OXIDATIVE DESULFURIZATION OF FUEL OIL
    7.
    发明申请
    OXIDATIVE DESULFURIZATION OF FUEL OIL 审中-公开
    燃油的氧化除油

    公开(公告)号:US20090242460A1

    公开(公告)日:2009-10-01

    申请号:US12055901

    申请日:2008-03-26

    IPC分类号: C10G45/04

    摘要: A method for purifying a sulfur-containing fuel oil comprising (a) contacting the fuel oil with a supported exogenous binary catalyst and oxygen at a temperature in a range of from about 25° C. to about 150° C., and at a pressure in a range of from about 1 atmosphere to about 150 atmospheres to provide a first oxidized mixture; and (b) separating at least one oxidized sulfur compound from the first oxidized mixture to a provide a purified fuel oil. In one embodiment, the sulfur-containing fuel oil is deasphalted prior to contacting with the supported exogenous binary catalyst and oxygen.

    摘要翻译: 一种用于纯化含硫燃料油的方法,包括(a)在约25℃至约150℃的温度和压力下使燃料油与负载的外源二元催化剂和氧接触 在约1大气压至约150大气压的范围内,以提供第一氧化混合物; 和(b)将至少一种氧化的硫化合物从第一氧化混合物中分离出来提供纯化的燃料油。 在一个实施方案中,含硫燃料油在与负载的外源二元催化剂和氧接触之前脱沥青。

    COMPOSITION AND ENERGY STORAGE DEVICE
    8.
    发明申请
    COMPOSITION AND ENERGY STORAGE DEVICE 有权
    组合物和能源储存装置

    公开(公告)号:US20120077070A1

    公开(公告)日:2012-03-29

    申请号:US12893661

    申请日:2010-09-29

    IPC分类号: H01M10/02 H01M2/18 H01M10/26

    摘要: A cathode composition is provided. The cathode composition includes at least one electroactive metal, wherein the electroactive metal is at least one selected from the group consisting of titanium, vanadium, niobium, molybdenum, nickel, iron, cobalt, chromium, manganese, silver, antimony, cadmium, tin, lead and zinc; a first alkali metal halide; an electrolyte salt comprising a reaction product of a second alkali metal halide and a metal halide, wherein the electrolyte salt has a melting point of less than about 300 degrees Centigrade; and a metal chlorosulfide compound having a formula (I) M1M2p+1SnCl4+3p-2n wherein “M1” is a metal selected from group IA of the periodic table, “M2” is a metal selected from group IIIA of the periodic table, “p” is 0 or 1, and “n” is equal to or greater than 0.5. An article and an energy storage device comprising the cathode composition is provided. A method of forming the energy storage device is provided.

    摘要翻译: 提供阴极组合物。 阴极组合物包括至少一种电活性金属,其中电活性金属是选自钛,钒,铌,钼,镍,铁,钴,铬,锰,银,锑,镉,锡, 铅锌 第一碱金属卤化物; 电解质盐,其包含第二碱金属卤化物和金属卤化物的反应产物,其中所述电解质盐的熔点小于约300摄氏度; 和具有式(I)M1M2p + 1SnCl4 + 3p-2n的金属氯化硫化物,其中“M1”是选自元素周期表的IA族的金属,“M2”是选自元素周期表IIIA族的金属, p“为0或1,”n“等于或大于0.5。 提供了一种包含阴极组合物的制品和储能装置。 提供一种形成能量存储装置的方法。

    Methods for preparing compositions which comprise magnesium borohydride, and related materials
    10.
    发明授权
    Methods for preparing compositions which comprise magnesium borohydride, and related materials 有权
    制备包含硼氢化镁的组合物的方法及相关材料

    公开(公告)号:US07906092B2

    公开(公告)日:2011-03-15

    申请号:US11767067

    申请日:2007-06-22

    IPC分类号: C01B6/13

    CPC分类号: C01B3/04 C01B6/21 Y02E60/364

    摘要: Disclosed herein is a method for preparing magnesium borohydride. The method includes the step of reacting a metal borohydride with a metal salt composition in a solvent, to form a reaction mixture. The metal salt composition comprises at least one magnesium salt. The metal borohydride and the metal salt composition are insoluble in the solvent. The method further includes the step of grinding the reaction mixture to produce a composition that includes magnesium borohydride; and removing the solvent from the composition. Another embodiment of this invention relates to a new material. The material is an orthorhombic crystal phase of magnesium borohydride.

    摘要翻译: 本文公开了一种制备硼氢化镁的方法。 该方法包括使金属硼氢化物与金属盐组合物在溶剂中反应以形成反应混合物的步骤。 金属盐组合物包含至少一种镁盐。 金属硼氢化物和金属盐组合物不溶于溶剂。 该方法还包括研磨反应混合物以产生包括硼氢化镁的组合物的步骤; 并从组合物中除去溶剂。 本发明的另一个实施例涉及一种新的材料。 该材料是硼氢化镁的斜方晶相。