Bioactive material coating method and tube
    8.
    发明授权
    Bioactive material coating method and tube 有权
    生物活性材料涂层方法和管

    公开(公告)号:US08075940B2

    公开(公告)日:2011-12-13

    申请号:US12866235

    申请日:2009-01-19

    Abstract: A method for coating bioactive material and a structured coated with a bioactive material are disclosed. The bioactive material coating method includes: flowing a coating solution, produced as a bioactive material is dissolved in a mixed solvent, inside a structure having a lumen; and coating the bioactive material on at least one of inner and outer surfaces of the structure, with different concentrations. The mixed solvent is mixed with two or more solvents having different features. The occurrence of the strangulation of blood vessels and inflammation can be reduced. An increase in the size of the myofibroblast is not suppressed. The coating solution is produced as a medication is dissolved in a mixed solvent, where the mixed solvent is produced as a polar solvent and a nonpolar solvent are mixed with each other at a certain ratio.

    Abstract translation: 公开了一种用于涂覆生物活性材料和涂覆有生物活性材料的结构的方法。 生物活性物质涂布方法包括:将作为生物活性物质生产的涂布溶液溶解在具有内腔的结构内的混合溶剂中; 以及在所述结构的内表面和外表面中的至少一个上以不同的浓度涂覆所述生物活性材料。 将混合溶剂与具有不同特征的两种或更多种溶剂混合。 可以减少血管和炎症的窒息的发生。 肌成纤维细胞的大小的增加不被抑制。 将药物溶解在混合溶剂中时,制成涂布溶液,混合溶剂是作为极性溶剂制备混合溶剂,非极性溶剂以一定比例混合。

    POLYOLEFIN AND PREPARATION METHOD THEREOF
    9.
    发明申请
    POLYOLEFIN AND PREPARATION METHOD THEREOF 审中-公开
    聚烯烃及其制备方法

    公开(公告)号:US20100121006A1

    公开(公告)日:2010-05-13

    申请号:US12451198

    申请日:2008-05-02

    Abstract: The present invention relates to a polyolefin that has high environmental stress cracking resistance (ESCR), a high impact property, and an excellent die swell property, and a method of preparing the same. According to the method of preparing polyolefin of the present invention, a supported hybrid metallocene catalyst and an alpha olefin comonomer having 4 or more carbon atoms are used to obtain polyolefin having the bimodal or multimodal molecular weight distribution curves during the single reactor polymerization. The polyolefin has excellent processability, a melt flow rate ratio (MFRR) that is useful to processing, excellent shapability, impact strength, tensile strength, in particular, environmental stress cracking resistance (ESCR) and full notch creep test (FNCT), thus being used to manufacture the blow molded product.

    Abstract translation: 本发明涉及具有高耐环境应力开裂性(ESCR),高冲击性和优异的模具膨胀性的聚烯烃及其制备方法。 根据本发明的制备聚烯烃的方法,使用负载的杂化茂金属催化剂和具有4个或更多个碳原子的α-烯烃共聚单体来获得在单反应器聚合期间具有双峰或多峰分子量分布曲线的聚烯烃。 聚烯烃具有优异的加工性能,对加工有用的熔体流动速率比(MFRR),优异的成形性,冲击强度,拉伸强度,特别是环境应力开裂性(ESCR)和全切口蠕变试验(FNCT),因此 用于制造吹塑产品。