摘要:
A heat resistant cast steel containing, in mass %, C: 0.05-0.15, Si: 0.03-0.2, Mn: 0.1-1.5, Ni: 0.1-1, Cr: 8-10.5, Mo: 0.2-1.5, V: 0.1-0.3, Co: 0.1-5, W: 0.1-5, N: 0.005-0.03, Nb: 0.01-0.2, B: 0.002-0.015, Ti: 0.01-0.1, Fe and unavoidable impurities. A method for manufacturing a heat resistant cast steel, the method including melting raw materials to obtain a molten metal, refining and degassing the molten metal, pouring the molten metal into a predetermined mold to form a shape, performing an annealing treatment at a temperature of 1000 to 1150° C., performing a normalizing treatment at a temperature of 1000 to 1200° C., performing a first stage tempering treatment at a temperature of 500 to 700° C., and performing a second stage tempering treatment at a temperature of 700 to 780° C.
摘要:
A lithium secondary-battery pack of the present invention includes: a lithium secondary battery including an electrode body and a non-aqueous electrolyte, the electrode body including a positive electrode and a negative electrode facing each other, and a separator interposed therebetween; a PTC (Positive Temperature Coefficient) element; and a protection circuit including a field-effect transistor, wherein the negative electrode includes a negative electrode material mixture layer containing a Si-containing material as a negative electrode active material, and, where Z represents an impedance (Ω) of the lithium secondary-battery pack and Q represents a capacity (Ah) of the lithium secondary-battery pack, an impedance capacity index represented by Z/Q is 0.055 Ω/Ah or less.
摘要:
The present invention provides a nonaqueous secondary battery with a high capacity, an excellent level of safety, and excellent charge-discharge cycle characteristics. The negative electrode contains, as negative electrode active materials, a graphite carbon material and a material containing Si as a constituent element, and the positive electrode includes, as a positive electrode active material, a lithium-containing composite oxide represented by the following general composition formula (1) and containing sulfur in a range of 0.01 mass % to 0.5 mass %: Li1+yMO2 (1) where y satisfies −0.3≦y
摘要:
An optical member including an oxide layer that has a stable fine textured structure and is excellent in durability is provided. The optical member includes a base material and an antireflection coating on a surface of the base material. The antireflection coating includes at least an oxide layer having a fine textured structure on the surface, and the oxide layer contains a phosphate compound. Furthermore, a method of manufacturing the optical member is provided.
摘要:
The non-aqueous secondary battery of the present invention includes a positive electrode, a negative electrode, a non-aqueous electrolyte, and a separator, the negative electrode contains a negative electrode active material containing a graphitic carbon material and a composite in which a carbon coating layer is formed on a surface of a core material containing Si and O as constituent elements, the composite has a carbon content of 10 to 30 mass %, the composite has an intensity ratio I510/I1343 of a peak intensity I510 at 510 cm−1 derived from Si to a peak intensity I1343 at 1343 cm−1 derived from carbon of 0.25 or less when a Raman spectrum of the composite is measured at a laser wavelength of 532 nm, and the half-width of the (111) diffraction peak of Si is less than 3.0° when the crystallite size of an Si phase contained in the core material is measured by X-ray diffractometry using CuKα radiation.
摘要:
In a seat (10), in a state in which tilting of a back main frame (16) around a tilting center (16A) is locked by a reclining mechanism (18), a lower end of a back joint link (26) is turnably joined to a vehicle side. Thus, turning of a first link (22), a back sub frame (24) and the back joint link (26) is locked, and operation of a back link mechanism (14) is locked. Therefore, a supporting rigidity from rear side of a back side portion (12B) can be enhanced by the back link mechanism (14) (the back sub frame (24)), and a crew sitting in the seat (10) can be thoroughly retained.
摘要:
A forging heat resistant steel of an embodiment contains in percent by mass C: 0.05-0.2, Si: 0.01-0.1, Mn: 0.01-0.15, Ni: 0.05-1, Cr: 8 or more and less than 10, Mo: 0.05-1, V: 0.05-0.3, Co: 1-5, W: 1-2.2, N: 0.01 or more and less than 0.015, Nb: 0.01-0.15, B: 0.003-0.03, and a remainder comprising Fe and unavoidable impurities.