    摘要: A process for making non-thermoplastic starch fibers comprises the steps of: (a) providing a non-thermoplastic starch composition comprising from about 50% to about 75% by weight of modified starch and from about 25% to about 50% of water and having a shear viscosity within the at least one nozzle from about 1 to about 80 Pascals·second at the processing temperature and at a shear rate of 3,000 sec−1; (b) extruding the non-thermoplastic starch composition through at least one extrusion nozzle terminating with a nozzle tip, thereby forming at least one embryonic starch fiber; (c) attenuating the at least one embryonic starch fiber with an attenuating air having an average velocity at the nozzle tip greater than about 30 meters per second, to cause the fiber to form an average equivalent diameter of less than about 20 microns; (d) dewatering the at least one embryonic starch fiber to a consistency of from about 70% to about 99% by weight, thereby producing at least one non-thermoplastic starch fiber, wherein the starch fiber as a whole has no melting point.

    摘要翻译: 制备非热塑性淀粉纤维的方法包括以下步骤:(a)提供非热塑性淀粉组合物,其包含约50%至约75%重量的改性淀粉和约25%至约50%的水,以及 在加工温度和3000秒-1的剪切速率下,在至少一个喷嘴内具有约1至约80帕斯卡秒的剪切粘度; (b)通过终止于喷嘴尖端的至少一个挤出喷嘴挤出非热塑性淀粉组合物,从而形成至少一种胚胎淀粉纤维; (c)用具有大于约30米/秒的喷嘴尖端的平均速度的衰减空气减弱至少一种胚胎淀粉纤维,以使纤维形成小于约20微米的平均当量直径; (d)将至少一种胚胎淀粉纤维脱水至约70%至约99%重量的稠度,从而制备至少一种非热塑性淀粉纤维,其中整个淀粉纤维没有熔点。