摘要:
A thermoplastic film including a microporous polymeric membrane; and a non-woven web comprising a plurality of fibers, the web being bonded to the microporous polymeric membrane, wherein the fibers comprise oxidation-protective polymer having an MFR ≧2.0×102.
摘要:
A thermoplastic film including a microporous polymeric membrane; and a non-woven web bonded to the polymeric microporous membrane, wherein the web comprises a plurality of fibers comprising polyolefin having a Tm≧85.0° C. and a Te-Tm≦10.0° C.
摘要:
Disclosed herein is a nonwoven fabric comprising within the range of from 1 to 49 wt %, by weight of the fabric, of a reactor grade propylene-α-olefin copolymer possessing; within the range of from 5 to 35 wt %, by weight of the copolymer, of units derived from one or more of ethylene and/or C4 to C12 α-olefins; a melt flow rate (230° C./2.16 kg) within the range of from 600 to 7500 g/10 min; and a weight average molecular weight of less than 200,000; and a second polypropylene having a melting point, Tm, of greater than 110° C. and a melt flow rate (230° C./2.16 kg) within the range of from 20 to 7500 g/10 min; wherein the fabric has a Handle value of less than 60% (measuring the fabric of 35 g/m2 basis weight). The fabric can be used in structures comprising one or more layers of the fabric described herein, and can include any number of other fabric layers made from other materials.
摘要:
Disclosed herein is a nonwoven fabric comprising within the range of from 50 to 99 wt %, by weight of the composition, of a reactor grade propylene-α-olefin copolymer possessing within the range of from 5 to 35 wt %, by weight of the copolymer, of units derived from one or more of ethylene and/or C4 to C12 α-olefins; a melt flow rate (230° C./2.16 kg) within the range of from 500 to 7500 g/10 min; and a weight average molecular weight of less than 200,000; and a second polypropylene having a melting point, Tm, of greater than 110° C. and a melt flow rate (230° C./2.16 kg) within the range of from 20 to 7500 g/10 min; wherein the fabric has a CD Elongation value of greater than 50% (measuring the fabric of 35 g/m2 basis weight). The fabric described herein can be used in structures comprising one or more layers of the fabric described herein, and can include any number of other fabric layers made from other materials.
摘要:
Disclosed herein is a nonwoven fabric comprising within the range of from 50 to 99 wt %, by weight of the composition, of a reactor grade propylene-α-olefin copolymer possessing within the range of from 5 to 35 wt %, by weight of the copolymer, of units derived from one or more of ethylene and/or C4 to C12 α-olefins; a melt flow rate (230° C./2.16 kg) within the range of from 500 to 7500 g/10 min; and a weight average molecular weight of less than 200,000; and a second polypropylene having a melting point, Tm, of greater than 110° C. and a melt flow rate (230° C./2.16 kg) within the range of from 20 to 7500 g/10 min; wherein the fabric has a CD Elongation value of greater than 50% (measuring the fabric of 35 g/m2 basis weight). The fabric described herein can be used in structures comprising one or more layers of the fabric described herein, and can include any number of other fabric layers made from other materials.
摘要:
Disclosed herein is a nonwoven fabric comprising within the range of from 50 to 99 wt %, by weight of the composition, of a reactor grade propylene-α-olefin copolymer possessing within the range of from 5 to 35 wt %, by weight of the copolymer, of units derived from one or more of ethylene and/or C4 to C12 α-olefins; a melt flow rate (230° C./2.16 kg) within the range of from 500 to 7500 g/10 min; and a weight average molecular weight of less than 200,000; and a second polypropylene having a melting point, Tm, of greater than 110° C. and a melt flow rate (230° C./2.16 kg) within the range of from 20 to 7500 g/10 min; wherein the fabric has a CD Elongation value of greater than 50% (measuring the fabric of 35 g/m2 basis weight). The fabric described herein can be used in structures comprising one or more layers of the fabric described herein, and can include any number of other fabric layers made from other materials.
摘要:
Low molecular weight semicrystalline propylene-alpha olefin copolymers containing propylene crystallinity are used as a nucleating agent in crystalline polypropylene and polypropylene copolymers. The nucleating copolymers are propylene-alpha olefin copolymers having a percent crystallinity of 5-75%, a melting point of 45° C.-105° C., and an MFR between 300 and 5000 g/10 min. Nucleated polypropylene compositions comprise a nucleating amount of the copolymer blended in a matrix of polypropylene homopolymer, or 0.01 to 9 wt % α-olefin copolymer, having a melting point greater than 110° C. The nucleating copolymer improves processing time with little or no effect on the crystallinity-associated characteristics of the matrix. The invention also provides methods of crystallizing polypropylene with the nucleating agent and of forming articles with the composition, and also provides articles formed from the composition and/or by the method.
摘要:
Low molecular weight semicrystalline propylene-alpha olefin copolymers containing propylene crystallinity are used as a nucleating agent in crystalline polypropylene and polypropylene copolymers. The nucleating copolymers are propylene-alpha olefin copolymers having a percent crystallinity of 5-75%, a melting point of 45° C.-105° C., and an MFR between 300 and 5000 g/10 min. Nucleated polypropylene compositions comprise a nucleating amount of the copolymer blended in a matrix of polypropylene homopolymer, or 0.01 to 9 wt % α-olefin copolymer, having a melting point greater than 110° C. The nucleating copolymer improves processing time with little or no effect on the crystallinity-associated characteristics of the matrix. The invention also provides methods of crystallizing polypropylene with the nucleating agent and of forming articles with the composition, and also provides articles formed from the composition and/or by the method.