摘要:
An abrasion-resistant fluoropolymer mixture comprising(A) from 75 to 99% by weight of a fluorocarbon polymer(B) from 1 to 25% by weight of an oxidized polyarylene sulfide and, based on the sum (A)+(B),(C) from 0 to 15% by weight of a filler,is used for the production of feed pipes for Bowden cables which are pressure-resistant and abrasion-resistant.
摘要:
An abrasion-resistant fluoropolymer mixture comprising (A) from 75 to 99% by weight of a fluorocarbon polymer (B) from 1 to 25% by weight of an oxidized polyarylene sulfide and, based on the sum (A)+(B), (C) from 0 to 15% by weight of a filler, is used for the production of feed pipes for Bowden cables which are pressure-resistant and abrasion-resistant.
摘要:
Mixtures of fluoropolymers and oxidized polyarylene sulfides A polymer mixture of A) at least one fluoropolymer in a proportion of from 50 to 99% by weight and B) at least one polyarylene sulfone or polyarylene compound containing at least two of the bridges --S--, --SO-- and --SO.sub.2 -- or a mixture of the two in a proportion of from 1 to 50% by weight, where the sum of components A) and B) is always 100% by weight. This mixture is used for the production of sliding bearings or gasket materials having a reduced tendency to creep and reduced abrasion.
摘要:
A foamed polyarylene sulfide according to the invention has a density which is reduced by at least 50% compared with the theoretical density of nonfoamed material, and is expediently produced by subjecting a polyarylene sulfoxide as such or a mixture of one or more polyarylene sulfides with a polyarylene sulfoxide to heat treatment. The temperature of the heat treatment is in the range from 250.degree. to 400.degree. C.
摘要:
Binary and tertiary mixtures comprise (A) from 33 to 99% by weight of at least one polyarylene sulfone, (B) from 1 to 67% by weight of at least one polyarylene sulfoxide and/or (C) from 1 to 67% by weight of a polyarylene sulfide, where the sum of the components (A), (B) and (C) is always 100%. These mixtures can be processed to give homogeneous shaped parts, which are converted by the processing procedure into homogeneous polymer masses and only have the glass transition temperature of the polyarylene sulfone.
摘要:
A foamed polyarylene sulfide according to the invention has a density which is reduced by at least 50% compared with the theoretical density of nonfoamed material, and is expediently produced by subjecting a polyarylene sulfoxide as such or a mixture of one or more polyarylene sulfides with a polyarylene sulfoxide to heat treatment. The temperature of the heat treatment is in the range from 250.degree. to 400.degree. C.
摘要:
The invention relates to a molding composition based on fluoropolymers which additionally contain from 1 to 50% by weight of at least one polymer containing sulfoxide groups. The polymer containing sulfoxide groups comprises, in particular, polyarylene sulfoxide units of the formula: —(—C6H4—SO—)—.
摘要:
Mixtures comprising polyarylene sulfides and polyarylene sulfoxides or partially oxidized polyarylene sulfides containing sulfoxide groups can be thermally crosslinked in a targeted manner depending on sulfoxide content. A process for producing crosslinked polyarylene sulfide moldings is based on the use of the mixtures in the thermal shaping.
摘要:
A molding material which contains a sinterable polymer and a wax as a binder and advantageously an ethylene/vinyl acetate copolymer, an organic peroxide, an azoester and an alcohol can be injection molded to give a molding, dewaxed without loss of dimensional stability of the molding and then sintered.
摘要:
The novel blend comprises:(A) from 1 to 99% by weight of at least one thermotropic-liquid-crystalline polyester and/or polyesteramide and(B) from 1 to 99% by weight of at least one sulfoxide group-containing polymer,in each case based on the total weight .SIGMA.�(A)+(B)!. Component (B) is a linear and/or branched polymer having a mean molecular weight M.sub.w in the range from 4,000 to 200,000 comprising recurring units of the formula �--F--S).sub.c --(F--SO).sub.d --!, where F, independently of one another, are simple or para-, meta- or ortho-linked arylene systems having 6 to 18 carbon atoms, preferably phenylene, naphthylene or biphenylene, where the sum c+d is 1, with the proviso that d is always .gtoreq.0.70. Component (A) is a thermotropic liquid-crystalline polymer having a mean molecular weight M.sub.w in the range from 10,000 to 200,000 g/mol and a transition temperature of >250.degree. C., and/or an amorphous thermotropic liquid-crystalline polymer having a mean molecular weight M.sub.w of from 10,000 to 200,000 g/mol and a glass transition temperature of >160.degree. C.