公开(公告)号:US09120199B2
公开(公告)日:2015-09-01
申请号:US13314397
申请日:2011-12-08
申请人: Taiki Yoshino
发明人: Taiki Yoshino
CPC分类号: B24B37/044 , C09G1/02 , C09K3/1463 , C09K13/06
摘要: A polishing liquid composition that makes it possible to provide a polished substrate surface on which scratches and/or waviness are reduced, without impairing productivity, is provided, and further, a method for manufacturing and polishing a substrate using this polishing liquid composition is provided. The polishing liquid composition contains an abrasive, a water-soluble polymer, and water, wherein the water-soluble polymer has a sulfonic acid group, and has an aromatic ring in each of a main chain and a side chain. The method for manufacturing a substrate, and the method for polishing a substrate, include performing polishing by supplying the above-described polishing liquid composition to a surface to be polished of a substrate to be polished, bringing a polishing pad into contact with the surface to be polished, and moving the polishing pad and/or the substrate to be polished.
摘要翻译: 提供了一种可以提供在不损害生产率的情况下提供划痕和/或波纹减小的抛光衬底表面的研磨液组合物,并且还提供了使用该研磨液组合物制造和研磨衬底的方法。 抛光液组合物含有研磨剂,水溶性聚合物和水,其中水溶性聚合物具有磺酸基,并且在主链和侧链各自具有芳香环。 基板的制造方法以及基板的研磨方法包括通过将上述研磨液组合物供给到待研磨基板的待研磨面上进行研磨,使抛光垫与表面接触, 抛光,并移动抛光垫和/或待抛光的基板。
-
公开(公告)号:US08722774B2
公开(公告)日:2014-05-13
申请号:US13055327
申请日:2009-07-21
申请人: Taiki Yoshino , Akira Takenaka , Keiko Fukaya
发明人: Taiki Yoshino , Akira Takenaka , Keiko Fukaya
CPC分类号: C08L67/04 , C08L1/02 , C08L101/00 , C08L101/16 , C08L2666/26
摘要: A biodegradable resin composition containing a biodegradable resin and a cellulose having a crystallinity of less than 50%; and a biodegradable resin molded article wherein the biodegradable resin composition as defined above is molded. The biodegradable resin composition can be suitably used for various industrial applications, such as daily sundries, household electric appliance parts, and automobile parts.
摘要翻译: 一种生物降解性树脂组合物,其含有生物可降解树脂和结晶度小于50%的纤维素; 和可生物降解的树脂成形品,其中模塑上述的可生物降解的树脂组合物。 生物降解性树脂组合物可以适用于日用杂货,家电部件,汽车部件等各种工业用途。
-
公开(公告)号:US08716373B2
公开(公告)日:2014-05-06
申请号:US13057942
申请日:2009-08-06
申请人: Taiki Yoshino , Akira Takenaka , Keiko Fukaya
发明人: Taiki Yoshino , Akira Takenaka , Keiko Fukaya
CPC分类号: C08L67/04 , C08K5/11 , C08L1/02 , C08L2666/26
摘要: A biodegradable resin composition containing a biodegradable resin and a cellulose having a crystallinity of X (%), wherein the cellulose is obtained by a step including subjecting a cellulose-containing raw material to a pulverization treatment (A), wherein the cellulose-containing raw material contains a cellulose having a crystallinity of Y (%), and has a bulk density of from 100 to 500 kg/m3, and an average particle size of from 0.01 to 1.0 mm, and contains a cellulose in an amount of 20% by weight or more of a residue component obtained by removing water from the raw material, wherein X and Y satisfy the following formulas: 50≦X≦Y−5 (1) and 55≦Y≦99 (2). The biodegradable resin composition can be suitably used for various industrial applications, such as daily sundries, household electric appliance parts, and automobile parts.
摘要翻译: 一种生物降解性树脂组合物,其含有生物降解性树脂和结晶度为X(%)的纤维素,其中,所述纤维素通过包含使含纤维素原料进行粉碎处理(A)的工序得到,所述纤维素原料 材料含有结晶度为Y(%)的纤维素,堆积密度为100〜500kg / m 3,平均粒径为0.01〜1.0mm,纤维素含量为20% 重量或更多的通过从原料中除去水而获得的残余成分,其中X和Y满足下式:50≦̸ X< E; Y-5(1)和55≦̸ Y≦̸ 99(2)。 生物降解性树脂组合物可以适用于日用杂货,家电部件,汽车部件等各种工业用途。
-
公开(公告)号:US08481620B2
公开(公告)日:2013-07-09
申请号:US13125730
申请日:2009-10-22
申请人: Taiki Yoshino , Masahiro Mori , Akira Takenaka
发明人: Taiki Yoshino , Masahiro Mori , Akira Takenaka
CPC分类号: C08J3/201 , C08J3/226 , C08J2323/10 , C08J2367/04 , C08J2467/00 , C08K5/0008 , C08K5/0016 , C08K5/0083 , C08K5/11 , C08L23/10 , C08L23/26 , C08L67/04 , C08L2666/02 , C08L2666/06
摘要: A method for producing a resin composition, including the steps of melt-kneading a raw material A containing a polylactic acid resin, a crystal nucleating agent, and a plasticizer containing an ester compound formed between a polycarboxylic acid having a hydrocarbon group having 1 to 7 carbon atoms and a mono-alcohol having a hydrocarbon group having 1 to 7 carbon atoms, to prepare a polylactic acid-containing melt-kneaded mixture having a relative crystallinity of 70% or more (step A); and further melt-kneading the polylactic acid-containing melt-kneaded mixture obtained by the step A and a raw material B containing a polypropylene resin and a compatibilizing agent (step B). The resin composition obtainable by the method of the present invention can be suitably used in various industrial applications, such as daily sundries, household electric appliance parts, and automobile parts.
摘要翻译: 一种树脂组合物的制造方法,其特征在于,包括将含有聚乳酸树脂的原料A,结晶成核剂和含有具有1〜7个烃基的多元羧酸形成的含有酯化合物的增塑剂进行熔融混炼的工序 碳原子和具有1〜7个碳原子的烃基的单醇制备相对结晶度为70%以上的聚乳酸熔融混炼物(步骤A)。 进一步将通过工序A得到的含聚乳酸的熔融混炼混合物和含有聚丙烯树脂和相容剂的原料B进行熔融捏合(工序B)。 通过本发明的方法得到的树脂组合物可以适用于日用杂货,家电部件,汽车部件等各种工业用途。
-
公开(公告)号:US20120077422A1
公开(公告)日:2012-03-29
申请号:US13314397
申请日:2011-12-08
申请人: Taiki YOSHINO
发明人: Taiki YOSHINO
CPC分类号: B24B37/044 , C09G1/02 , C09K3/1463 , C09K13/06
摘要: A polishing liquid composition that makes it possible to provide a polished substrate surface on which scratches and/or waviness are reduced, without impairing productivity, is provided, and further, a method for manufacturing and polishing a substrate using this polishing liquid composition is provided. The polishing liquid composition contains an abrasive, a water-soluble polymer, and water, wherein the water-soluble polymer has a sulfonic acid group, and has an aromatic ring in each of a main chain and a side chain. The method for manufacturing a substrate, and the method for polishing a substrate, include performing polishing by supplying the above-described polishing liquid composition to a surface to be polished of a substrate to be polished, bringing a polishing pad into contact with the surface to be polished, and moving the polishing pad and/or the substrate to be polished.
摘要翻译: 提供了一种可以提供在不损害生产率的情况下提供划痕和/或波纹减小的抛光衬底表面的研磨液组合物,并且还提供了使用该研磨液组合物制造和研磨衬底的方法。 抛光液组合物含有研磨剂,水溶性聚合物和水,其中水溶性聚合物具有磺酸基,并且在主链和侧链各自具有芳香环。 基板的制造方法以及基板的研磨方法包括通过将上述研磨液组合物供给到待研磨基板的待研磨面上进行研磨,使抛光垫与表面接触, 抛光,并移动抛光垫和/或待抛光的基板。
-
公开(公告)号:US20110144241A1
公开(公告)日:2011-06-16
申请号:US13057942
申请日:2009-08-06
申请人: Taiki Yoshino , Akira Takenaka , Keiko Fukaya
发明人: Taiki Yoshino , Akira Takenaka , Keiko Fukaya
IPC分类号: C08L1/02
CPC分类号: C08L67/04 , C08K5/11 , C08L1/02 , C08L2666/26
摘要: A biodegradable resin composition containing a biodegradable resin and a cellulose having a crystallinity of X (%), wherein the cellulose is obtained by a step including subjecting a cellulose-containing raw material to a pulverization treatment (A), wherein the cellulose-containing raw material contains a cellulose having a crystallinity of Y (%), and has a bulk density of from 100 to 500 kg/m3, and an average particle size of from 0.01 to 1.0 mm, and contains a cellulose in an amount of 20% by weight or more of a residue component obtained by removing water from the raw material, wherein X and Y satisfy the following formulas: 50≦X≦Y−5 (1) and 55≦Y≦99 (2). The biodegradable resin composition can be suitably used for various industrial applications, such as daily sundries, household electric appliance parts, and automobile parts.
摘要翻译: 一种生物降解性树脂组合物,其含有生物降解性树脂和结晶度为X(%)的纤维素,其中,所述纤维素通过包含使含纤维素原料进行粉碎处理(A)的工序得到,所述纤维素原料 材料含有结晶度为Y(%)的纤维素,堆积密度为100〜500kg / m 3,平均粒径为0.01〜1.0mm,纤维素含量为20% 重量或更多的通过从原料中除去水而获得的残余成分,其中X和Y满足下式:50≦̸ X< E; Y-5(1)和55≦̸ Y≦̸ 99(2)。 生物降解性树脂组合物可以适用于日用杂货,家电部件,汽车部件等各种工业用途。
-
公开(公告)号:US20120283363A1
公开(公告)日:2012-11-08
申请号:US13514883
申请日:2010-12-10
申请人: Yoshiaki Kumamoto , Kenta Mukai , Hironobu Kawajiri , Akira Takenaka , Taiki Yoshino , Akira Isogai , Motoi Konishi , Tetsuji Kito
发明人: Yoshiaki Kumamoto , Kenta Mukai , Hironobu Kawajiri , Akira Takenaka , Taiki Yoshino , Akira Isogai , Motoi Konishi , Tetsuji Kito
CPC分类号: C08K7/02 , C08B15/04 , C08J5/045 , C08J2367/04 , C08L1/02 , C08L1/04 , C08L67/04 , C08L97/02 , C08L2205/16 , C08L2205/18 , C08L2666/26
摘要: A composite material of the invention is a mixture of cellulose microfibers having a carboxyl group content of 0.1 to 3 mmol/g and a moldable polymeric material selected from the group consisting of a biomass-derived polymer and a petroleum-derived polymer. The biomass-derived polymer is preferably polylactic acid or pulp. The cellulose microfibers are preferably present in an amount of 0.01% to 60% by mass. Another composite material of the invention is a mixture of cellulose composite microfibers and a moldable resin, the cellulose composite microfibers being obtained by adsorbing a surfactant onto cellulose microfibers having a carboxyl group content of 0.1 to 3 mmol/g.
摘要翻译: 本发明的复合材料是羧基含量为0.1〜3mmol / g的纤维素微纤维与选自由生物质衍生的聚合物和石油衍生的聚合物组成的组的可成型聚合材料的混合物。 生物质衍生聚合物优选为聚乳酸或纸浆。 纤维素微纤维优选以0.01〜60质量%的量存在。 本发明的另一种复合材料是纤维素复合微纤维和可模制树脂的混合物,纤维素复合微纤维通过将表面活性剂吸附在羧基含量为0.1至3mmol / g的纤维素微纤维上而获得。
-
公开(公告)号:US20110130488A1
公开(公告)日:2011-06-02
申请号:US13055327
申请日:2009-07-21
申请人: Taiki Yoshino , Akira Takenaka , Keiko Fukaya
发明人: Taiki Yoshino , Akira Takenaka , Keiko Fukaya
IPC分类号: C08L1/02
CPC分类号: C08L67/04 , C08L1/02 , C08L101/00 , C08L101/16 , C08L2666/26
摘要: A biodegradable resin composition containing a biodegradable resin and a cellulose having a crystallinity of less than 50%; and a biodegradable resin molded article wherein the biodegradable resin composition as defined above is molded. The biodegradable resin composition can be suitably used for various industrial applications, such as daily sundries, household electric appliance parts, and automobile parts.
摘要翻译: 一种生物降解性树脂组合物,其含有生物可降解树脂和结晶度小于50%的纤维素; 和可生物降解的树脂成形品,其中模塑上述的可生物降解的树脂组合物。 生物降解性树脂组合物可以适用于日用杂货,家用电器零件,汽车部件等各种工业用途。
-
公开(公告)号:US09243128B2
公开(公告)日:2016-01-26
申请号:US13514883
申请日:2010-12-10
申请人: Yoshiaki Kumamoto , Kenta Mukai , Hironobu Kawajiri , Akira Takenaka , Taiki Yoshino , Akira Isogai , Motoi Konishi , Tetsuji Kito
发明人: Yoshiaki Kumamoto , Kenta Mukai , Hironobu Kawajiri , Akira Takenaka , Taiki Yoshino , Akira Isogai , Motoi Konishi , Tetsuji Kito
CPC分类号: C08K7/02 , C08B15/04 , C08J5/045 , C08J2367/04 , C08L1/02 , C08L1/04 , C08L67/04 , C08L97/02 , C08L2205/16 , C08L2205/18 , C08L2666/26
摘要: A composite material of the invention is a mixture of cellulose microfibers having a carboxyl group content of 0.1 to 3 mmol/g and a moldable polymeric material selected from the group consisting of a biomass-derived polymer and a petroleum-derived polymer. The biomass-derived polymer is preferably polylactic acid or pulp. The cellulose microfibers are preferably present in an amount of 0.01% to 60% by mass. Another composite material of the invention is a mixture of cellulose composite microfibers and a moldable resin, the cellulose composite microfibers being obtained by adsorbing a surfactant onto cellulose microfibers having a carboxyl group content of 0.1 to 3 mmol/g.
摘要翻译: 本发明的复合材料是羧基含量为0.1〜3mmol / g的纤维素微纤维与选自由生物质衍生的聚合物和石油衍生的聚合物组成的组的可成型聚合材料的混合物。 生物质衍生的聚合物优选为聚乳酸或纸浆。 纤维素微纤维优选以0.01〜60质量%的量存在。 本发明的另一种复合材料是纤维素复合微纤维和可模制树脂的混合物,纤维素复合微纤维通过将表面活性剂吸附在羧基含量为0.1至3mmol / g的纤维素微纤维上而获得。
-
公开(公告)号:US20110196076A1
公开(公告)日:2011-08-11
申请号:US13125730
申请日:2009-10-22
申请人: Taiki Yoshino , Masahiro Mori , Akira Takenaka
发明人: Taiki Yoshino , Masahiro Mori , Akira Takenaka
IPC分类号: C08L23/12 , C08K3/34 , C08K5/3417 , C08K5/51 , C08K5/25 , C08K5/20 , C08K5/1515
CPC分类号: C08J3/201 , C08J3/226 , C08J2323/10 , C08J2367/04 , C08J2467/00 , C08K5/0008 , C08K5/0016 , C08K5/0083 , C08K5/11 , C08L23/10 , C08L23/26 , C08L67/04 , C08L2666/02 , C08L2666/06
摘要: A method for producing a resin composition, including the steps of melt-kneading a raw material A containing a polylactic acid resin, a crystal nucleating agent, and a plasticizer containing an ester compound formed between a polycarboxylic acid having a hydrocarbon group having 1 to 7 carbon atoms and a mono-alcohol having a hydrocarbon group having 1 to 7 carbon atoms, to prepare a polylactic acid-containing melt-kneaded mixture having a relative crystallinity of 70% or more (step A); and further melt-kneading the polylactic acid-containing melt-kneaded mixture obtained by the step A and a raw material B containing a polypropylene resin and a compatibilizing agent (step B). The resin composition obtainable by the method of the present invention can be suitably used in various industrial applications, such as daily sundries, household electric appliance parts, and automobile parts.
摘要翻译: 一种树脂组合物的制造方法,其特征在于,包括将含有聚乳酸树脂的原料A,结晶成核剂和含有具有1〜7个烃基的多元羧酸形成的含有酯化合物的增塑剂进行熔融混炼的工序 碳原子和具有1〜7个碳原子的烃基的单醇制备相对结晶度为70%以上的聚乳酸熔融混炼物(步骤A)。 进一步将通过工序A得到的含聚乳酸的熔融混炼混合物和含有聚丙烯树脂和相容剂的原料B进行熔融捏合(工序B)。 通过本发明的方法得到的树脂组合物可以适用于日用杂货,家电部件,汽车部件等各种工业用途。
-
-
-
-
-
-
-
-
-