摘要:
A polyimide tube composed of a polyimide resin composition in which 5 to 23.5 volume percent of boron nitride and 1 to 15 volume percent of an acicular substance are dispersed as a filler in a polyimide resin on the basis of the total volume of the composition, a method of producing the tube, a method of producing a polyimide varnish used for producing the tube, and a fixing belt including the tube as a base member are provided.
摘要:
Provided are a polyimide tube including a polyimide resin composition, wherein the polyimide resin composition contains a polyimide resin in which an acicular highly thermally conductive filler such as carbon nanotubes is dispersed in 15 volume percent or more relative to the total volume of the composition; the acicular highly thermally conductive filler has an orientation of 1.3 or more, the orientation being represented by the modulus of elasticity of the polyimide resin composition in the circumferential direction/the modulus of elasticity of the polyimide resin composition in the axial direction; and the polyimide tube has high thermal conductivity, is excellent in terms of mechanical strength and indentation strength, and provides a high fixing property and an excellent offsetting property; a process for producing such a tube; and a fixing belt including such a tube serving as a base member.
摘要:
A polyimide tube composed of a polyimide resin composition in which 5 to 23.5 volume percent of boron nitride and 1 to 15 volume percent of an acicular substance are dispersed as a filler in a polyimide resin on the basis of the total volume of the composition, a method of producing the tube, a method of producing a polyimide varnish used for producing the tube, and a fixing belt including the tube as a base member are provided.
摘要:
Provided is a heating fixing roller which includes a tubular base member and a fluororesin layer provided on an outer circumferential surface of the base member directly or through an adhesive layer, the heating fixing roller being characterized in that the fluororesin layer contains phosphorus-doped tin oxide. The heating fixing roller has a surface resistance capable of stably and effectively preventing the occurrence of electrostatic offsets, and also has an excellent releasing property. Also provided is a process for producing the heating fixing roller, characterized by including the steps of applying a fluororesin dispersion containing an aqueous dispersion of phosphorus-doped tin oxide onto a tubular base member or an adhesive layer disposed on an outer circumferential surface of the tubular base member, and then sintering the fluororesin.
摘要:
Provided are a method for producing a roller for office automation (OA) equipment, the roller capable of realizing an increase in the printing speed and having a good releasing property, and a roller for OA equipment. The method for producing a roller for OA equipment, the roller including a fluororesin layer provided on an outer circumferential surface of a tubular base either directly or with an intermediate layer therebetween, includes the steps of preparing a fluororesin coating material containing a tetrafluoroethylene-perfluoroalkylvinylether copolymer (PFA) and polytetrafluoroethylene (PTFE) in a ratio of 99:1 to 50:50 (mass ratio); applying the fluororesin coating material onto an outer circumferential surface of a tubular base either directly or with an intermediate layer therebetween; baking the fluororesin coating material at a temperature of 340° C. or higher to form a fluororesin layer; and after baking, cooling the fluororesin layer at a cooling rate of 20° C./min or less.
摘要:
Provided is a heating fixing roller which includes a tubular base member and a fluororesin layer provided on an outer circumferential surface of the base member directly or through an adhesive layer, the heating fixing roller being characterized in that the fluororesin layer contains phosphorus-doped tin oxide. The heating fixing roller has a surface resistance capable of stably and effectively preventing the occurrence of electrostatic offsets, and also has an excellent releasing property. Also provided is a process for producing the heating fixing roller, characterized by including the steps of applying a fluororesin dispersion containing an aqueous dispersion of phosphorus-doped tin oxide onto a tubular base member or an adhesive layer disposed on an outer circumferential surface of the tubular base member, and then sintering the fluororesin.
摘要:
Provided are a polyimide tube including a polyimide resin composition, wherein the polyimide resin composition contains a polyimide resin in which an acicular highly thermally conductive filler such as carbon nanotubes is dispersed in 15 volume percent or more relative to the total volume of the composition; the acicular highly thermally conductive filler has an orientation of 1.3 or more, the orientation being represented by the modulus of elasticity of the polyimide resin composition in the circumferential direction/the modulus of elasticity of the polyimide resin composition in the axial direction; and the polyimide tube has high thermal conductivity, is excellent in terms of mechanical strength and indentation strength, and provides a high fixing property and an excellent offsetting property; a process for producing such a tube; and a fixing belt including such a tube serving as a base member.