摘要:
Thermoplastic moulding compositions composed ofI) 99.8-95% by weight of(A) 0-100% by weight of one or more graft polymers comprise the monomers styrene, .alpha.-methyl styrene, methyl methacrylate or a mixture of 95-50% by weight of styrene, .alpha.-methyl styrene, ring substituted styrene, methyl methacrylate or mixtures thereof with 5-50% by weight of methacrylonitrile, acrylonitrile, maleric acid anhydride, N-substituted malerimides or mixtures thereof, grafted onto a rubber substrate, andB) 100 to 0%, by weight of one or more thermoplastic vinyl polymers, andII) 0.2 to 5% by weight of a polyalkylene ether modified by a radical former which can be compounds conventionally used as an initiator for radical polymerization such as peroxides.
摘要:
Thermoplastic moulding materials, of vinyl chloride polymers, which contain a polymer, prepared in the presence of mercaptans, from styrene, .alpha.-methylstyrene, vinyltoluene, acrylonitrile, methyl methacrylate or mixtures thereof and which possess improved processing properties.
摘要:
Sulphosuccinamide acids and their salts corresponding to the following general formula ##STR1## wherein X denotes the residue of a hydrophobic, optionally branched vinyloligomer having an average molecular weight M.sub.n of from 200-5,000, preferably from 300-3,000,of the groups denoted byR.sup.1 R.sup.2, one is hydrogen and the other is --SO.sub.3 M, andn represents a number with a value of from 1.4-3.0, preferably form 1.6-2.3. andM denotes hydrogen, an alkali metal, or an ammonium, C.sub.1 -C.sub.4 -alkyl-ammonium or C.sub.2 -C.sub.3 -hydroxy alkyl-ammonium group.
摘要:
The invention relates to flame-resistant mixtures of polycarbonates with graft polymers and copolymers which are characterized in that they contain modified polyalkylene ethers as antistatic agent.
摘要:
Thermoplastic moulding compounds containing(A) from 5-90 parts by weight of one or more thermoplastic polymers,(B) from 5-90 parts by weight of one or more graft polymers and(C) from 0.25-40 parts by weight of a blocked copolymer corresponding to the idealized formula (I)A - B - A; B - A - B or (A - B).sub.x (I) whereinA denotes the residue of a homopolymer, e.g. of styrene, andB denotes the residue of a homopolymer of a cyclic carbonate or lactone.
摘要:
The invention relates to thermoplastic molding compounds containing(1.) thermoplastic aromatic polycarbonates and/or thermoplastic aromatic polyesters,(2.) graft polymers and, optionally,(2.a) thermoplastic copolymers,which are characterized in that they additionally contain aliphatic polycarbonates having weight average molecular weights Mw (as measured by ultracentrifugation or light scattering) in the range from 15,000 to 500,000.
摘要:
The invention relates to thermoplastic particulate graft polymers of a rubber (AB), consisting of a core (A) of rubber-like polymer of olefinically unsaturated monomers having softening temperatures (glass temperatures) below 0.degree. C. and a shell (B) of organopolysiloxane, and a polymer (C) of at least one ethylenically unsaturated monomer grafted into the rubber (AB) and to their use, optionally in admixture with brittle thermoplastic vinyl resins, as thermoplastic molding compositions.
摘要:
Thermoplastic moulding compositions consisting ofI. 75 to 99.5% by weight of a polymer ofA. 0 to 95% by weight, 95% or less by weight; of a graft copolymer prepared by grafting polymerization ofA.1 5 to 95% by weight of a mixture ofA.1.1 50 to 95% by weight of styrene, .alpha.-methylstyrene, nuclear-substituted styrene, methyl methacrylate or mixtures thereof andA.1.2 50 to 5% by weight of (meth)acrylonitrile, methyl methacrylate, maleic anhydride, N-substituted maleimide or mixtures thereof onA.2 95 to 5% by weight of a rubber with a glass transition temperature Tg or
摘要:
Process for the polymerization of cyclic aliphatic carbonates in the presence of aprotic organic solvents with exclusion of atmospheric oxygen and atmospheric moisture, wherein organometallic compounds of elements of main group 1 of the periodic table are used as initiators, the monomer/solvent ratio is in the range from 1 part by weight to 50 parts by weight of monomer per 100 parts by weight of solvent and the polymerization temperature is between -100.degree. C. and +20.degree. C.