摘要:
An improved method for the after-treatment of washed and dried fibre cable having a minimum mass of 250 ktex by crimping, fixing, cooling and optionally cutting or tearing is achieved in that the band width of the cable issuing from the drier with a covering density of at most 5 ktex/cm is reduced by at least 50% of the original band width with a corresponding increase in the packing density, is crimped in a stuffer box crimping means at a stuffer box pressure of from 4 to 10 N/cm and a stuffer box temperature of from 80.degree. to 95.degree. C., the crimping is fixed in or immediately after the stuffer box, the cable is deposited on the surface of an air-permeable conveyor belt, air is blown or sucked there through fibre package or conveyor belt and the cable is then optionally supplied to a tearing converter or a cutting machine.
摘要:
Improved dressings for synthetic fibers, especially acrylonitrile fibers, comprise an anion-active preparation, a polyethylene dispersion and a dicarboxylic acid semi-ester salt.
摘要:
The invention relates to dry-spun modacrylic filaments with improved coloristic properties based on a polymer mixture, which comprises at least one acrylonitrile-vinyl chloride copolymer and a chlorine-containing copolymer containing sulphonic acid ester groups or sulphuric acid ester groups.
摘要:
The invention relates to new finishing mixtures, which contain fatty acid alkanolamides having softening points above 70.degree. C. as anti-blocking components, for synthetic fibers, particularly fibers of polyacrylonitrile, which are used as staple fibers. The invention also relates to the use of these finishing mixtures for the finishing of staple fibers, particularly polyacrylonitrile-based staple fibers.
摘要:
The invention relates to a process for the production of dyed filaments of aromatic polyamides which have not been modified with acid or basic group.
摘要:
The invention relates to wet-spun modacrylic filaments with improved coloristic properties based on a polymer mixture, which comprises at least one acrylonitrilevinyl chloride copolymer and a chlorine-containing copolymer containing sulphonic acid ester groups or sulphuric acid ester groups.
摘要:
High-shrinkage stretch-broken tows of acrylonitrile polymers are obtained by fixing with saturated steam at maximum temperatures of 140.degree. C. after drawing and before stretch breaking and stretch breaking at a draft of at least 30%.