includes the shower plate mentioned above.
-
44.
公开(公告)号:US20210031404A1
公开(公告)日:2021-02-04
申请号:US16897486
申请日:2020-06-10
Applicant: General Electric Company
Inventor: Xi Yang , Brian Peterson
IPC: B28B1/00 , B28B1/14 , B28B11/24 , B28B23/02 , F01D5/18 , C04B37/02 , B28B7/34 , C04B37/00 , B32B18/00 , C04B35/14 , C04B35/111 , C04B35/505 , C04B35/48 , C04B35/622
Abstract: This invention relates to a product and a method of preparing ceramic and/or ceramic hybrid materials through the construction of a printed die. The printed die being made by three dimensional printing or additive manufacturing processes possesses both an external geometry and an internal geometry.
-
公开(公告)号:US10906203B2
公开(公告)日:2021-02-02
申请号:US15651839
申请日:2017-07-17
Inventor: Jung-Kun Lee , Ian Nettleship , Ryan W. Read
IPC: B28B1/00 , C04B35/56 , C04B35/565 , C04B37/00 , C04B35/64 , C04B35/571 , B33Y70/00 , B33Y10/00 , C04B35/632
Abstract: A method for joining carbide ceramic particles, comprising: forming a first mixture comprising carbide ceramic particles, preceramic polymer liquid, fine carbon particles and metal nanoparticles that form a eutectic liquid at temperatures below 1400° C.; and heating the first mixture at a temperature of about 1150° C. to about 1400° C.
-
公开(公告)号:US20210009476A1
公开(公告)日:2021-01-14
申请号:US17042998
申请日:2019-03-13
Applicant: GOO CHEMICAL CO., LTD.
Inventor: Yutaka KAWAI
IPC: C04B35/626 , C04B35/26 , C04B35/634 , C04B35/64 , C04B37/00 , H01G4/30
Abstract: A baking slurry composition of the present invention contains an amino alcohol compound represented by formula, inorganic powder , a polyvinyl alcohol resin, and water. In the formula, R is a hydrogen atom or an alkyl group having a carbon number larger than or equal to 1 and smaller than or equal to 20, and m and n being values satisfying conditions m≥0, n≥0, and m+n≥1.
-
47.
公开(公告)号:US10863587B2
公开(公告)日:2020-12-08
申请号:US15425098
申请日:2017-02-06
Applicant: NGK INSULATORS, LTD.
Inventor: Kyohei Atsuji , Noboru Nishimura , Yuji Katsuda
IPC: H05B3/28 , C04B37/00 , C04B35/645 , C04B35/581 , H05B3/26 , H01L21/67 , H05B3/14 , C04B37/02 , H05B1/02 , H05B3/12
Abstract: A ceramic structure 10 includes a heater electrode 14 within a disk-shaped AlN ceramic substrate 12. The heater electrode 14 contains a metal filler in the main component WC. The metal filler (such as Ru or RuAl) has a lower resistivity and a higher thermal expansion coefficient than AlN. An absolute value of a difference |ΔCTE| between a thermal expansion coefficient of the AlN ceramic substrate 12 and a thermal expansion coefficient of the heater electrode 14 at a temperature in the range of 40° C. to 1000° C. is 0.35 ppm/° C. or less.
-
48.
公开(公告)号:US10814435B2
公开(公告)日:2020-10-27
申请号:US15039996
申请日:2014-11-28
Applicant: DIAMONDE
Inventor: Timothée Grunder , Anne Piquerez
IPC: B32B9/00 , B23C5/18 , B23C5/20 , B23D61/04 , B23K1/00 , B23P15/28 , B32B15/04 , B23K31/02 , B23K35/30 , B23D61/02 , C04B37/02 , B23K1/20 , B23K35/02 , B32B9/04 , B32B15/18 , C04B37/00 , B23K101/20 , B23K103/18 , B23K103/00 , B23K103/16
Abstract: The invention relates to an insert brazed on a body of cutting tools (101), consisting of: a metal substrate (11), in the form of plates, having a surface for attachment to the tool body; a high-temperature, brazing, alloy layer (12); an intermediate layer; and a ceramic plate (14). The brazing alloy layer connects the metal substrate (11) of the ceramic plate (14) via the metal layer (13). A low-temperature brazing layer (1) connects the insert (1, 1′) to the body of the tool (101).
-
49.
公开(公告)号:US20200317586A1
公开(公告)日:2020-10-08
申请号:US16956335
申请日:2018-11-23
Applicant: TOKAI CARBON KOREA CO., LTD
Inventor: Chang Wook SEOL
Abstract: Described herein are a bonded ceramic having a channel through which a fluid can flow, and a method for manufacturing the same. The bonded ceramic includes: a first ceramic base material; and a second ceramic base material, wherein: the first ceramic base material and the second ceramic base material are bonded by adhesive layer-free bonding; a pattern is formed on either or both of the bonding surface of the first ceramic base material where the first ceramic base material comes in contact with the second ceramic base material and the bonding surface of the second ceramic base material where the second ceramic base material comes in contact with the first ceramic base material; and the bonded ceramic includes pores having a size of 0.01 μm to 50 μm and formed along the bonding surface between the first ceramic base material and the second ceramic base material.
-
公开(公告)号:US10774008B2
公开(公告)日:2020-09-15
申请号:US15710954
申请日:2017-09-21
Applicant: General Electric Company
Inventor: Suresh Subramanian , Mark Eugene Noe , James Dale Steibel , Jason David Shapiro , Brandon ALIanson Reynolds , Kurtis C. Montgomery , Jared Hogg Weaver , Daniel Gene Dunn
IPC: C04B37/00 , C04B35/80 , C04B35/657 , C04B35/628 , F02K9/97 , F01D11/08 , F01D25/00 , F01D5/28 , F23R3/00 , C04B35/573 , F01D9/04 , F02K1/82 , B32B18/00
Abstract: A ceramic matrix composite article includes a chemical vapor infiltration ceramic matrix composite base portion including ceramic fiber reinforcement material in a ceramic matrix material having between 0% and 5% free silicon. The ceramic matrix composite article further includes a melt infiltration ceramic matrix composite covering portion including a ceramic fiber reinforcement material in a ceramic matrix material having a greater percentage of free silicon than the chemical vapor infiltration ceramic matrix composite base portion.
-
-
-
-
-
-
-
-
-