摘要:
Embodiments of the present invention relate to article comprising 1) a functionalized component, 2) tackifier, and 3) an olefin polymer comprising one or more C3 to C40 olefins, optionally one or more diolefins, and less than 5 mole % of ethylene having a Dot T-Peel of 1 Newton or more, a branching index (g′) of 0.95 or less measured at the Mz of the polymer; and an Mw of 100,000 or less; where the functional component is selected from the group consisting of functionalized polymers, functionalized oligomers and beta nucleating agents; and where the Gardner color of the adhesive does not change by more than 7 Gardner units when the adhesive has been heat aged at 180° C. for 48 hours as compared to the Gardner color of the unaged composition.
摘要:
This invention relates to a propylene polymer comprising a component having a crystallinity of 10% or less and a component having a crystallinity of 20% or more, said propylene polymer having: a) a melting point of X ° C. or more where X=−0.0038(Tp)2+0.36(Tp)+150, where Tp is the temperature of polymerization in ° C.; b) an Mw of 10,000 g/mol or more; c) a heat of fusion of from 1-70 J/g; d) Stereodefects per 10,000 monomer units of Y or less where Y=2.35(Tp)−100 (where Tp is the temperature of polymerization in ° C.) for the portion of the blend that is insoluble in hexane at 23° C.; e) a dot T-Peel on Kraft paper of 1 N or more; and f) a branching factor of 0.98 or less, where the branching factor is the ratio of g′ measured at Mz to g′ measured at Mw, and process to produce such polymers.
摘要:
The present invention relates to a process for preparing a thermoplastic vulcanizate (TPV) comprising: contacting a thermoplastic polymer, a cross-linkable elastomer, at least one curative, and at least one cure activator in a solvent to form Composition A. The solvent is then removed, and thereafter the cross-linkable elastomer is at least partially cured. The average particle size of the cross-linkable elastomer is 10 microns or less after the solvent is removed.
摘要:
A heterogeneous polymer blend comprises a dispersed phase comprising a thermoplastic first polymer having a crystallinity of at least 30% and a continuous phase comprising a second polymer different from the first polymer. The second polymer has a crystallinity of less than 20% and is at least partially cross-linked.
摘要:
The present application relates to a new catalyst system for the polymerization of olefins, comprising a new ionic activator having the formula: [R1R2R3AH]+ [Y]−, wherein [Y]− is a non-coordinating anion (NCA), A is nitrogen or phosphorus, R1 and R2 are hydrocarbyl groups or heteroatom-containing hydrocarbyl groups and together form a first, 3- to 10-membered non-aromatic ring with A, wherein any number of adjacent ring members may optionally be members of at least one second, aromatic or aliphatic ring or aliphatic and/or aromatic ring system of two or more rings, wherein said at least one second ring or ring system is fused to said first ring, and wherein any atom of the first and/or at least one second ring or ring system is a carbon atom or a heteroatom and may be substituted independently by one or more substituents selected from the group consisting of a hydrogen atom, halogen atom, C1 to C10 alkyl, C5 to C15 aryl, C6 to C25 arylalkyl, and C6 to C25 alkylaryl, and R3 is a hydrogen atom or C1 to C10 alkyl, or R3 is a C1 to C10 alkylene group that connects to said first ring and/or to said at least one second ring or ring system. The present application also relates to a process for the polymerization of olefins, preferably propylene, using this and other catalyst systems, as well as to polymers made by said process.
摘要:
This invention relates to an isotactic propylene homopolymer having: more than 15 and less than 100 regio defects (sum of 2,1-erythro and 2,1-threo insertions and 3,1-isomerizations) per 10,000 propylene units; an Mw of 35000 g/mol or more; a peak melting temperature of greater than 149° C.; an mmmm pentad fraction of 0.85 or more; a heat of fusion of 80 J/g or more; and a peak melting temperature minus peak crystallization temperature (Tmp−Tcp) of less than or equal to (0.907 times Tmp) minus 99.64 (Tmp−Tcp
摘要:
Disclosed herein are adhesives comprising a copolymer comprising at least 80 wt % of units derived from propylene and from about 1 to about 20 wt % of units derived from at least one C6 to C10 alpha-olefin. The copolymer has a molecular weight of less than 100,000 and a heat of fusion between about 10 and about 70 J/g. An adhesive containing the copolymer preferably exhibits at least 50% fiber tear at −18° C. and at least 50% fiber tear at +25° C. using Inland paper board as a substrate; a viscosity of less than 50,000 mPa sec at 190° C., a set time of less than 4 seconds and a toughness of at least 3.4 megajoule/m3.
摘要:
This invention relates to a molded article comprising an in-reactor polymer blend comprising: (a) a first propylene polymer comprising 90 to 100 wt % propylene and from 0 to less than 10 wt % comonomer, said first propylene component having a Tm of 135° C. or more; and (b) a second propylene polymer comprising from 30 to 90 wt % propylene and 70 to 10 wt % comonomer, said second propylene polymer having an Mw of 30,000 g/mol or more, and said second propylene-containing polymer having a crystallinity different by at least 5% from the first polymer, wherein the polymer blend has: (a) a Tm of at least 135° C., (b) a melt flow rate of at least 70 dg/min, (c) a tensile strength of at least 8 MPa, (d) an elongation at break of at least 200%, (e) a tensile strength at break of 10 MPa or more, and (f) a GME 60280 scratch resistance of less than 1.2 DL at a scratching load of 5 Newtons.
摘要:
The present application relates to a new catalyst system for the polymerization of olefins, comprising a new ionic activator having the formula: [R1R2R3AH]+ [Y]−, wherein [Y]− is a non-coordinating anion (NCA), A is nitrogen or phosphorus, R1 and R2 are hydrocarbyl groups or heteroatom-containing hydrocarbyl groups and together form a first, 3- to 10-membered non-aromatic ring with A, wherein any number of adjacent ring members may optionally be members of at least one second, aromatic or aliphatic ring or aliphatic and/or aromatic ring system of two or more rings, wherein said at least one second ring or ring system is fused to said first ring, and wherein any atom of the first and/or at least one second ring or ring system is a carbon atom or a heteroatom and may be substituted independently by one or more substituents selected from the group consisting of a hydrogen atom, halogen atom, C1 to C10 alkyl, C5 to C15 aryl, C6 to C25 arylalkyl, and C6 to C25 alkylaryl, and R3 is a hydrogen atom or C1 to C10 alkyl, or R3 is a C1 to C10 alkylene group that connects to said first ring and/or to said at least one second ring or ring system. The present application also relates to a process for the polymerization of olefins, preferably propylene, using this and other catalyst systems, as well as to polymers made by said process.
摘要:
Disclosed herein is an in-reactor produced multi-component copolymer comprises a semi-crystalline component having a crystallinity of 20% or more, and an amorphous component having a crystallinity of 5% or less. The copolymer comprises at least 80 wt % of units derived from propylene and from about 1 to about 20 wt % of units derived from at least one C6 to C12 alpha-olefin. The copolymer has a viscosity at 190° C. of at least 530 mPa sec and a heat of fusion between about 10 and about 70 J/g. An adhesive containing the copolymer exhibits a good balance of adhesive properties and mechanical strength.