公开(公告)号:US09944743B2
公开(公告)日:2018-04-17
申请号:US15009851
申请日:2016-01-29
Applicant: Allnex Netherlands B.V.
Inventor: Dirk Emiel Paula Mestach , Rob Adolphs , Adam Berry , Maria Paulis , Maria Barandiaran , José Asua , Monika Goikoetxea , Itxaso Beristain
IPC: C08F290/06 , C09D11/105 , C09D151/08 , C09J151/08 , C08F2/24 , C09D5/02 , C09D11/10
CPC classification number: C08F290/061 , C08F2/24 , C09D5/02 , C09D11/10 , C09D11/105 , C09D151/08 , C09J151/08 , C08F220/00
Abstract: The process for the manufacture of an auto-oxidatively cross-linking hybrid polymer, in particular an aqueous hybrid polymer dispersion, comprises the step of reacting in a mini-emulsion process one or more ethylenically unsaturated monomers to form an addition polymer in the presence of a modified auto-oxidatively crosslinkable (AOC) polymer which has been modified with terminal unsaturated groups of the formula —C(R1)═CH2 wherein R1 is hydrogen, alkyl or aryl and wherein the AOC polymer is a hydrophobic polymer having an acid number between 5 to 30. The resulting aqueous hybrid polymer dispersion can be used for the manufacture of coating compositions, ink compositions or adhesives and coating compositions comprising the hybrid polymer dispersion as a binder.
-
公开(公告)号:US11084953B2
公开(公告)日:2021-08-10
申请号:US16750049
申请日:2020-01-23
Applicant: Allnex Netherlands B.V.
Inventor: Jaap Michiel Akkerman , Dirk Emiel Paula Mestach , Wincenty Lambertus Stanislaw Pilaszek , Rob Adolphs
IPC: C09D133/12 , C08F220/18 , C08F220/28 , C08F283/00 , C08G18/34 , C08G18/62 , C08G18/69 , C08G18/75 , C09D133/14 , C09D151/08 , C09D175/14 , C08G18/08
Abstract: The invention relates to a method of making an aqueous coating composition comprising a blend of at least a first aqueous polymer dispersion and a second aqueous polymer dispersion comprising a film-forming second polymer wherein the first aqueous polymer dispersion comprises a first polymer having a number average molecular weight, Mn, of from 2000 to 120000, an acid value of 30 to 150 mg KOH/g, a glass transition temperature Tg of at least 20° C. as calculated with the Fox formula, and an ethylene-oxide content of from 1 to 20 wt %, the method comprising blending an aqueous dispersion of the first polymer having a solids content of 25 to 50 wt % and a pH of 4.5 to 8.0 with an aqueous dispersion of the second polymer having a solids content of 25 to 55 wt % and a pH of 4.5 to 8.0.
-