Polyether-acetal polyol compositions

    公开(公告)号:US10435502B2

    公开(公告)日:2019-10-08

    申请号:US15542323

    申请日:2016-01-08

    摘要: Embodiments of the present disclosure are directed to polyether-acetal polyol compositions, more particularly to polyol compositions including a polyether-acetal polyol that can be utilized to form polyurethanes. As an example, a polyurethane formulation can include a polyol composition including a polyether-acetal polyol functionalized with at least one acetal functional group, where the polyol composition has an average hydroxyl functionality from 2 to 8 and a hydroxyl equivalent weight from 150 to 4000, where the portion of the polyether-acetal polyol that is functionalized with the at least one acetal functional group is 1 percent to 40 percent of a total weight of the polyether-acetal polyol, where the polyether-acetal polyol has a primary hydroxyl group content of at least 55 percent, and a polyisocyanate, where the polyurethane formulation has an isocyanate index in a range from 70 to 500.

    Dual catalyst system for high primary hydroxyl polyols

    公开(公告)号:US09896542B2

    公开(公告)日:2018-02-20

    申请号:US15504368

    申请日:2015-10-19

    IPC分类号: C08G65/26

    摘要: A method of producing a high primary hydroxyl group content and a high number average molecular weight polyol includes preparing a mixture that includes a double metal cyanide catalyst and a low molecular weight polyether polyol having a number average molecular weight of less than 1,000 g/mol, the polyether polyol is derived from propylene oxide, ethylene oxide, or butylene oxide, setting the mixture to having a first temperature, adding at least one selected from propylene oxide, ethylene oxide, and butylene oxide to the mixture at the first temperature, allowing the mixture to react to form a reacted mixture, adding a Lewis acid catalyst to the reacted mixture, setting the reaction mixture including the second catalyst to have a second temperature that is less than the first temperature, and adding additional at least one selected from propylene oxide, ethylene oxide, and butylene oxide to the reacted mixture at the second temperature such that a resultant polyol having a primary hydroxyl group content of at least 60% and a number average molecular weight greater than 2,500 g/mol is formed.