Method for producing rare earth alloy magnet powder
    2.
    发明授权
    Method for producing rare earth alloy magnet powder 失效
    稀土合金磁粉的制造方法

    公开(公告)号:US5417773A

    公开(公告)日:1995-05-23

    申请号:US319465

    申请日:1994-10-06

    CPC分类号: H01F1/0573 B22F9/023

    摘要: The present invention provides a method for producing a rare earth alloy magnet powder exhibiting stable and superior magnetic properties using hydrogenation followed by dehydrogenation. In a method for producing a rare earth alloy magnet powder wherein a homogenized rare earth alloy magnet alloy material is subjected to hydrogenation at a temperature in a range between 750.degree. C. and 950.degree. C., followed by dehydrogenation at a temperature in a range between 750.degree. C. and 950.degree. C.; cooled; and crushed, both the hydrogenation and the dehydrogenation are carried out in a vacuum tube furnace; and the alloy material in the dehydrogenation step maintains a temperature drop of at most 50.degree. C. due to an endothermic reaction which occurs during the dehydrogenation step.

    摘要翻译: 本发明提供一种稀土合金磁粉的制造方法,其特征在于,使用氢化脱氢后表现出稳定而优异的磁性能。 在稀土合金磁铁粉末的制造方法中,在750〜950℃的温度范围内使均质化的稀土类合金磁铁合金材料进行氢化,然后在一定范围的温度下脱氢 在750℃和950℃之间。 冷却 粉碎,氢化和脱氢均在真空管式炉中进行; 并且脱氢步骤中的合金材料由于在脱氢步骤期间发生的吸热反应而保持至多50℃的温度下降。

    Cu-BASED SINTERED SLIDING MEMBER
    3.
    发明申请
    Cu-BASED SINTERED SLIDING MEMBER 审中-公开
    基于Cu的烧结滑动构件

    公开(公告)号:US20120145284A1

    公开(公告)日:2012-06-14

    申请号:US13390883

    申请日:2010-08-27

    IPC分类号: C22C9/06

    摘要: A Cu-based sintered sliding member that can be used under high-load conditions. The sliding member is age-hardened, including 5 to 30 mass % Ni, 5 to 20 mass % Sn, 0.1 to 1.2 mass % P, and the rest including Cu and unavoidable impurities. In the sliding member, an alloy phase containing higher concentrations of Ni, P and Sn than their average concentrations in the whole part of the sliding member, is allowed to be present in a grain boundary of a metallic texture, thereby achieving excellent wear resistance. Hence, without needing expensive hard particles, there can be obtained, at low cost, a Cu-based sintered sliding member usable under high-load conditions. Even more excellent wear resistance is achieved by containing 0.3 to 10 mass % of at least one solid lubricant selected from among graphite, graphite fluoride, molybdenum disulfide, tungsten disulfide, boron nitride, calcium fluoride, talc and magnesium silicate mineral powders.

    摘要翻译: 可在高负荷条件下使用的Cu基烧结滑动件。 滑动构件经时效硬化,其中包括5至30质量%的Ni,5至20质量%的Sn,0.1至1.2质量%的P,其余包括Cu和不可避免的杂质。 在滑动构件中,允许在金属组织的晶界中存在Ni,P和Sn的含量高于其在滑动构件的整个部分中的平均浓度的合金相,从而获得优异的耐磨性。 因此,在不需要昂贵的硬质颗粒的情况下,可以以低成本获得可在高负载条件下使用的Cu系烧结滑动构件。 通过含有0.3〜10质量%的选自石墨,氟化石墨,二硫化钼,二硫化钨,氮化硼,氟化钙,滑石粉和硅酸镁矿物粉末中的至少一种固体润滑剂,可以获得更优异的耐磨性。

    Iron-based sintered alloy, iron base sintered alloy member, method for production thereof, and oil pump rotor
    6.
    发明申请
    Iron-based sintered alloy, iron base sintered alloy member, method for production thereof, and oil pump rotor 审中-公开
    铁基烧结合金,铁基烧结合金部件,其制造方法以及油泵转子

    公开(公告)号:US20060099079A1

    公开(公告)日:2006-05-11

    申请号:US10541308

    申请日:2003-10-20

    IPC分类号: F03B3/12 B63H1/26

    摘要: An iron-based sintered alloy member having a composition consisting of 0.5 to 7% by mass of Cu, 0.1 to 0.98% by mass of C, 0.02 to 0.3% by mass of oxygen and, optionally, 0.0025 to 1.05% by mass of Mn and/or 0.001 to 0.7% by mass of Zn, and the balance of Fe and inevitable impurities is manufactured by formulating an Fe powder, a graphite powder and a Cu alloy powder, as raw powders, mixing the powders to form a powder mixture, forming the powder mixture into a green compact and sintering the green compact. The Cu alloy powder has a composition consisting of 1 to 10% by mass of Fe, 0.2 to 1% by mass of oxygen and, optionally, 0.2 to 10% by mass of Zn and/or 0.5 to 15% by mass of Mn, and the balance of Cu and inevitable impurities.

    摘要翻译: 一种铁基烧结合金构件,其组成为:Cu:0.5〜7质量%,C:0.1〜0.98质量%,氧0.02〜0.3质量%,Mn:0.0025〜1.05质量% 和/或0.001〜0.7质量%的Zn,其余的Fe和不可避免的杂质通过配制Fe粉末,石墨粉末和Cu合金粉末作为原料粉末制成,将粉末混合形成粉末混合物, 将粉末混合物形成生坯并烧结生坯。 Cu合金粉末的组成为:Fe:1〜10质量%,0.2〜1质量%的氧,0.2〜10质量%的Zn和/或0.5〜15质量%的Mn, 余量为Cu和不可避免的杂质。

    SINTERED BEARING FOR MOTOR-POWERED FUEL INJECTION PUMPS
    7.
    发明申请
    SINTERED BEARING FOR MOTOR-POWERED FUEL INJECTION PUMPS 有权
    用于电动燃油喷射泵的烧结轴承

    公开(公告)号:US20130189150A1

    公开(公告)日:2013-07-25

    申请号:US13876084

    申请日:2011-11-07

    IPC分类号: C22C9/06 C22C9/02

    摘要: There is provided a bearing for motor-powered fuel injection pumps, made from Cu—Ni-based sintered alloy, which is able to be obtained at a low cost, having excellent corrosion and abrasion resistances. The bearing contains 10 to 20% by mass of Ni, 5 to 13% by mass of Sn, 0.1 to 0.8% by mass of P, 1 to 6% by mass of C, and a remainder containing Cu and inevitable impurities, and is formed with a Ni—Sn—Cu—P phase containing at least 30% by mass of Sn in a grain boundary, and has a 8 to 18% porosity. The Ni—Sn—Cu—P phase contains 30 to 49% by mass of Ni, 10 to 30% by mass of Cu, 0.5 to 1.5% by mass of P, and a remainder containing Sn and inevitable impurities.

    摘要翻译: 提供了一种由Cu-Ni系烧结合金制成的电动燃油喷射泵的轴承,其能够以低成本获得,具有优良的耐腐蚀和耐磨性。 该轴承含有10〜20质量%的Ni,5〜13质量%的Sn,0.1〜0.8质量%的P,1〜6质量%的C,剩余部分含有Cu和不可避免的杂质,并且 由在晶界中含有至少30质量%的Sn的Ni-Sn-Cu-P相形成,并且具有8〜18%的孔隙率。 Ni-Sn-Cu-P相含有30〜49质量%的Ni,10〜30质量%的Cu,0.5〜1.5质量%的P,余量含有Sn和不可避免的杂质。

    Cu-based oil-impregnated sintered bearing
    8.
    发明授权
    Cu-based oil-impregnated sintered bearing 有权
    铜基浸油烧结轴承

    公开(公告)号:US09476453B2

    公开(公告)日:2016-10-25

    申请号:US13882595

    申请日:2011-11-07

    摘要: There is provided a Cu-based oil-impregnated sintered bearing which can be used for high-load applications such as an ABS system and a wiper motor system in automobile, can be manufactured at low cost, and is excellent in abrasion resistance and seizure resistance. The bearing contains 5 to 40% by mass of Ni, 3 to 15% by mass of Sn, 0.5 to 4.0% by mass of P, or further 0.3 to 5.0% by mass of a solid lubricant, and a remainder comprising Cu and inevitable impurities, and has a metallic structure in which a phase mainly composed of Ni and P is dispersed in a matrix, and has a 5 to 25% porosity.

    摘要翻译: 提供了可用于汽车中的ABS系统和刮水器马达系统等高负荷应用的Cu系油浸烧结轴承,可以低成本地制造,耐磨损性和耐发泡性优异 。 该轴承含有5〜40质量%的Ni,3〜15质量%的Sn,0.5〜4.0质量%的P,或者还有0.3〜5.0质量%的固体润滑剂,余量包含Cu和不可避免的 并且具有其中主要由Ni和P组成的相分散在基质中并具有5至25%孔隙率的金属结构。

    Cu-BASED OIL-IMPREGNATED SINTERED BEARING
    9.
    发明申请
    Cu-BASED OIL-IMPREGNATED SINTERED BEARING 有权
    基于铜的油浸铸造轴承

    公开(公告)号:US20130223774A1

    公开(公告)日:2013-08-29

    申请号:US13882595

    申请日:2011-11-07

    IPC分类号: F16C33/10

    摘要: There is provided a Cu-based oil-impregnated sintered bearing which can be used for high-load applications such as an ABS system and a wiper motor system in automobile, can be manufactured at low cost, and is excellent in abrasion resistance and seizure resistance. The bearing contains 5 to 40% by mass of Ni, 3 to 15% by mass of Sn, 0.5 to 4.0% by mass of P, or further 0.3 to 5.0% by mass of a solid lubricant, and a remainder comprising Cu and inevitable impurities, and has a metallic structure in which a phase mainly composed of Ni and P is dispersed in a matrix, and has a 5 to 25% porosity.

    摘要翻译: 提供了可用于汽车中的ABS系统和刮水器马达系统等高负荷应用的Cu系油浸烧结轴承,可以低成本地制造,耐磨损性和耐发泡性优异 。 该轴承含有5〜40质量%的Ni,3〜15质量%的Sn,0.5〜4.0质量%的P,或者还有0.3〜5.0质量%的固体润滑剂,余量包含Cu和不可避免的 并且具有其中主要由Ni和P组成的相分散在基质中并具有5至25%孔隙率的金属结构。