摘要:
A process for the surface treatment of moldings based on liquid crystalline polymers with acidic or alkaline reagents includes using the reagents in a solvent which is an organic solvent to an extent of not less than 60% by weight.
摘要:
A thermoplastic molding material based onA) from 2 to 97.5% w/w of a homopolymer or copolymer of polyoxymethyleneB) from 2 to 97.5% w/w of a polyamideC) from 0.5 to 25% w/w of a polycondensate of 2,2-di(4-hydroxyphenyl)propane and epichlorohydrinD) from 0 to 60% w/w of an impact modifier, andE) from 0 to 60% w/w of fibrous or particulate fillers or mixtures thereof.
摘要:
Moldings based on polyamides are surface treated with mixtures of at least 20% strength by weight aqueous hydrochloric acid with mono- or diethers of an aliphatic polyfunctional hydroxy compound in a mixing ratio of from 90:10 to 10:90% by volume.
摘要:
Thermoplastic molding materials preparedA) from 35 to 99.5% by weight of a matrix copolymer (A) ofa.sub.1) from 50 to 95% by weight of styrene and/or .alpha.-methylstyrene,a.sub.2) from 5 to 50% by weight of acrylonitrile anda.sub.3) from 0 to 20% by weight of further comonomersB) from 0 to 50% by weight of a particulate graft copolymer (B) which is insoluble in (A), has a median particle diameter of from 0.03 to 1 .mu.m and preparedb.sub.1) from 30 to 80% by weight of a core comprising an elastomeric polymer having a glass transition temperature of less than -10.degree. C. andb.sub.2) from 20 to 70% by weight of a graft shell comprising a polymer which is compatible or partly compatible with (A)andC) from 0.5 to 30% by weight of a particulate crosslinked copolymer (C) which is insoluble in (A), has a median particle diameter of from 0.5 to 50 .mu.m and comprisesc.sub.1) from 50 to 89.95% by weight of styrene and/or .alpha.-methylstyrene,c.sub.2) from 10 to 50% by weight of acrylonitrile,c.sub.3) from 0.05 to 5% by weight of a polyfunctional, crosslinking monomer,c.sub.4) from 0 to 10% by weight of a monomer which contains acidic or basic groups andc.sub.5) from 0 to 20% by weight of further comonomers.
摘要:
Impact-resistant thermoplastic polyester molding materials are prepared by thoroughly mixingA. from 52 to 99 parts by weight of a melt of one or more polyalkylene terephthalates withB. from 1 to 48 parts by weight of one or more elastomeric graft polymers prepared by emulsion polymerization and composed of1. from 70 to 90% by weight of a grafting base consisting of elastomeric polymers having a gel content of not less than 80% and a glass transition temperature Tg of less than -20.degree. C. and2. from 10 to 30% by weight of a grafted shell consisting of one or more polymers having a glass transition temperature Tg greater than 40.degree. C.,in the form of an aqueous dispersion in which not less than 80% of the particles of graft polymer B have a size of from 0.05 to 0.15 .mu.m, with simultaneous removal of the water which vaporizes.
摘要:
A process for the preparation of finely divided acicular hexagonal ferrites which have a high coercive force and are of the general formula MFe.sub.12 O.sub.19, where M is barium or strontium, and their use for the production of magnetic recording media and plastoferrites.
摘要:
A thermoplastic molding composition composed of, based on the total of A, B, C and D,40-95% by weight of a copolymer A of, based on A,90-95% by weight of styrene and/or its derivatives and 10-50% by weight of acrylonitrile, optionally up to 50% by weight of a graft copolymer B of 20-80% by weight of a monomer mixture of either styrene/acrylonitrile in the ration from 9:1 to 4:6 or styrene/acrylonitrile/methylacrylate in the ration from 19:1:1 to 8:6:6 onto 80-20% by weight of an elastomer based on butadiene or acrylic ester as grafting base, graft copolymerization being effected in either emulsion or solution, 1-50% by weight of a reinforcing glass fiber material C and 0.1-50% by weight of a terpolymer D of styrene, methyl methacrylate and maleic anhydride composed of 1-15% by weight each of styrene and maleic anhydride and a styrene/maleic anhydride ratio of from 5:1 to 1:5, and methyl methacrylate.
摘要:
The flameproofing agent content of molding compositions containing polyesters (a.sub.1), acrylate graft polymers (a.sub.2), styrene/acrylonitrile copolymers (a.sub.3) and glass fibers can be reduced without affecting the flame resistance by adding finely divided PTFE.
摘要:
Thermoplastic molding materials contain, as essential components,(A) from 10 to 89.99% by weight of a polyester,(B) from 10 to 89.99% by weight of a polycarbonate and(C.sub.1) from 0.01 to 1% by weight of a low molecular weight organic compound of not more than 70 carbon atoms which contains (--SO.sub.3).sub.m Q groups where Q is hydrogen, NH.sub.4 or an alkali or alkaline earth metal and m is an integer equal to the valency of Q, and/or(C.sub.2) from 0.01 to 30% by weight of a polymer containing sulfo groups and having a weight average molecular weight of not less than 1000,and, as a further component,(D) from 0 to 30% by weight of a rubber impact modifier.
摘要:
Fireproofed thermoplastic molding materials which contain red phosphorus as a flame-proofing agent are obtainable by mixing(A) from 5 to 95% by weight of a polyamide or of a polyester or of a mixture of these,(B) from 5 to 95% by weight of an elastomer dispersion containing, as essential components,(b.sub.1) from 5 to 75% by weight of an elastomer prepared by emulsion polymerization,(b.sub.2) from 10 to 70% by weight of red phosphorus, p2 (b.sub.3) from 10 to 80% by weight of water and(b.sub.4) from 0.1 to 5% by weight of dispersant, and(C) from 0 to 60% by weight of fibrous or particulate fillers or a mixture of these,the total content of red phosphorus in the molding material being from 3 to 20% by weight, based on the total weight of the molding material, and the elastomer composition being introduced into a melt of the polyamide or of the polyester or of a mixture of these.