Liquid phase diffusion bonding method for dissimilar metal sheets and liquid phase diffusion bonding apparatus for the same
    2.
    发明授权
    Liquid phase diffusion bonding method for dissimilar metal sheets and liquid phase diffusion bonding apparatus for the same 有权
    用于异种金属片的液相扩散接合方法和用于其的液相扩散接合装置

    公开(公告)号:US07119309B2

    公开(公告)日:2006-10-10

    申请号:US11054547

    申请日:2005-02-10

    IPC分类号: B23K13/01

    CPC分类号: B23K20/2275 B23K20/06

    摘要: A liquid phase diffusion bonding method for dissimilar metal sheets by allowing a galvanized steel sheet and an aluminum alloy sheet to come into close contact with each other and pressing both sheets by using a first mold of a liquid phase diffusion bonding apparatus and a second mold of the same; and heating the sheets at approximately the same heat-up rate and at approximately the same temperature to perform liquid phase diffusion bonding of the sheets by using induction heat generated by applying high frequency currents to a first high frequency induction heating coil provided on the first mold and a second high frequency induction heating coil provided on the second mold. The first high frequency induction heating coil and the second high frequency induction heating coil are positioned to sandwich the sheets at predetermined distances from the sheets, respectively.

    摘要翻译: 通过使用镀锌钢板和铝合金板彼此紧密接触并通过使用液相扩散接合装置的第一模具和第二模具来压制两个片材来进行异相金属片的液相扩散接合方法 一样; 并以大致相同的加热速度和大致相同的温度加热片材,以通过使用通过向设置在第一模具上的第一高频感应加热线圈施加高频电流而产生的感应热来进行片材的液相扩散接合 以及设置在第二模具上的第二高频感应加热线圈。 第一高频感应加热线圈和第二高频感应加热线圈分别定位成将片材夹住预定距离的片材。

    Liquid phase diffusion bonding method for dissimilar metal sheets and liquid phase diffusion bonding apparatus for the same
    3.
    发明申请
    Liquid phase diffusion bonding method for dissimilar metal sheets and liquid phase diffusion bonding apparatus for the same 有权
    用于异种金属片的液相扩散接合方法和用于其的液相扩散接合装置

    公开(公告)号:US20050178819A1

    公开(公告)日:2005-08-18

    申请号:US11054547

    申请日:2005-02-10

    CPC分类号: B23K20/2275 B23K20/06

    摘要: A liquid phase diffusion bonding method for dissimilar metal sheets of the present invention has the steps of: allowing a galvanized steel sheet and an aluminum alloy sheet to come into close contact with each other and pressing both sheets by using a first mold of a liquid phase diffusion bonding apparatus and a second mold of the same; and heating the galvanized steel sheet and the aluminum alloy sheet at approximately the same heat-up rate and at approximately the same temperature to perform liquid phase diffusion bonding of the sheets by using induction heat generated by applying high frequency currents to a first high frequency induction heating coil provided on the first mold and a second high frequency induction heating coil provided on the second mold. The first high frequency induction heating coil and the second high frequency induction heating coil are positioned to sandwich the galvanized steel sheet and the aluminum alloy sheet at predetermined distances from the sheets, respectively. By this method, it is possible to reduce a time for bonding the galvanized steel sheet and the aluminum alloy sheet and to ensure sufficient bonding strength between the sheets.

    摘要翻译: 本发明的异种金属片的液相扩散接合方法具有以下步骤:使镀锌钢板和铝合金板彼此紧密接触并通过使用液相的第一模具来压制两片 扩散接合装置和第二模具; 以大致相同的加热速度和大约相同的温度加热镀锌钢板和铝合金板,通过使用通过将高频电流施加到第一高频感应产生的感应热来进行片的液相扩散接合 设置在第一模具上的加热线圈和设置在第二模具上的第二高频感应加热线圈。 第一高频感应加热线圈和第二高频感应加热线圈分别定位成将预定距离的片材夹在镀锌钢板和铝合金板之间。 通过该方法,可以减少接合镀锌钢板和铝合金板的时间,并且确保片之间的充分的接合强度。

    Flanged parts producing method, and heat-treating device and heat treating method therefor
    4.
    发明授权
    Flanged parts producing method, and heat-treating device and heat treating method therefor 有权
    法兰部件生产方法,热处理装置及其热处理方法

    公开(公告)号:US07147731B2

    公开(公告)日:2006-12-12

    申请号:US10471517

    申请日:2002-03-27

    IPC分类号: C21D1/10

    摘要: A spacer 44 is inserted between an upper end face 44a of a contact column 40, and a lower face of a flange 14. The flange 14 is supported at plural positions by supporting columns 42. In heating a shoulder portion 16 to a hardening temperature, an electroconductive member 56 is placed close to the shoulder portion 16, and an AC current having a frequency which will cause mutual attraction between the current flowing through the elctroconductive member 56 and the current flowing through the shoulder portion 16 is applied to flow through the electroconductive member 56. The shoulder portion 16 having been heated to the hardening temperature is quenched by ejecting a liquid coolant through ejection outlets of a cooling jacket.

    摘要翻译: 间隔件44插入在接触柱40的上端面44a和凸缘14的下表面之间。 凸缘14通过支撑柱42支撑在多个位置。 在将肩部16加热到硬化温度时,导电部件56靠近肩部16放置,并且具有频率将导致流过导电部件56的电流与流过导电部件56的电流之间引起相互吸引的交流电流 肩部16被施加以流过导电构件56。 已经加热到硬化温度的肩部16通过冷却套的喷射出口喷射液体冷却剂来淬火。

    Constrained hardening method and apparatus for deformed bar workpieces
    5.
    发明授权
    Constrained hardening method and apparatus for deformed bar workpieces 有权
    变形棒工件的约束硬化方法和装置

    公开(公告)号:US06328829B1

    公开(公告)日:2001-12-11

    申请号:US09411204

    申请日:1999-10-04

    IPC分类号: C21D1673

    CPC分类号: C21D1/673 C21D9/0068

    摘要: Hardening is accomplished by heating a longitudinal section of a workpiece such as an odd-shaped bar, and by quenching while constraining the workpiece section in dies. The quenching is executed while the workpiece is pressed in a direction perpendicular to its longitudinal direction by a pressing device which is installed adjacent to the workpiece section constrained in the dies. Warping by quenching can thus be minimized in odd-shaped workpieces, such as an automobile steering rack bar.

    摘要翻译: 通过加热诸如异型棒的工件的纵向部分,并且通过在模具中约束工件部分的同时进行淬火来实现硬化。 通过与被限制在模具中的工件相邻设置的加压装置沿垂直于其纵向的方向按压工件来执行淬火。 因此,在诸如汽车转向架杆的异型工件中可以使淬火变形最小化。

    Method and apparatus for quenching a tubular workpiece
    6.
    发明授权
    Method and apparatus for quenching a tubular workpiece 失效
    用于淬火管状工件的方法和装置

    公开(公告)号:US5626693A

    公开(公告)日:1997-05-06

    申请号:US504755

    申请日:1995-07-19

    CPC分类号: C21D1/673 C21D9/08 C21D11/00

    摘要: This invention provides a method and apparatus for quenching a tubular workpiece such as cylindrical tubes or different-shaped tubes, which are difficult to be exerted constraining force for preventing warping especially in case of thinner thickness. Warping is prevented by applying a constraining force which is increased from beginning of the quenching to termination thereof, corresponding to increase of elasticity limit stress in accordance with temperature drop of the workpiece. Furthermore, apparatus for carrying out the method for quenching a tubular workpiece are offered, wherein the apparatus are provided with a pressure controller for pressure rolls or dies, thereby the pressure controller changes setting input for the pressure during the quenching.

    摘要翻译: 本发明提供了一种用于淬火管状工件的方法和装置,例如圆柱形管或不同形状的管,其难以施加约束力以防止翘曲,特别是在厚度较薄的情况下。 通过施加从淬火开始到终止的约束力,根据工件的温度下降对应于弹性极限应力的增加来防止翘曲。 此外,提供了用于实施用于淬火管状工件的方法的装置,其中该装置设置有用于压力辊或模具的压力控制器,由此压力控制器改变淬火期间的压力的设定输入。

    Constrained quenching apparatus and heat treatment apparatus
    7.
    发明授权
    Constrained quenching apparatus and heat treatment apparatus 失效
    约束淬火装置和热处理装置

    公开(公告)号:US5492308A

    公开(公告)日:1996-02-20

    申请号:US295727

    申请日:1994-08-26

    CPC分类号: C21D1/673 C21D9/08 C21D9/085

    摘要: A constrained quenching apparatus is provided for hardening a workpiece such as an asymmetrical bar which has a notable tendency to warping when quenched, without warping the workpiece. The apparatus comprises a set of two or more dies having plural projections provided on the inner side thereof, the projections coinciding with the contour of the workpiece when the dies are closed so that their die faces in contact with one another, and having plural recesses therein defined by the projections. The recesses are provided with one or more cooling liquid blow holes. The apparatus does not exert pressure on the workpiece at the start of the quenching when the workpiece is soft, so the flattening of the hollow workpiece such as a pipe, can be prevented.

    摘要翻译: 提供一种约束淬火装置,用于硬化诸如不对称杆的工件,其在淬火时具有显着的翘曲倾向,而不会使工件翘曲。 该设备包括一组两个或更多个模具,其具有设置在其内侧上的多个突起,当模具闭合时突起与工件的轮廓重合,使得它们的模具面彼此接触并且在其中具有多个凹部 由投影定义。 凹部设置有一个或多个冷却液体吹出孔。 该装置在工件柔软时在淬火开始时不对工件施加压力,因此可以防止中空工件(例如管)的扁平化。

    Method and apparatus for isothermal holding of wire when a wire is
heat-treated in-line
    8.
    发明授权
    Method and apparatus for isothermal holding of wire when a wire is heat-treated in-line 失效
    线材在线热处理时等温保持线材的方法和装置

    公开(公告)号:US4943036A

    公开(公告)日:1990-07-24

    申请号:US262733

    申请日:1988-10-12

    IPC分类号: C21D9/56 C21D9/62

    CPC分类号: C21D9/56 C21D9/62

    摘要: The present invention is drawn to a method and apparatus for holding wire at a specified temperature for a specified period of time by a direct-resistance heating device which applies such voltage as to generate Joule's heat in the wire, sufficient to offset the quantity of heat that would tend to be released from the heated wire during unforced cooling, after the travelling wire is heated rapidly to a specified temperature throughout its cross section. A temperature-holding apparatus, employed subsequent to the heating of wire, may either supply power directly to a wire through feeding wheel electrodes or entail a combination of a shell type transformer and a hollow annular holding furnace incorporating guide rollers, and having wheel electrodes electrically connected by a lead, disposed outside of the inlet and outlet of the holding furnace incorporating guide rollers, and producing secondary current in the multiple-wound wire in the furnace with the lead as a return, depending upon the holding time desired. The latter form of the apparatus imparts an advancing force and curl to the wire so that thick and inflexible wire can be placed in the holding furnace, and rollers are provided to create a desired number of turns in the wire in the holding furnace.

    摘要翻译: 本发明涉及一种用于通过直流电阻加热装置在特定温度保持指定温度的方法和装置,所述直流电阻加热装置施加在电线中产生焦耳热的电压,足以抵消热量 在行走导线在整个横截面中被快速加热至特定温度之后,将在非强制冷却期间倾向于从加热的线释放。 在加热电线之后使用的温度保持装置可以通过馈电轮电极直接供电到电线,或者需要壳型变压器和包含导向辊的中空环形保持炉的组合,并且具有电极 通过引线连接,设置在包含引导辊的保持炉的入口和出口的外部,并且根据所需的保持时间,以引线作为返回在炉中的多绕线中产生二次电流。 装置的后一种形式赋予线的前进力并卷曲,使得厚而不弯曲的线可以放置在保持炉中,并且提供辊以在保持炉中的线中产生所需数量的匝数。