Stabilized water-soluble polymer powders on the basis of polyoxy alkylene glycol carboxylates and method for producing same
    2.
    发明授权
    Stabilized water-soluble polymer powders on the basis of polyoxy alkylene glycol carboxylates and method for producing same 有权
    基于聚氧化亚烷基二醇羧酸酯的稳定的水溶性聚合物粉末及其制备方法

    公开(公告)号:US06573316B1

    公开(公告)日:2003-06-03

    申请号:US09720922

    申请日:2000-12-28

    IPC分类号: C08K534

    摘要: Stabilized, water-soluble polymer powders based on polyoxyalkylene glycol carboxylates are described, wherein the powders comprise from 0.01 to 10% by weight of a stabilizer selected from the group consisting of phenols, amines, phosphites, thioethers, and also thioacids, and where the stabilizer was added in liquid or dissolved form to the aqueous polymer solution prior to its conversion into the powder form. The polymer powders thus protected against autoignition and oxidative degradation have unexpectedly high thermooxidative stability, even on exposure to high temperatures and oxidizing action (air, oxygen).

    摘要翻译: 描述了基于聚氧亚烷基二醇羧酸酯的稳定的水溶性聚合物粉末,其中粉末包含0.01至10重量%的选自酚,胺,亚磷酸酯,硫醚和硫代酸的稳定剂,并且其中 稳定剂在其转化成粉末形式之前以液体或溶解形式加入到聚合物水溶液中。 因此,即使暴露于高温和氧化作用(空气,氧气),因此防止自燃和氧化降解的聚合物粉末具有出乎意料的高的热氧化稳定性。

    Process for the production of sulphonic acid group-containing
condensation products with a low content of free formaldehyde
    3.
    发明授权
    Process for the production of sulphonic acid group-containing condensation products with a low content of free formaldehyde 失效
    生产含有低含量免费甲醛的含有酸性基团的冷凝产品的方法

    公开(公告)号:US5071945A

    公开(公告)日:1991-12-10

    申请号:US561353

    申请日:1990-08-01

    IPC分类号: C08G12/30 C08G12/40

    CPC分类号: C08G12/30 C08G12/40

    摘要: A process for the production of sulphonic acid group-containing condensation products based on amino-s-triazines with at least two amino groups and formaldehyde with a low content of free formaldehyde, whereina) an amino-s-triazine, formaldehyde and sulphite is condensed in a mole ratio of 1:1.3 to 6:0.3 to 1.5 in aqueous solution at a pH value of 9.0 to 12.0 and at a temperature of 50.degree. to 90.degree. C. until sulphite is no longer detectable.b) subsequently, further condensation is carried out at a pH value of 2.0 to 7.0 and at a temperature of 50.degree. to 90.degree. C. until the viscosity of the solution is 4 to 1000 mm.sup.2 /s at 80.degree. C. andc) thereafter the condensation product is subjected to an after-treatment in a strongly alkaline range of pH.sqroot.11.0 and at an elevated temperature.

    摘要翻译: 一种基于具有至少两个氨基的氨基-s-三嗪和游离甲醛含量低的甲醛生产含磺酸基的缩合产物的方法,其中a)氨基-s-三嗪,甲醛和亚硫酸盐是 在9.0至12.0的pH值和50-90℃的温度下,以1:1.3至6:0.3至1.5的摩尔比浓缩,直到亚硫酸盐不再可检测。 b)随后,在2.0至7.0的pH值和在50至90℃的温度下进行进一步的缩合,直到80℃下溶液的粘度为4至1000mm 2 / s,c) 然后在pH 2ROOT 11.0的强碱性范围内和在升高的温度下对缩合产物进行后处理。

    Flow improving agents for binder suspensions containing cement
    4.
    发明授权
    Flow improving agents for binder suspensions containing cement 失效
    含水泥粘合剂悬浮液的流动改进剂

    公开(公告)号:US5558709A

    公开(公告)日:1996-09-24

    申请号:US517818

    申请日:1995-08-22

    摘要: Disclosed is a flow improving agent for binder suspensions containing cement which is composed of a) amino-s-triazine-formaldehyde-sulfite condensation products having a molar ratio of amino-s-triazine:formaldehyde:sulfite of 1:1.3 to 6.0: 0.3 to 1.5 and a low content of free formaldehye as well as b) casein. The flow improving agents have the advantage that the flowability is considerably improved compared to casein (alone) for example and the increased flowability remains constant even over a longer time period.

    摘要翻译: 公开了一种含有水泥的粘结剂悬浮液的流动改进剂,其由a)氨基-s-三嗪 - 甲醛 - 亚硫酸盐缩合产物组成,其氨基-s-三嗪:甲醛:亚硫酸盐的摩尔比为1:1.3至6.0:0.3 至1.5和低含量的游离形式,以及b)酪蛋白。 流动改进剂的优点在于,与酪蛋白(单独)相比,流动性显着提高,并且即使在更长的时间内也增加流动性保持恒定。

    Condensation products based on amino-s-triazines and the use thereof
    5.
    发明授权
    Condensation products based on amino-s-triazines and the use thereof 失效
    基于氨基-s-三嗪的缩合产物及其用途

    公开(公告)号:US06555683B1

    公开(公告)日:2003-04-29

    申请号:US08930839

    申请日:1997-09-29

    IPC分类号: C07D25164

    摘要: In the proposed condensation product based on amino-s-triazines with at least two amino groups, formaldehyde and sulphite, the molar ratio of amino-s-triazine, formaldehyde and sulphite is 1:2.5-6.0:1.51-2.0 and the formiate content is less than 0.3 wt %. The condensation product is obtained by a) heating amino-s-triazine, formaldehyde and a sulphite in the molar ratio 1:2.5-6.0:1.51-2.0 in an aqueous solution at a temperature of 60-90° C. and a pH level of between 9.0 and 13.0 until the sulphite can no longer be detected; b) continuing the condensation at a pH level of between 3.0 and 6.5 and a temperature of 60-80° C. until the condensation product has a viscosity of 5-50 mm/s at 80° C.; and c) adjusting the pH level of the condensation product to 7.5-12.0 or carrying out thermal secondary treatment at a pH level of >10.0 and a temperature of 60-100° C. The product can be used as an additive for inorganic binders such as cement.

    摘要翻译: 在提出的基于具有至少两个氨基的氨基-s-三嗪,甲醛和亚硫酸盐的缩合产物中,氨基-s-三嗪,甲醛和亚硫酸盐的摩尔比为1:2.5-6.0:1.51-2.0,甲酸含量 小于0.3重量%。 缩合产物通过以下步骤获得:a)在60-90℃的温度下,在水溶液中加热氨基-s-三嗪,甲醛和摩尔比为1:2.5-6.0:1.51-2.0的亚硫酸盐,pH值 在9.0和13.0之间,直到亚硫酸盐不能再被检出; b)在3.0至6.5的pH水平和60-80℃的温度下继续冷凝,直到缩合产物在80℃下的粘度为5-50mm / s; 和c)将缩合产物的pH值调节至7.5-12.0,或在pH值> 10.0,温度为60-100℃下进行热二次处理。该产品可用作无机粘合剂的添加剂 作为水泥。

    Flow improving agents for binder suspensions containing cement
    6.
    发明授权
    Flow improving agents for binder suspensions containing cement 失效
    含水泥粘合剂悬浮液的流动改进剂

    公开(公告)号:US6150437A

    公开(公告)日:2000-11-21

    申请号:US478331

    申请日:1995-06-07

    摘要: Flow improving agents for binder suspensions containing cement are described, which consist of:a) Graft polymers which have been prepared by radical grafting of a polyalkylene oxide of the general formula (I) with an ethylenically unsaturated mono- or dicarboxylic acid or the anhydride thereof, and then by derivatizing with a primary or secondary amine and/or alcohol, and also ofb) Casein.These flow improving agents have the advantage that the ability to flow is considerably improved in comparison, for example, with casein alone, and the improved ability to flow is preserved over a longer period of time.

    摘要翻译: 描述了含有水泥的粘合剂悬浮液的流动改进剂,其由以下组成:a)通过使通式(I)的聚环氧烷通过烯键式不饱和单或二羧酸或其酸酐进行自由基接枝而制备的接枝聚合物 然后通过用伯胺或仲胺和/或醇衍生化,以及b)酪蛋白。 这些流动改进剂的优点在于,例如,仅使用酪蛋白,流动的能力在很长一段时间内被保持,从而显着改善了流动能力。

    Water-soluble graft polymers
    7.
    发明授权
    Water-soluble graft polymers 失效
    水溶性接枝聚合物

    公开(公告)号:US5739212A

    公开(公告)日:1998-04-14

    申请号:US545546

    申请日:1995-10-19

    摘要: Water-soluble graft polymers are described which have been produced by a) radical grafting of a polyalkylene oxide of the general formula I ##STR1## in which R.sup.1 =--H, --C.sub.n H.sub.2n+1, --C.sub.6 H.sub.4 --C.sub.n H.sub.2n+1, ##STR2## --(CH--R.sup.2).sub.m NHR.sup.2, --(CH--R.sup.2).sub.m OH, --(CH--R.sup.2).sub.m --COOH, --CO--R.sup.5 R.sup.2 =--H, --CH.sub.3, --C.sub.2 H.sub.5 R.sup.3 =--H, --C.sub.n H.sub.2n+1, --C.sub.m H.sub.2m --SO.sub.3 Na, --(CH--R.sup.2).sub.m NHR.sup.2, --(CH--R.sup.2).sub.m OH, --(CH--R.sup.2).sub.m --COOH, --CO--R.sup.5 R.sup.4 =--H, --(CH--R.sup.2).sub.m --COOH, --CO--R.sup.5 R.sup.5 =--C.sub.m H.sub.2m+1, --C.sub.6 H.sub.5, --(CH--R.sup.2).sub.m --COOH, --C.sub.6 H.sub.4 --COOH n denotes 1-18, m denotes 1-5, x denotes 2-200, y denotes 0 or 1 with an ethylenically unsaturated mono or dicarboxylic acid or their anhydride and subsequently b) derivatising with a primary or secondary amine and/or alcohol. These graft polymers are suitable as dispersants for inorganic binding agents containing water such as e.g. cement, gypsum, anhydrite.

    摘要翻译: 描述了通过以下方法制备的水溶性接枝聚合物:a)通式I的聚环氧烷的自由基接枝,其中R1 = -H,-CnH2n + 1,-C6H4-CnH2n + 1,< IMAGE> - (CH-R2)mNHR2, - (CH-R2)mOH, - (CH-R2)m -COOH,-CO-R5R2 = -H,-CH3,-C2H5 R3 = -H,-CnH2n + (CH-R2)mOH, - (CH-R2)mOH, - (CH-R2)m-COOH,-CO-R5 R4 = -H, - (CH-R2)m -COOH, -CO-R5 R5 = -CmH2m + 1,-C6H5, - (CH-R2)m-COOH,-C6H4-COOH n表示1-18,m表示1-5,x表示2-200,y表示0或 1与烯键式不饱和单或二羧酸或其酸酐反应,随后b)用伯或仲胺和/或醇衍生。 这些接枝聚合物适合作为含水的无机结合剂的分散剂,例如水。 水泥,石膏,无水石膏。

    Solvent-free polyurethane dispersion
    9.
    发明授权
    Solvent-free polyurethane dispersion 有权
    无溶剂的聚氨酯分散体

    公开(公告)号:US06635723B1

    公开(公告)日:2003-10-21

    申请号:US09623649

    申请日:2000-10-30

    IPC分类号: C08J300

    摘要: A description is given of a solvent-free polyurethane dispersion having a high solids content of polyurethane polymer or fillers, which is obtainable by a) allowing a relatively high molecular weight polyol component (A) (i) and, if desired, a low molecular weight polyol component (A) (ii) to react with a polyisocyanate component (B) in the presence or absence of a catalyst to give a polyurethane preadduct, then b) reacting the polyurethane preadduct from step a) with a low molecular weight and anionically modifiable polyol component (A) (iii) containing two or more hydroxyl groups and one or more carboxyl groups to give the corresponding prepolymer, c) allowing the prepolymer from step b) to react with a neutralization component (C) until the carboxyl groups have been completely or partially neutralized, subsequently or simultaneously d) dispersing the neutralized prepolymer from step c) in water which may further comprise a formulation component (F) comprising fillers, pigments, plasticizers, fibrous materials and other customary additives, subsequently e) reacting the dispersion from step d) with a chain extension component (D), and f) if desired, allowing the dispersion from step e) to react with a chain stopper component (E). The polyurethane dispersion of the invention has an ideal linear segmented structure due to its method of preparation and has extraordinarily high solids contents combined with comparatively low viscosities, complete freedom from solvents, excellent materials properties (e.g. elasticity, elongation and tensile strength) and is prepared by a technically simple process.

    摘要翻译: 给出了具有高固体含量的聚氨酯聚合物或填料的无溶剂聚氨酯分散体的描述,其可通过以下方式获得:a)允许相对高分子量的多元醇组分(A)(i),并且如果需要,可以获得低分子量 多元醇组分(A)(ⅱ)在催化剂存在或不存在下与多异氰酸酯组分(B)反应得到聚氨酯预加成物,然后b)使来自步骤a)的聚氨酯预加合物与低分子量和阴离子可修饰的多元醇 含有两个或多个羟基和一个或多个羧基以得到相应的预聚物的组分(A)(iii),c)使来自步骤b)的预聚物与中和组分(C)反应,直到羧基完全 或部分中和,随后或同时)将中和的预聚物从步骤c)分散在水中,其可以进一步包含配料组分(F),其包含填料,颜料,塑性 使得步骤d)的分散体与链延伸组分(D)反应,和f)如果需要,使步骤e)的分散体与链终止组分(E)反应。 由于其制备方法,本发明的聚氨酯分散体具有理想的线性分段结构,并且具有非常高的固体含量,结合相对低的粘度,完全不含溶剂,优异的材料性能(例如 弹性,伸长率和拉伸强度),并通过技术上简单的工艺制备。

    Hybrid polyurethane-polymer dispersion with high film hardness, method for the production and the use thereof
    10.
    发明授权
    Hybrid polyurethane-polymer dispersion with high film hardness, method for the production and the use thereof 失效
    具有高膜硬度的混合聚氨酯 - 聚合物分散体,其制备方法和用途

    公开(公告)号:US06566438B1

    公开(公告)日:2003-05-20

    申请号:US09787939

    申请日:2001-03-22

    IPC分类号: C08J300

    摘要: Described is a polyurethane/polymer hybrid dispersion with high film hardness, which comprises the reaction components (A) from 3 to 25% by weight of a polyol component consisting of (i) from 2 to 20% by weight of a relatively high molecular mass polyol component, (ii) from 0.5 to 5% by weight of a low molecular mass polyol component, (iii) from 0.5 to 3% by weight of a low molecular mass and anionically modifiable polyol component, (B) from 2 to 20% by weight of a polyisocyanate component, (C) if desired, from 0 to 6% by weight of a solvent component consisting of (i) at least one polyisocyanate-inert organic solvent and/or (ii) a polyisocyanate-inert reactive diluent, (D) from 0.15 to 1.5% by weight of a neutralizing component, (E) from 0.1 to 1% by weight of a chain extender component, (F) from 5 to 40% by weight of a monomer component, (G) from 0.01 to 1.5% by weight of an initiator component, and water as the remainder. The advantages of the polyurethane/polymer hybrid dispersion of the invention, such as high hardness coupled with high flexibility of the crack-free films, good chemical resistance, great stability of the dispersion within a wide pH range, good freeze/thaw stability, and the use of inexpensive raw materials, are achieved in a simplified synthesis route, without subsequence chemical crosslinking, with a simultaneously low organic solvent content (≦4% by weight), and with good filming at temperatures ≦+10° C.

    摘要翻译: 描述了具有高膜硬度的聚氨酯/聚合物混合分散体,其包含3至25重量%的多元醇组分的反应组分(A),其由(i)2至20重量%的较高分子量 多元醇组分,(ii)0.5至5重量%的低分子量多元醇组分,(iii)0.5至3重量%的低分子量和阴离子可修饰的多元醇组分,(B)2至20重量% 重量的多异氰酸酯组分,(C)如果需要,0至6重量%的由(i)至少一种多异氰酸酯惰性有机溶剂和/或(ii)多异氰酸酯惰性反应性稀释剂组成的溶剂组分, (D)0.15〜1.5重量%的中和成分(E)0.1〜1重量%的增链剂成分(F)5〜40重量%的单体成分(G)来自 0.01〜1.5重量%的引发剂组分,余量为水。本发明的聚氨酯/聚合物混合分散体的优点 例如高硬度,无裂纹膜的高柔韧性,良好的耐化学性,在宽的pH范围内的分散体的稳定性,良好的冷冻/融化稳定性和廉价原料的使用,在 简化的合成路线,没有亚序列化学交联,同时低有机溶剂含量(<= 4重量%),并且在<= + 10℃的温度下具有良好的成膜性。