Method for improving the internal surface of seamless tube of
multi-layer plastics film laminate
    81.
    发明授权
    Method for improving the internal surface of seamless tube of multi-layer plastics film laminate 失效
    改善多层塑料薄膜层压板无缝管内表面的方法

    公开(公告)号:US5296170A

    公开(公告)日:1994-03-22

    申请号:US543833

    申请日:1990-07-13

    摘要: A method for improving the internal surface of a gas-barrier, when required heat-shrinkable, multi-layer plastics film laminate in the form of a seamless tube having the innermost layer of olefin resin, the method including applying corona discharge employing at least two pairs of electrodes to the innermost layer from the outside of the tube having a gas sealed therein and pressed to a flat state avoiding the contact of opposed surface areas of innermost olefin resin layer with each other, the two pairs of electrodes being arranged such that one electrode of each pair is in contact with the outermost layer of the tube and the other of the same pair out of contact therewith while one electrode of one pair is kept in contact with the outermost layer of the tube with which one electrode of another pair is kept out of contact on the same side of the tube, so that the wetting tension of the innermost layer surface is increased to at least 35 dyne/cm by the corona discharge treatment.

    摘要翻译: PCT No.PCT / JP89 / 01170 Sec。 371日期1990年7月13日第 102(e)日1990年7月13日PCT 1989年11月16日PCT PCT。 公开号WO90 / 05757 日期:1990年5月31日。一种用于改进气体阻隔层的内表面的方法,当需要具有最内层烯烃树脂的无缝管形式的需要的热收缩性多层塑料膜层压体时, 电离放电采用至少两对电极从最外层的管子的外部密封在其中,并被压到平坦的状态,避免了最内层的烯烃树脂层相对的表面区域相互接触, 电极布置成使得每对的一个电极与管的最外层接触,并且相同对中的另一个与其不相接触,而一对的一个电极与管的最外层保持接触, 另一对的一个电极在管的同一侧保持脱离接触,使得最内层表面的润湿张力通过电晕放电增加到至少35达因/厘米 e治疗。

    Bearing component, rolling bearing, and method for producing bearing component
    83.
    发明授权
    Bearing component, rolling bearing, and method for producing bearing component 有权
    轴承部件,滚动轴承以及轴承部件的制造方法

    公开(公告)号:US08714831B2

    公开(公告)日:2014-05-06

    申请号:US13259680

    申请日:2010-03-17

    申请人: Nobuyuki Mori

    发明人: Nobuyuki Mori

    摘要: An outer ring, an inner ring and a roller serving as a bearing component that adopts as a source material a steel ensuring a large fracture toughness value and also having an alloy element added thereto in a reduced amount and also provides sufficient wear resistance, are configured of a steel containing 0.15-0.3% by mass of carbon, 0.15-0.7% by mass of silicon, and 0.15-1.0% by mass of manganese, with a remainder of iron and an impurity, and have a raceway/rolling contact surface included in a region having a carbon enriched layer and a nitrogen enriched layer. In the nitrogen enriched layer the raceway/rolling contact surface has a nitrogen concentration equal to or larger than 0.3% by mass.

    摘要翻译: 作为轴承部件的作为轴承部件的外圈,内圈和滚子,用于确保大的断裂韧性值的钢,并且还具有减少量并且还提供足够的耐磨性的合金元素, 含有0.15-0.3质量%的碳,0.15-0.7质量%的硅和0.15-1.0质量%的锰,剩余的铁和杂质含有轨道/滚动接触表面 在具有碳富集层和富氮层的区域中。 在富氮层中,滚道/滚动面的氮浓度等于或大于0.3质量%。

    Method of manufacturing a martensitic stainless steel pipe
    85.
    发明授权
    Method of manufacturing a martensitic stainless steel pipe 有权
    制造马氏体不锈钢管的方法

    公开(公告)号:US08366843B2

    公开(公告)日:2013-02-05

    申请号:US11727467

    申请日:2007-03-27

    申请人: Nobuyuki Mori

    发明人: Nobuyuki Mori

    IPC分类号: C21D9/08

    摘要: A method of manufacturing a 13Cr steel pipe which satisfies a hardness (HRC) of at most 22 with 13Cr grade L80 of American Petroleum Institute (API) standards, which is an indicator of a high strength, high yield ratio, and good corrosion resistance, is provided. A steel billet having a chemical composition comprising, in mass percent, C: 0.15-0.21%, Si: 0.16-1.0%, Mn: 0.35-1.0%, Cr: 10.5-14.0%, P: at most 0.020%, S: at most 0.0050%, Al: 0.025-0.050%, and a remainder of Fe and impurities is subjected to hot working with a finishing temperature of 800-960° C. to form a mother pipe, which is immediately quenched at a cooling rate of at least air cooling and then tempered by heating.

    摘要翻译: 13Cr钢管的制造方法,其是以美国石油学会(API)标准的13Cr级L80的硬度(HRC)为22以下,高强度,高屈服比,耐腐蚀性良好的指标, 被提供。 具有以质量%计含有C:0.15-0.21%,Si:0.16-1.0%,Mn:0.35-1.0%,Cr:10.5-14.0%,P:0.020%以下的化学组成的钢坯,S: 至多0.0050%,Al:0.025-0.050%,余下的Fe和杂质进行热加工,最终温度为800-960℃,形成母管,立即以冷却速度骤冷 至少空气冷却,然后通过加热回火。

    Image pickup apparatus, method and computer-readable storage medium for processing an image based on user manipulation on a display surface
    86.
    发明授权
    Image pickup apparatus, method and computer-readable storage medium for processing an image based on user manipulation on a display surface 有权
    用于基于显示表面上的用户操纵来处理图像的图像拾取装置,方法和计算机可读存储介质

    公开(公告)号:US08314844B2

    公开(公告)日:2012-11-20

    申请号:US12466069

    申请日:2009-05-14

    IPC分类号: H04N5/228

    摘要: Disclosed herein is an image pickup apparatus, including: an image pickup portion configured to capture an image; a detecting portion configured to detect a manipulation made on a display surface, for the image displayed on a display portion; and a grid and dust removing portion configured to carry out removal of grid and dust an image of which appears on the captured image by executing image processing based on a position about the manipulation detected by the detecting portion.

    摘要翻译: 本文公开了一种图像拾取装置,包括:被配置为捕获图像的图像拾取部分; 检测部,被配置为检测在显示部上显示的图像对显示面进行的操作; 以及网格除尘部,被配置为通过基于由所述检测部检测到的关于所述操作的位置执行图像处理,执行在所述拍摄图像上出现的图像的网格和灰尘的去除。

    MAGNESIUM ALLOY MEMBER AND METHOD FOR PRODUCING SAME
    87.
    发明申请
    MAGNESIUM ALLOY MEMBER AND METHOD FOR PRODUCING SAME 审中-公开
    镁合金构件及其制造方法

    公开(公告)号:US20110268986A1

    公开(公告)日:2011-11-03

    申请号:US13142360

    申请日:2009-11-17

    IPC分类号: B21D39/00 B23P11/00

    摘要: The method of producing a magnesium alloy joined part has the following steps: a joining step of joining a reinforcing material made of metal to a plate material made of magnesium alloy without allowing an organic material to remain at the joined portion and a plastic-working step of performing plastic working on the plate material to which the reinforcing material is joined. A desirable means of joining the reinforcing material to the plate material can be to use an inorganic adhesive. Because the magnesium alloy joined part is formed by a structure in which the reinforcing material is joined to the plate material, in comparison with the case where the reinforcing material is formed by machining or the like, the magnesium alloy structural member can be obtained with high production efficiency.

    摘要翻译: 镁合金接合部的制造方法具有以下步骤:将由金属制成的增强材料与镁合金制的板材接合而不使有机材料残留在接合部的接合工序和塑性加工工序 对加强材料接合的板材进行塑性加工。 将增强材料接合到板材的期望的方法可以是使用无机粘合剂。 由于镁合金接合部分是通过加强材料与板材接合的结构形成的,与通过机加工等形成增强材料的情况相比,可以获得高的镁合金结构件 生产效率。

    FORMED PRODUCT OF MAGNESIUM ALLOY AND MAGNESIUM ALLOY SHEET
    89.
    发明申请
    FORMED PRODUCT OF MAGNESIUM ALLOY AND MAGNESIUM ALLOY SHEET 审中-公开
    镁合金和镁合金板的成型产品

    公开(公告)号:US20110203706A1

    公开(公告)日:2011-08-25

    申请号:US13125023

    申请日:2009-09-29

    IPC分类号: C22C23/02

    CPC分类号: C22C23/02 C22F1/06

    摘要: A formed product of a magnesium alloy having excellent impact resistance and a magnesium alloy sheet suitable as a material for the formed product are provided. The formed product is produced by press-forming a magnesium alloy sheet having an Al content of 7% by mass to 12% by mass and has a flat portion that is not subjected to drawing deformation. In a metal texture in a cross section of the flat portion in the thickness direction, the number of coarse intermetallic compound (Mg17Al12) particles having a particle size of 5 μm or more present in a surface area region extending from a surface of the flat portion to a position one-third of the thickness from the surface in the thickness direction is five or less. The formed product has a texture in which the number of coarse precipitations d1 is small and in which fine precipitations d0 are dispersed. The formed product is less likely to be dented even when impacted because of dispersion strengthening owing to the fine precipitations and solid-solution strengthening owing to Al that sufficiently forms a solid solution.

    摘要翻译: 提供了具有优异抗冲击性的镁合金的成型产品和适合成型产品的材料的镁合金板。 形成的产品通过压制形成Al含量为7质量%至12质量%的镁合金板而制成,并具有不受拉伸变形的平坦部分。 在平坦部分的厚度方向的横截面中的金属结构中,存在于从平坦部分的表面延伸的表面区域中具有5μm以上的粒子的粗大的金属间化合物(Mg17Al12)颗粒的数量 到厚度方向上的表面厚度的三分之一的位置为五分之一以下。 形成的产品具有其中粗沉淀物d1的数量少并且其中分散有细小沉淀物d0的织构。 即使由于由于充分形成固溶体的Al的细小沉淀和固溶强化而引起的分散强化,即使被冲击也难以形成凹陷。

    MAGNESIUM ALLOY STRUCTURAL MEMBER
    90.
    发明申请
    MAGNESIUM ALLOY STRUCTURAL MEMBER 审中-公开
    镁合金结构件

    公开(公告)号:US20110097573A1

    公开(公告)日:2011-04-28

    申请号:US12527530

    申请日:2009-01-09

    IPC分类号: B32B15/04

    摘要: The invention offers a magnesium alloy structural member having a high metallic texture. The magnesium alloy structural member is provided with a base material made of magnesium alloy and a covering layer formed on the base material. The base material is provided, in at least one part of its surface, with a surface-processed portion that is subjected to a fine asperity-forming processing so as to obtain a metallic texture. The covering layer is transparent. The structural member can effectively increase the metallic texture by having the surface-processed portion. Because the structural member is provided with the covering layer, it has excellent corrosion resistance. Because the covering layer is transparent, the metallic texture in the surface-processed portion is readily sensed. The asperity-forming processing is performed through hairline finish, diamond cut finish, and the like.