摘要:
A pad assembly for eyeglass frames, in which an insert with a mounting portion is molded-in into the nose pad, whereby the mounting opening of the mounting portion is located outside of the nose pad; a connecting area is provided at the pad arm end which includes one or several projections and is adapted to be inserted into the mounting opening. The mounting opening is dimensionally reduced by plastic deformation of the mounting portion to such an extent that with an inserted connecting area of the pad arm end, a form-locking connection will result between the mounting portion and the pad arm.
摘要:
Absorbing layers of a low-emissivity (low-E) coating are designed to cause the coating to have a reduced film side reflectance which is advantageous for aesthetic purposes. In certain embodiments, the absorbing layers are metallic or substantially metallic (e.g., NiCr or NiCrNx) and are positioned in order to reduce or prevent oxidation of the absorbing layers during optional heat treatment (e.g., thermal tempering, heat bending, and/or heat strengthening). Coated articles according to certain example embodiments of this invention may be used in the context of insulating glass (IG) window units, other types of windows, etc.
摘要:
Absorbing layers of a low-emissivity (low-E) coating are designed to cause the coating to have a reduced film side reflectance which is advantageous for aesthetic purposes. In certain embodiments, the absorbing layers are metallic or substantially metallic (e.g., NiCr or NiCrNx) and are each provided between first and second nitride layers (e.g., silicon nitride based layers) in order to reduce or prevent oxidation of the absorbing layers during optional heat treatment (e.g., thermal tempering, heat bending, and/or heat strengthening). Coated articles according to certain example embodiments of this invention may be used in the context of insulating glass (IG) window units, other types of windows, etc.
摘要:
Absorbing layers of a low-emissivity (low-E) coating are designed to cause the coating to have a reduced film side reflectance which is advantageous for aesthetic purposes. In certain embodiments, the absorbing layers are metallic or substantially metallic (e.g., NiCr or NiCrNx) and are positioned in order to reduce or prevent oxidation of the absorbing layers during optional heat treatment (e.g., thermal tempering, heat bending, and/or heat strengthening). Coated articles according to certain example embodiments of this invention may be used in the context of insulating glass (IG) window units, other types of windows, etc.
摘要:
Certain example embodiments relate to techniques for depositing transparent conductive oxide (TCO) coatings using dual C-MAG sputtering apparatuses. Certain example embodiments provide a closed-loop system with the following process conditions. About 90% of the oxygen gas provided to the apparatus is provided via a top gas inlet. Pressure within the apparatus is increased to about 10−3 to 10−2 mbar, e.g., by providing an inert gas flow of at least about 600 sccm in certain example embodiments. Tube rotation is reduced to less than about 5 RPM. The power provided to the apparatus is adjusted in dependence on the presence or absence of oxygen partial pressure oscillations. TCOs such as, for example, ITO, ZnAlOx, SnSbOx, may be deposited according to the techniques of certain example embodiments.
摘要:
A mirror (e.g., first surface mirror) is provided with a layer of or including chromium nitride (CrNx). In certain example embodiments, the CrNx layer may be the primary reflective layer of the mirror. Surprisingly and unexpectedly, it has been found the addition of nitrogen to the chromium to form CrNx reduces pinhole formations in the resulting layer. In certain example embodiments, the more nitrogen which is introduced into the layer, the smaller the number and/or size of pinholes in the Cr inclusive layer. In certain example embodiments, it has also been found that the addition of nitrogen to Cr may improve durability.
摘要:
A coated article is provided that may be heat treated in certain example embodiments. A coating of the coated article includes a zinc oxide inclusive layer located over and contacting a contact layer that is in contact with an infrared (IR) reflecting layer of a material such as silver. It has been found that the use of such a zinc oxide inclusive layer results in improved thermal stability upon heat treatment, increased visible transmission, and/or lower sheet resistance (Rs).
摘要:
A coated article is provided so as to include a solar control coating having an infrared (IR) reflecting layer sandwiched between at least a pair of dielectric layers. The IR reflecting layer may be of or include NbZrOx, NbZr, NiCr, NiCrNx, or the like in certain embodiments of this invention. In particular, a zirconium silicon oxynitride (e.g., ZrSiOxNy) inclusive layer is provided which unexpectedly improves blocking (reflecting and/or absorption) of UV radiation in a manner which does not significantly degrade other optical properties of a coated article. Moreover, the ZrSiOxNy also has been found to improve (lower) the ΔE* value upon heat treatment, thereby permitting a coated article when heat treated (HT) to more closely match its non-HT counterpart with respect to glass side reflective color after such HT.
摘要翻译:提供一种涂覆制品,以便包括具有夹在至少一对电介质层之间的红外线(IR)反射层的太阳能控制涂层。 在本发明的某些实施方案中,IR反射层可以是或包括NbZrO x X,NbZr,NiCr,NiCrN x x等。 特别地,提供了一种包括锆的氮氧化锆(例如,ZrSiO x N N y)(包括层),其意外地改善了UV辐射的阻挡(反射和/或吸收) 这不会显着降低涂层制品的其它光学性能。 此外,也已经发现,ZrSiO x N N y Y在热处理时可以改善(降低)DeltaE *值,从而允许涂覆制品经热处理(HT)至 在这样的HT之后,其非HT对应物与玻璃侧反射颜色更紧密地匹配。
摘要:
A mirror (e.g., first surface mirror) is provided with a layer of or including chromium nitride (CrNx). In certain example embodiments, the CrNx layer may be the primary reflective layer of the mirror. Surprisingly and unexpectedly, it has been found the addition of nitrogen to the chromium to form CrNx reduces pinhole formations in the resulting layer. In certain example embodiments, the more nitrogen which is introduced into the layer, the smaller the number and/or size of pinholes in the Cr inclusive layer. In certain example embodiments, it has also been found that the addition of nitrogen to Cr may improve durability.
摘要翻译:反射镜(例如,第一表面反射镜)设置有氮化铬层或包含氮化铬(CrN)的层。 在某些示例性实施例中,CrN x层可以是反射镜的主要反射层。 令人惊奇和意外的是,已经发现向铬中添加氮以形成在所得层中的CrN x x缩小针孔形成。 在某些示例性实施例中,被引入层中的氮越多,包含Cr的层中的针孔的数量和/或尺寸越小。 在某些示例性实施方案中,还已经发现,向Cr中添加氮可以提高耐久性。
摘要:
A coated article is provided which may be heat treated (e.g., thermally tempered) in certain instances. In certain example embodiments, an interlayer of or including a metal oxide such as tin oxide is provided under an infrared (IR) reflecting layer so as to be located between respective layers comprising silicon nitride and zinc oxide. It has been found that the use of such a tin oxide inclusive interlayer results in significantly improved mechanical durability, thermal stability and/or haze characteristics.