Abstract:
A carbon material for producing endohedral metallofullerenes in a high yield is made of a mixture of a metal or metal compound with a carbonaceous material and is used in producing a endohedral metallofullerenes, wherein said carbon material contains a metal carbide and a bulk density of said carbon material is set to 1.80 g/cm3 or less.
Abstract translation:用于以高产率生产内嵌金属富勒烯的碳材料由金属或金属化合物与碳质材料的混合物制成,并用于生产内嵌金属富勒烯,其中所述碳材料包含金属碳化物和所述碳的堆积密度 材料设定为1.80g / cm 3以下。
Abstract:
A fluorine gas generator is provided with which the gases used and/or generated, in case of leakage thereof, can be prevented from mixing together as far as possible and, even in case of gas leakage into the outside of the generator system, the leakage gas can be treated safely and in which the maintenance, exchange and other operations are easy to carry out. The generator comprises a box-shaped body containing an electrolyzer for fluorine gas generation, and the box-shaped body is divided into two or more compartments, including a compartment containing the electrolyzer.
Abstract:
Realized are a carbon support for a fuel cell catalyst and a catalyst for a fuel cell which have excellent durability and excellent catalytic activity when a catalyst metal is supported. A carbon support according to an embodiment of the present invention has diffraction peaks of a (002) plane which are observed at least at 2θ=22.5° to 25°, 26°, and 26.5° in an X-ray diffraction spectrum with CuKα rays, has an intensity ratio I(P1)/I(P2) between a peak P1 at 2θ=26° and a peak P2 at 2θ=26.5° of not less than 1.4, and has a BET specific surface area of not less than 1000 m2/g.
Abstract:
Provided is a C/C composite having a long life in an environment including a heating process and a cooling process and having less adverse effects on surrounding facilities and the quality of treatment objects. A C/C composite in which, in measurement for open pores by mercury porosimetry, an open porosity for open pores with a radius of not less than 0.4 μm and less than 10 μm in the C/C composite is 2.0% or less.
Abstract:
In a method for manufacturing a reformed SiC wafer 41 (a surface treatment method for a SiC wafer) having its surface that is reformed by processing an untreated SiC wafer 40 before formation of an epitaxial layer 42, the method includes a surface reforming step as described below. That is, the untreated SiC wafer 40 includes BPDs as dislocations parallel to an inside of a (0001) face, and TEDs. Property of the surface of the untreated SiC wafer 40 is changed so as to have higher rate in which portions having BPDs on the surface of the untreated SiC wafer 40 propagate as TEDs at a time of forming the epitaxial layer 42.
Abstract:
In a method for manufacturing an SiC wafer, a work-affected layer removal step of removing a work-affected layer generated in a surface and inside of an SiC wafer is performed, so that the SiC wafer from which the work-affected layer is at least partially removed is manufactured. In the work-affected layer removal step, the SiC wafer having undergone a polishing step is etched with an etching amount of 10 μm or less by being heated under Si vapor pressure so that the work-affected layer is removed. In the polishing step, an oxidizer is used to produce a reaction product in the SiC wafer while abrasive grains are used to remove the reaction product. In the SiC wafer having undergone the polishing step, an internal stress caused by the work-affected layer is present at a location inner than the work-affected layer, and an internal stress of the SiC wafer is reduced by removing the work-affected layer in the work-affected layer removal step.
Abstract:
[Problem] A carrier for retaining anammox bacteria, an anammox bacteria-adhered particle, and a wastewater treatment apparatus are provided that can remarkably reduce the start-up period for obtaining a nitrogen removal speed of 1 kg-N/m3/day. [Solution] A carrier for retaining anammox bacteria includes carbon particles. The carbon particles are desirably graphite particles, particularly isotropic graphite particles. The carbon particles desirably have a zeta potential of −35 mV to 0 mV and an average particle size of 2 μm to 1000 μm.
Abstract:
A positive electrode for an air battery that can remarkably improve the battery performance is provided by uniformly dispersing fine Nb (Nb oxide) therein. An air battery using the positive electrode as well as a method of manufacturing the positive electrode is also provided.A positive electrode for an air battery includes an expanded graphite sheet containing expanded graphite and Nb dispersed within the sheet. It is desirable that the Nb be contained in a weight proportion of from 5 ppm to 50000 ppm with respect to the expanded graphite.
Abstract:
A carbonaceous material is fabricated by a mixture of carbon powder and a binder. 10% by weight or more and 60% by weight or less of metal powder to the fabricated carbonaceous material is mixed. The mixed carbonaceous material and metal powder are pressurized and formed. A brush base material is fabricated by burning of the pressurized and formed carbonaceous material and metal powder. The fabricated brush base material is impregnated with oil. An impregnation rate of the oil to the mixed carbonaceous material and metal powder may be 0.5% by weight or more, for example.