Abstract:
In a method of producing a grain-oriented electrical steel sheet by subjecting a coil for grain-oriented electrical steel sheet after cold rolling to a primary recrystallization annealing, applying an annealing separator thereon, and conducting final annealing, rapid heating is conducted at a rate of not less than 80° C./sec from 500° C. to 700° C. in the course of heating for the primary recrystallization annealing, and a temperature keeping treatment is conducted for 2 to 100 hours from 700° C. to 1000° C. in the course of heating for the final annealing, and further, the final annealing is preferably conducted by laying a thermal insulation material on an upper surface of a coil supporting stand in an annealing furnace used for the final annealing concentrically from the outer periphery of the coil supporting stand and over an area of not less than 20% of the radius of the coil supporting stand.
Abstract:
An optical element for terahertz waves that transmits terahertz-wave incident beams through itself after being compressed into half or less a wavelength of the beam, the optical element comprising: a substrate that allows terahertz waves to be transmitted through itself; and a conductive coat that covers a surface of the substrate and is capable of blocking the waves, wherein the coat has an aperture provided in a circular region and ring-shaped grooves, provided on a surface of the coat, having the same center as the circular region and having radii which increase every fixed length, and wherein in the circular region, four or more fan-shaped tips each having an arc with the same radius of curvature as the radius of the region, are arranged at equal distances toward the center of the circle without contacting each other as the arc contacts an outer periphery of the region.
Abstract:
In a method of producing a grain-oriented electrical steel sheet by hot-rolling a steel slab of a chemical composition containing C: 0.001˜0.10%, Si: 1.0˜5.0%, Mn: 0.01˜1.0%, at least one of S and Se: 0.01˜0.05% in total, sol. Al: 0.003˜0.050%, N: 0.001˜0.020% by mass, subjecting to cold rolling, a primary recrystallization annealing, application of an annealing separator mainly composed of MgO and a finish annealing, a temperature rising rate S1 between 500˜600° C. in the primary recrystallization annealing is made to not less than 100° C./s and a temperature rising rate S2 between 600˜700° C. is made to 30° C./s˜0.6×S1° C./s, while a total content W (mol %) of an element having an ionic radius of 0.6˜1.3 Å and an attracting force between the ion and oxygen of not more than 0.7 Å−2 included in the annealing separator to MgO is adjusted to satisfy 0.01S2−5.5≦Ln (W)≦0.01S2−4.3 to produce a grain-oriented electrical steel sheet having excellent iron loss properties and coating properties.
Abstract:
Provided is a strain belonging to the genus Aurantiochytrium, the strain being characterized by there being at least 10 mass % of squalene in all the lipids produced by the strain, and by forming colonies exhibiting an orange-to-red color.
Abstract:
An insulin resistance marker, a method of evaluating insulin resistance, a method of screening a substance that improves insulin resistance, and a pharmaceutical composition for improving insulin resistance are provided. The insulin resistance marker includes a polypeptide comprising at least any 15 continuous amino acids in the specific amino acid sequence of SEQ ID NO: 1 (sequence of a proepithelin protein). The insulin resistance marker includes a polynucleotide selected from the group consisting of (1) a polynucleotide comprising at least any 45 continuous bases in the base sequence of SEQ ID NO:2 encoding the above specific amino acid sequence, and (2) a polynucleotide that is complementary to the polynucleotide of (1).
Abstract translation:提供胰岛素抵抗标记,评价胰岛素抵抗的方法,筛选改善胰岛素抵抗的物质的方法和用于改善胰岛素抵抗的药物组合物。 胰岛素抵抗标记物包括在SEQ ID NO:1的特定氨基酸序列(前列腺素蛋白质序列)中包含至少15个连续氨基酸的多肽。 胰岛素抵抗标记物包括选自(1)包含编码上述特定氨基酸序列的SEQ ID NO:2的碱基序列中至少任何45个连续碱基的多核苷酸的多核苷酸,和(2)多核苷酸, 与(1)的多核苷酸互补。
Abstract:
A system and method for controlling an operation of a power door of a vehicle are presented. An activation of a user interface device associated with the power door is detected. A cue is provided using a notification device after detecting the activation of the user interface device. In one implementation, the notification device includes an audible alarm. When the user interface device is activated for greater than a predetermined time period, the power door is caused to be in a power mode of operation, and the notification device is used to indicate a current operational mode of the power door. In one implementation, when the user interface device is deactivated within the predetermined time period, the power door is caused to be in a manual mode of operation.
Abstract:
In order to facilitate connecting to a SIP network, a router (20) forming a communication system (1) acquires information from a carrier network (30) by using DHCP. The information is necessary for connecting to a server (SIP server) placed on the carrier network. Moreover, a communication device (10) acquires the information from the router (20) by using local protocol that differs from the SIP and the DHCP. For example, UPnP protocol is adopted as the local protocol.
Abstract:
There is provided a coating composition capable of realizing a coating layer having conductivity and sufficient transparency. The coating composition contains respective components of a component (a) and a component (b) below, Component (a): acrylic resin or methane resin, Component (b): conductive polymer.
Abstract:
A treatment solution for an insulation coating for a grain oriented electrical steel sheet includes at least one member selected from phosphates of Mg, Ca, Ba, Sr, Zn, Al, and Mn, and colloidal silica in a proportion of 0.5 to 10 mol in terms of SiO2 and at least one member selected from permanganates of Mg, Sr, Zn, Ba, and Ca in a proportion of 0.02 to 2.5 mol in terms of metal elements in the permanganates, relative to PO4:1 mol in the phosphates.
Abstract:
The present invention provides a tumor screening marker that can be actually used in clinical practice to detect colorectal cancer, and a tumor progression marker that can complement CEA or CA19-9. Vitronectin for use as a tumor progression marker, a tumor screening marker or a prognostic prediction marker for colorectal cancer. A method of analyzing a vitronectin concentration in a collected blood sample. In the method, a measured value of vitronectin and a reference value of vitronectin are compared. Vitronectin is preferably used in combination with existing marker for colorectal cancer such as carcinoembryonic antigen and CA19-9.