摘要:
A Ni-based single crystal superalloy according to the invention has, for example, a composition including: 5.0 to 7.0 wt % of Al, 4.0 to 10.0 wt % of Ta, 1.1 to 4.5 wt % of Mo, 4.0 to 10.0 wt % of W, 3.1 to 8.0 wt % of Re, 0.0 to 2.0 wt % of Hf, 2.5 to 8.5 wt % of Cr, 0.0 to 9.9 wt % of Co, 0.0 to 4.0 wt % of Nb, and 1.0 to 14.0 wt % of Ru in terms of weight ratio; and the remainder including Ni and incidental impurities. In addition, the contents of Cr, Hf and Al are preferably set so as to satisfy the equation OP≧108. According to the Ni-based single crystal superalloy of the invention, high creep strength can be maintained and the oxidation resistance can be improved.
摘要:
A Ni-based single crystal superalloy according to the invention has, for example, a composition including: 5.0 to 7.0 wt % of Al, 4.0 to 10.0 wt % of Ta, 1.1 to 4.5 wt % of Mo, 4.0 to 10.0 wt % of W, 3.1 to 8.0 wt % of Re, 0.0 to 2.0 wt % of Hf, 2.5 to 8.5 wt % of Cr, 0.0 to 9.9 wt % of Co, 0.0 to 4.0 wt % of Nb, and 1.0 to 14.0 wt % of Ru in terms of weight ratio; and the remainder including Ni and incidental impurities. In addition, the contents of Cr, Hf and Al are preferably set so as to satisfy the equation OP≧108. According to the Ni-based single crystal superalloy of the invention, high creep strength can be maintained and the oxidation resistance can be improved.
摘要:
A Ni-based single crystal superalloy which has the following composition: Co: 0.0 wt % or more to 15.0 wt % or less, Cr: 4.1 to 8.0 wt %, Mo: 2.1 to 6.5 wt %, W: 0.0 to 3.9 wt %, Ta: 4.0 to 10.0 wt %, Al: 4.5 to 6.5 wt %, Ti: 0.0 to 1.0 wt %, Hf: 0.00 to 0.5 wt %, Nb: 0.0 to 3.0 wt %, Re: 3.0 to 8.0 wt % and Ru: 0.5 to 6.5 wt % with the remainder including Ni and unavoidable impurities, wherein P1≦700 is satisfied in which P1 represents a parameter 1, which is obtained by a formula: P1=137×[W (wt %)]+24×[Cr (wt %)]+46×[Mo (wt %)]−18×[Re (wt %)]. The Ni-based single crystal superalloy has excellent specific creep strength.
摘要:
A Ni-based single crystal superalloy which has the following composition: Co: 0.0 wt % or more to 15.0 wt % or less, Cr: 4.1 to 8.0 wt %, Mo: 2.1 to 4.5 wt %, W: 0.0 to 3.9 wt %, Ta: 4.0 to 10.0 wt %, Al: 4.5 to 6.5 wt %, Ti: 0.0 to 1.0 wt %, Hf: 0.00 to 0.5 wt %, Nb: 0.0 to 3.0 wt %, Re: 8.1 to 9.9 wt % and Ru: 0.5 to 6.5 wt % with the remainder including Ni and unavoidable impurities. As a result, the Ni-based single crystal superalloy which includes more than 8 wt % of Re in the composition ratio and has excellent specific creep strength and the turbine blade incorporating the Ni-based single crystal superalloy may be made.
摘要:
A Ni-based single crystal superalloy which has the following composition: Co: 0.0 wt % or more to 15.0 wt % or less, Cr: 4.1 to 8.0 wt %, Mo: 2.1 to 4.5 wt %, W: 0.0 to 3.9 wt %, Ta: 4.0 to 10.0 wt %, Al: 4.5 to 6.5 wt %, Ti: 0.0 to 1.0 wt %, Hf: 0.00 to 0.5 wt %, Nb: 0.0 to 3.0 wt %, Re: 8.1 to 9.9 wt % and Ru: 0.5 to 6.5 wt % with the remainder including Ni and unavoidable impurities. As a result, the Ni-based single crystal superalloy which includes more than 8 wt % of Re in the composition ratio and has excellent specific creep strength and the turbine blade incorporating the Ni-based single crystal superalloy may be made.
摘要:
A heat resistant material, wherein one type or plural types of materials that do not generate interdiffusion with an Ni-based superalloy are coated on the Ni-based superalloy to prevent the interdiffusion of elements through the substrate/coating interface even at such high temperatures as 1100° C. or above 1100° C., is provided.
摘要:
A heat-resistant member is provided that includes a Ni-base superalloy substrate coated with at least one substance. The substrate and the substance are formed of materials that are substantially in a state of thermodynamic equilibrium, or in a state similar to a state of thermodynamic equilibrium, so that interdiffusion is suppressed. The heat-resistant member therefore inhibits interdiffusion of elements at the substrate/coating interface even at elevated temperatures of 1,100° C. and higher.
摘要:
A heat resistant material, wherein one type or plural types of materials that do not generate interdiffusion with an Ni-based superalloy are coated on the Ni-based superalloy to prevent the interdiffusion of elements through the substrate/coating interface even at such high temperatures as 1100° C. or above 1100° C., is provided.
摘要:
A heat-resistant member is provided that includes a Ni-base superalloy substrate coated with at least one substance. The substrate and the substance are formed of materials that are substantially in a state of thermodynamic equilibrium, or in a state similar to a state of thermodynamic equilibrium, so that interdiffusion is suppressed. The heat-resistant member therefore inhibits interdiffusion of elements at the substrate/coating interface even at elevated temperatures of 1,100° C. and higher.
摘要:
Disclosed is a novel heat-resistant superalloy for turbine disks having a chemical composition consisting of, in mass %, 19.5-55% of cobalt, 2-25% of chromium, 0.2-7% of aluminum, 3-15% of titanium and the balance of nickel and inevitable impurities.