摘要:
Compounds of the formula I ##STR1## where R is a polyethylene glycol radical of 3 to 60 chain members or a polypropylene glycol radical of 3 to 60 chain members or the radical of an ethylene oxide/propylene oxide block polymer of average molecular weight from 300 to 8,500, and R' is straight-chain or branched alkyl of 1 to 10 carbon atoms, or benzyl.
摘要:
##STR1## where the individual radicals R are identical or different and are each hydrogen, an alkali metal, or ammonium which is unsubstituted or substituted by organic radicals, or are each C 1 -C 20 -alkyl or a polyoxyethylene radical which contains from 1 to 10 ethylene oxide units and whose terminal OH group may be etherified by an alcohol of 1 to 3 carbon atoms, are used as sun screen agents.
摘要:
Compounds of the formula I ##STR1## where the individual radicals R are identical or different and are each hydrogen, an alkali metal, or ammonium which is unsubstituted or substituted by organic radicals, or are each C.sub.1 -C.sub.20 -alkyl or a polyoxyethylene radical which contains from 1 to 10 ethylene oxide units and whose terminal OH group may be etherified by an alcohol of 1 to 3 carbon atoms, are used as sun screen agents.
摘要:
A process for the preparation of high-viscosity polyvinylpyrrolidone, wherein an aqueous polyvinylpyrrolidone solution is subjected to a heat treatment in the presence of a water-insoluble peroxide and in the absence of oxygen, and thickeners containing the polyvinylpyrrolidone thus prepared.
摘要:
A process for the preparation of high-viscosity polyvinylpyrrolidone, wherein an aqueous polyvinylpyrrolidone solution is subjected to a heat treatment in the presence of a water-insoluble peroxide and in the absence of oxygen, and thickeners containing the polyvinylpyrrolidone thus prepared.
摘要:
A molding material comprises styrene/butadiene block copolymers obtainable by anionic polymerization and from 0.01 to 1% by weight, based on the polymer, of .alpha.-tocopherol.
摘要:
Elastomeric block copolymers comprising at least one hard block A composed of styrene monomers and at least one elastomeric block (B/A) composed of styrene monomers and dienes, the glass transition temperature Tg of the block A being more than 25° C. and that of block (B/A) being less than 25° C. and the phase volume ratio of block A to block (B/A) being chosen so that the proportion of the hard phase in the total block copolymer is from 1 to 40% by volume and the amount by weight of the diene is less than 50% by weight, and the relative proportion of 1,2 linkages of the polydiene, based on the sum of 1,2- and 1,4-cis/trans linkages, being below 15%, are prepared by anionic polymerization by means of a lithium alkyl in a nonpolar solvent in the presence of a soluble potassium salt and are used for the production of shaped articles.
摘要:
Dicyclohexylalkanes, their preparation, cosmetic and pharmaceutical formulations containing these compounds, and their use in these formulations as oil components for cosmetic and pharmaceutical purposes.
摘要:
The invention relates to thermoplastic moulded masses containing, a) at least one block copolymer (A), comprising, with relation to (A), a1) 50 to 90 wt. % of at least one styrol monomer, a2) 10 to 50 wt. % of at least one diene monomer, with the following as stabilisers, relative to the moulded mass, b) 0.001 to 0.18 wt. % of at least one benzofuranone derivative (B), c) 0.05 to 1 wt. % of at least one organic phosphite (C), and d) 0.1 to 0.3 wt. % of at least one stabiliser compound (D), selected from sterically hindered phenols and aromatic amines.