Poly aryl ether ketone polymer blends
    1.
    发明申请
    Poly aryl ether ketone polymer blends 有权
    聚芳基醚酮聚合物共混物

    公开(公告)号:US20070219324A1

    公开(公告)日:2007-09-20

    申请号:US11229455

    申请日:2005-09-16

    IPC分类号: C08L61/00

    摘要: Phase separated blends of polyaryl ether ketones, polyaryl ketones, polyether ketones, polyether ether ketones and mixtures thereof with at least one polysulfone etherimide, wherein the polysulfone etherimide has greater than or equal to 50 mole % of the polymer linkages contain at least one aryl sulfone group are described. Such blends have improved load bearing capability at high temperature. In another aspect a high crystallization temperature, especially at fast cooling rates, is achieved

    摘要翻译: 聚芳基醚酮,聚芳基酮,聚醚酮,聚醚醚酮及其与至少一种聚砜醚酰亚胺的混合物的相分离共混物,其中聚砜醚酰亚胺具有大于或等于50摩尔%的聚合物键含有至少一个芳基砜 组被描述。 这种混合物在高温下具有改善的承载能力。 在另一方面,实现了高结晶温度,特别是在快速冷却速率下

    POLY ARYL ETHER KETONE POLYMER BLENDS

    公开(公告)号:US20070197739A1

    公开(公告)日:2007-08-23

    申请号:US11687749

    申请日:2007-03-19

    IPC分类号: C08F20/00

    摘要: Filled phase-separated blends of polyaryl ether ketones, polyaryl ketones, polyether ketones, polyether ether ketones and mixtures thereof with at least one polysulfone etherimide, wherein the polysulfone etherimide has greater than or equal to 50 mole % of the polymer linkages contain at least one aryl sulfone group are described. Such filled blends have improved load-bearing capability at high temperature. In another aspect the filled blends have a higher crystallization temperature, especially at fast cooling rates.

    摘要翻译: 聚芳基醚酮,聚芳基酮,聚醚酮,聚醚醚酮及其与至少一种聚砜醚酰亚胺的混合物的填充相分离共混物,其中聚砜醚酰亚胺具有大于或等于50摩尔%的聚合物键含有至少一个 描述芳基砜基团。 这种填充的共混物在高温下具有改善的承载能力。 在另一方面,填充的共混物具有更高的结晶温度,特别是在快速冷却速率下。

    Polyarlyl ether ketone polymer blends
    4.
    发明申请
    Polyarlyl ether ketone polymer blends 有权
    聚芳醚酮聚合物共混物

    公开(公告)号:US20070066765A1

    公开(公告)日:2007-03-22

    申请号:US11456449

    申请日:2006-07-10

    IPC分类号: C08F20/00

    摘要: Phase separated blends of polyaryl ether ketones, polyaryl ketones, polyether ketones, polyether ether ketones and mixtures thereof with at least one polysulfone etherimide, wherein the polysulfone etherimide has greater than or equal to 50 mole % of the polymer linkages contain at least one aryl sulfone group are described. Such blends have improved load bearing capability at high temperature. In another aspect a high crystallization temperature, especially at fast cooling rates, is achieved.

    摘要翻译: 聚芳基醚酮,聚芳基酮,聚醚酮,聚醚醚酮及其与至少一种聚砜醚酰亚胺的混合物的相分离共混物,其中聚砜醚酰亚胺具有大于或等于50摩尔%的聚合物键含有至少一个芳基砜 组被描述。 这种混合物在高温下具有改善的承载能力。 在另一方面,实现了高结晶温度,特别是在快速冷却速率下。

    Poly aryl ether ketone polymer blends
    6.
    发明授权
    Poly aryl ether ketone polymer blends 有权
    聚芳基醚酮聚合物共混物

    公开(公告)号:US08945694B2

    公开(公告)日:2015-02-03

    申请号:US11687749

    申请日:2007-03-19

    摘要: Filled phase-separated blends of polyaryl ether ketones, polyaryl ketones, polyether ketones, polyether ether ketones and mixtures thereof with at least one polysulfone etherimide, wherein the polysulfone etherimide has greater than or equal to 50 mole % of the polymer linkages contain at least one aryl sulfone group are described. Such filled blends have improved load-bearing capability at high temperature. In another aspect the filled blends have a higher crystallization temperature, especially at fast cooling rates.

    摘要翻译: 聚芳基醚酮,聚芳基酮,聚醚酮,聚醚醚酮及其与至少一种聚砜醚酰亚胺的混合物的填充相分离共混物,其中聚砜醚酰亚胺具有大于或等于50摩尔%的聚合物键含有至少一个 描述芳基砜基团。 这种填充的共混物在高温下具有改善的承载能力。 在另一方面,填充的共混物具有更高的结晶温度,特别是在快速冷却速率下。

    Thermally stable thermoplastic resin compositions, methods of manufacture thereof and articles comprising the same
    7.
    发明申请
    Thermally stable thermoplastic resin compositions, methods of manufacture thereof and articles comprising the same 审中-公开
    热稳定性热塑性树脂组合物,其制造方法和包含其的制品

    公开(公告)号:US20060183841A1

    公开(公告)日:2006-08-17

    申请号:US11056810

    申请日:2005-02-11

    IPC分类号: C08K3/04

    摘要: Disclosed herein is a thermoplastic article comprising a thermoplastic polymer having a glass transition temperature of greater than or equal to about 150° C.; and an electrically conductive filler; wherein the thermoplastic article when annealed to a temperature of greater than or equal to about 245° C. for a period of greater than or equal to about 24 hours produces a warpage of less than or equal to about 3 millimeters/100 square millimeters, expressed as a percentage, and wherein the article has a volume resistivity of less than or equal to about 1012 ohm-cm and a surface resistivity of less than or equal to about 1010 ohm per square.

    摘要翻译: 本文公开了包含玻璃化转变温度大于或等于约150℃的热塑性聚合物的热塑性制品; 和导电填料; 其中当大于或等于约245℃的温度退火大于或等于约24小时的时间时,所述热塑性制品产生小于或等于约3毫米/ 100平方毫米的翘曲,表示为 以及其中所述制品的体积电阻率小于或等于约10 12欧姆 - 厘米,表面电阻率小于或等于约10 10欧姆 >欧姆/平方。