Cold-Rolled Steel Sheet and Method for Producing the Same
    2.
    发明申请
    Cold-Rolled Steel Sheet and Method for Producing the Same 审中-公开
    冷轧钢板及其制造方法

    公开(公告)号:US20100221600A1

    公开(公告)日:2010-09-02

    申请号:US12086988

    申请日:2007-01-05

    IPC分类号: H01M2/02 C21D8/02 C22C38/00

    摘要: A cold-rolled steel sheet having superior non-ageing properties and low planar anisotropy can be produced at low cost without decreased productivity. This cold-rolled steel sheet contains, by mass, 0.010% to 0.040% carbon, 0.02% or less silicon, 1.0% to 2.5% manganese, 0.02% or less phosphorus, 0.015% or less sulfur, 0.004% or less nitrogen, and 0.020% to 0.070% aluminum, the balance being iron and incidental impurities. The steel sheet has a microstructure including a ferrite phase and a second phase. The volume percentage of the second phase is 0.2% to less than 10%. The steel sheet has an AI of 50 MPa or less, −0.20≦Δr≦0.20, and a thickness of 0.5 mm or less.

    摘要翻译: 可以低成本地制造具有优异的非时效性和低平面各向异性的冷轧钢板,而不降低生产率。 该冷轧钢板以质量计含有0.010〜0.040%的碳,0.02%以下的硅,1.0〜2.5%的锰,0.02%以下的磷,0.015%以下的硫,0.004%以下的氮,以及 0.020%至0.070%的铝,余量为铁和杂质。 钢板具有包括铁素体相和第二相的微结构。 第二相的体积百分比为0.2%至小于10%。 钢板的AI为50MPa以下,-0.20< lE;&Dgr; r≦̸ 0.20,厚度为0.5mm以下。