Active material and method of manufacturing active material
    2.
    发明授权
    Active material and method of manufacturing active material 有权
    活性物质的制造方法和活性物质的制造方法

    公开(公告)号:US08821763B2

    公开(公告)日:2014-09-02

    申请号:US12568145

    申请日:2009-09-28

    摘要: An active material capable of forming an electrochemical device excellent in its discharge capacity and rate characteristic is provided. The active material in accordance with a first aspect of the present invention comprises a compound particle containing a compound having a composition represented by the following chemical formula (1), a carbon layer covering the compound particle, and a carbon particle. The active material in accordance with a second aspect of the present invention comprises a carbon particle and a compound particle having an average primary particle size of 0.03 to 1.4 μm, being carried by the carbon particle, and containing a compound represented by the following chemical formula (1): LiaMXO4  (1) where a satisfies 0.9≦a≦2, M denotes one species selected from the group consisting of Fe, Mn, Co, Ni, and VO, and X denotes one species selected from the group consisting of P, Si, S, V, and Ti.

    摘要翻译: 提供能够形成其放电容量和速率特性优异的电化学装置的活性物质。 根据本发明的第一方面的活性材料包含含有具有由以下化学式(1)表示的组成的化合物,覆盖该化合物颗粒的碳层和碳颗粒的化合物颗粒。 根据本发明的第二方面的活性材料包含碳颗粒和平均一次粒径为0.03-1.4μm的由碳颗粒携带的化合物颗粒,并且含有由以下化学式表示的化合物 (1):LiaMXO4(1)其中a满足0.9≦̸ a≦̸ 2,M表示选自Fe,Mn,Co,Ni和VO中的一种,X表示选自以下的一种: P,Si,S,V和Ti。

    Method of manufacturing active material
    4.
    发明授权
    Method of manufacturing active material 有权
    活性物质的制造方法

    公开(公告)号:US08142750B2

    公开(公告)日:2012-03-27

    申请号:US12723041

    申请日:2010-03-12

    IPC分类号: C01B25/30 H01M4/04 H01M4/1395

    摘要: The present invention provides a method of manufacturing an active material which can form an electrochemical device excellent in discharge capacity. The method of manufacturing an active material in accordance with the present invention comprises a hydrothermal synthesis step of heating a mixture including a lithium compound, a metal compound containing one species selected from the group consisting of Fe, Mn, Co, Ni, and V, a phosphorus compound, and water within a reactor while keeping an internal pressure of the reactor at 0.3 MPa or lower by ventilating the inside of the reactor to the outside, and closing the reactor at a time when the temperature of the mixture reaches 100 to 150° C.; and a firing step of firing the mixture after the hydrothermal synthesis step.

    摘要翻译: 本发明提供一种能够形成放电容量优异的电化学装置的活性物质的制造方法。 根据本发明的制备活性材料的方法包括水热合成步骤,其加热包含锂化合物,含有选自Fe,Mn,Co,Ni和V中的一种的金属化合物的混合物, 磷化合物和反应器内的水,同时通过将反应器内部通风到外部将反应器的内部压力保持在0.3MPa或更低,并且在混合物的温度达到100至150℃时关闭反应器 C。; 以及在水热合成步骤之后焙烧该混合物的焙烧步骤。

    Composite magnetic material and process for production
    5.
    发明授权
    Composite magnetic material and process for production 有权
    复合磁性材料及生产工艺

    公开(公告)号:US08999075B2

    公开(公告)日:2015-04-07

    申请号:US13700675

    申请日:2011-06-28

    摘要: A composite magnetic material manufactured by mixing a metal magnetic powder with an insulating binder to produce a mixed powder, press-molding the mixed powder to produce a molded product, and heat-treating the molded product in an oxidizing atmosphere at not lower than 80° C. and not higher than 400° C. to form an oxide film on a surface of the molded product. The metal magnetic powder includes Si, Fe, and component A, and the composition thereof satisfies 5.5%≦Si≦9.5%, 10%≦Si+component A≦13.5%, and the remainder is Fe, where % denotes weight %. The component A includes at least one of Ni, Al, Ti, and Mg.

    摘要翻译: 一种复合磁性材料,其是通过将金属磁性粉末与绝缘粘合剂混合以制造混合粉末,将该混合粉末压制成型以制备成型产品,并在不低于80℃的氧化气氛中对该模制品进行热处理 并且不高于400℃以在模制产品的表面上形成氧化膜。 金属磁性粉末包括Si,Fe和组分A,其组成满足5.5%< NlE; Si&NlE; 9.5%,10%&NlE; Si +组分A& NlE; 13.5%,余量为Fe,其中%表示重量% 。 组分A包括Ni,Al,Ti和Mg中的至少一种。

    BOOM FOR CONSTRUCTION MACHINE
    6.
    发明申请
    BOOM FOR CONSTRUCTION MACHINE 审中-公开
    建筑机械

    公开(公告)号:US20140056677A1

    公开(公告)日:2014-02-27

    申请号:US13994821

    申请日:2011-04-20

    IPC分类号: E02F3/38

    CPC分类号: E02F3/38

    摘要: In left and right web plates (12) of a boom (11), first to fifth web materials (12A to 12E) are joined at edge portions in a front-rear direction along welding lines (13A to 13D). In an upper flange plate (14), a rear upper flange material (14A), a front upper flange material (14B), and a middle upper flange material (14C) are joined at edge portions in a front-rear direction along welding lines (15A, 15B). Ina lower flange plate (16), first to sixth lower flange materials (16A to 16F) are joined at edge portions in a front-rear direction along welding lines (17A to 17E). The welding lines (13A to 13D) of the left and right web plates (12) are disposed in positions that are different from those of the welding lines (15A, 15B) of the upper flange plate (14) and the welding lines (17A to 17E) of the lower flange plate (16) in a front-rear direction. This makes it possible to reduce the entire weight and thereby achieve reduction in weight while ensuring bending strength, torsional strength, and the like of the boom (11).

    摘要翻译: 在悬臂(11)的左右腹板(12)中,第一至第五腹板材料(12A至12E)沿着焊接线(13A至13D)沿前后方向的边缘部分接合。 在上法兰板(14)中,沿着焊接线的前后方向的边缘部分接合有后上凸缘材料(14A),前上凸缘材料(14B)和中上凸缘材料(14C) (15A,15B)。 下凸缘板(16),第一至第六下凸缘材料(16A至16F)沿焊接线(17A至17E)沿前后方向的边缘部分接合。 左和右腹板(12)的焊接线(13A〜13D)配置在与上部法兰板(14)的焊接线(15A,15B)和焊接线(17A)的位置不同的位置 至17E)的前后方向。 由此,能够减轻整体重量,能够实现起重臂(11)的弯曲强度,扭转强度等的减轻。

    Engine
    7.
    发明授权
    Engine 有权
    发动机

    公开(公告)号:US08646270B2

    公开(公告)日:2014-02-11

    申请号:US13059209

    申请日:2009-06-11

    IPC分类号: F02D23/00 F02B33/44 F02B33/00

    摘要: Turbines and compressors, which constitute superchargers, are disposed in series on an exhaust gas passage and an air intake passage, respectively. The supercharger is equipped with a supercharger rotation sensor, which transmits a detection signal obtained according to the rotation of the compressor to a control device, a bypass passage, which bypasses exhaust gas from the upstream side to the downstream side of the turbine, and a bypass valve, which regulates the flow rate of exhaust gas flowing through the bypass passage. Control device regulates the rotational speed of the compressors in a high-efficiency range by producing a control signal based on the detection signal from the supercharger rotation sensor, and sending the control signal to the bypass valve.

    摘要翻译: 构成增压器的涡轮机和压缩机分别串联设置在排气通道和进气通道上。 增压器配备有增压器旋转传感器,其将根据压缩机的旋转获得的检测信号传递到控制装置,旁路通路,旁路通路从涡轮机的上游侧到下游侧旁路排气, 旁通阀,其调节流过旁路通道的废气的流量。 控制装置通过基于来自增压器旋转传感器的检测信号产生控制信号,并将控制信号发送到旁通阀,来调节压缩机在高效率范围内的转速。

    ARM FOR CONSTRUCTION MACHINE
    8.
    发明申请
    ARM FOR CONSTRUCTION MACHINE 有权
    建筑机械用臂

    公开(公告)号:US20140010624A1

    公开(公告)日:2014-01-09

    申请号:US14003341

    申请日:2012-05-16

    IPC分类号: E02F3/38

    CPC分类号: E02F3/38

    摘要: An arm of a hydraulic excavator is formed as a box-shaped structural body surrounded by left and right side plates, an upper plate joined to each of the upper end sides of each side plate, a lower plate joined to each of the lower end sides of each side plate, and a thick rear plate joined to each of the rear end sides of each side plate and the upper plate. The side plates are formed by joining a rear thick side plate and a front thin side plate. The upper plate is formed by joining two members, that is, a rear thick upper plate and a front thin upper plate, and the lower plate is formed by joining two members, that is, a rear thick lower plate and a front thin lower plate.

    摘要翻译: 液压挖掘机的臂形成为由左右侧板围绕的箱状结构体,与各侧板的上端侧连接的上板,与各下端侧连接的下板 并且连接到每个侧板和上板的每个后端侧的厚的后板。 侧板通过连接后厚侧板和前薄侧板而形成。 上板通过连接两个构件,即后厚的上板和前薄的上板形成,并且下板通过将两个构件,即后厚的下板和前薄的下板 。

    COMPOSITE MAGNETIC MATERIAL
    9.
    发明申请
    COMPOSITE MAGNETIC MATERIAL 有权
    复合磁性材料

    公开(公告)号:US20120007013A1

    公开(公告)日:2012-01-12

    申请号:US13203271

    申请日:2010-03-24

    IPC分类号: H01F1/047 H01F1/04

    摘要: A composite magnetic material is made by performing pressure compacting on metal magnetic powder to which a binding material is added, and the binding material contains an acrylic resin having a silyl group as a functional group. In addition, the composite magnetic material is subjected to a heat treatment at a temperature between 700 and 1,000° C. in a non-oxidizing atmosphere after the pressure compacting. The composite magnetic material has magnetic characteristics useful for electromagnetic components such as an inductor, a choke coil, and a transformer with a small size and at a high frequency.