摘要:
This invention relates to graft polymers of the ABS type which are produced in emulsion, and to thermoplastic molding compositions which are based thereon and which exhibit a very considerably increased notched bar impact strength compared with known ABS molding compositions and which at the same time exhibit high hardness values or high modulus values and good thermoplastic processability.
摘要:
Elastic-thermoplastic graft polymers manufactured by radical emulsion polymerization of resin-forming vinyl monomers in the presence of rubber present in latex form with the use of a combination of a peroxide of formula (I) ##STR1## where R.sup.1 signifies alkyl, cycloalkyl and aryl groups with 4 to 20 carbon atoms, X the groups --COOH and --SO.sub.3 H as well as their alkali, alkaline-earth or ammonium salts, n an integer in the range from 1 to 6, A alkylene, cycloalkylene and arylene groups with 6 to 40 carbon atoms and a reducing agent as initiator system, a method for their manufacture and their use as moulding compositions.
摘要:
Elastic-thermoplastic graft polymers manufactured by radical emulsion polymerisation of resin-forming vinyl monomers in the presence of rubber present in latex form with the use of a combination of a peroxide of formula (I) ##STR1## where R.sup.1 signifies alkyl, cycloalkyl and aryl groups with 4 to 20 carbon atoms,X the groups --COOH and --SO.sub.3 H as well as their alkali, alkaline-earth or ammonium salts,n an integer in the range from 1 to 6,A alkylene, cycloalkylene and arylene groups with 6 to 40 carbon atomsand a reducing agent as initiator system, a method for their manufacture and their use as moulding compositions.
摘要:
A molding composition having good surface gloss, high elongation at break and good thermoplastic processability is disclosed. The composition contains (A) a graft polymer that is obtained by free-radical polymerization of resin-forming vinyl monomers in the presence of rubber in latex form, (B) a copolymer of styrene and acrylonitrile and an optional (C) a resin selected from the group consisting of polycarbonates, polyester-carbonates, polyesters and polyamides. The preparation of the graft polymer is characterized in that (i) before the start of the grafting polymerization reaction the rubber latex is brought to a pH of 9 to 11, (ii) the redox initiator components are employed in amounts of 0.1 to 2.5 wt. % (based on the monomers metered in) and (iii) during the entire grafting polymerization reaction the pH remains constant±0.5 and in the range of 11.0 to 8.8, and (iv) the temperature difference between the start and end of the reaction is at least 10° C.
摘要:
A thermoplastic, flame-retardant moulding composition having improved mechanical properties is disclosed. The composition contains 40 to 99 parts by weight of a thermoplastic polycarbonate or polyester carbonate, 0.5 to 60 parts by weight of a graft polymer, 0 to 45 parts by weight of a thermoplastic vinyl copolymer, 0.5 to 20 parts by weight of a mixture of at least one mono- and at least one oligo-phosphorus conforming to the general formula and 0.05 to 5 parts by weight of a fluorinated polyolefine.
摘要:
Thermoplastic moulding materials containing A. 15 to 80 parts by weight of a thermoplastic polycarbonate or polyester carbonate, and B. 4 to 40 parts by weight of a graft polymer of B.1 20 to 60 weight % of one or more monomers on B.2 40 to 80 weight % of one or more graft bases having glass transition temperatures
摘要:
A molding composition containing a graft polymer is disclosed. The graft is a product of a free-radical emulsion polymerization of resin-forming vinyl monomers in the presence of rubber present in latex form having a glass transition temperature of ≦0° C. using an initiator combination comprising a persulfate compound and a redox initiator system. The process for preparing the graft polymer entails adding the persulfate compound at the beginning of the graft polymerization reaction and a later addition of the redox initiator. The composition that features good gloss and flowability is suitable for the preparation of molded articles.
摘要:
A thermoplastic molding composition that exhibits antistatic properties and improved color stability is disclosed. The composition contains a major amount of resinous component that contains A) 0 to 100 % by weight of one or more graft polymers B) 100 to 0 % by weight of a thermoplastic vinyl (co)polymer, and a minor amount of a mixture of a) a modified or unmodified polyalkylene ethers and b) a phenolic oxidant wherein the weight ratio (a):(b) is 20:1 to 1:1.
摘要:
Thermoplastic moulding compositions containingA. a thermoplastic polymer andB. 0.1 to 50% by weight, with respect to A, of an inorganic substance with an average particle diameter of 0.1 to 100 nm,and the use of superfine inorganic substances as defined by B for increasing the X-ray contrast of thermoplastic moulding compositions comprising A and B.
摘要:
Thermoplastic polycarbonate/graft polymer moulding compositions containingA) 5 to 95 parts by weight of an aromatic polycarbonate,B) 1 to 50 parts by weight of at least one thermoplastic homopolymer, copolymer or terpolymer of styrene, .alpha.-methylstyrene, acrylonitrile, N-substituted maleimide or mixtures thereof,C) 1 to 50 parts by weight of at least one graft polymer ofC.1) 5 to 90 parts by weight of styrene, .alpha.-methylstyrene, acrylonitrile, N-substituted maleimide or mixtures thereof, onC.2) 95 to 10 parts by weight of a rubber with a glass transition temperature .ltoreq.0.degree. C. andD) 1 to 25 parts by weight (per 100 parts by weight A+B+C) of at least one additive selected from flame retardants, lubricants, antistatic agent, mould release agents or mixtures thereof,characterised in that the component B) is produced by bulk, solution or suspension polymerisation and has an oligomer content .ltoreq.1 wt. %, component C) is produced by emulsion polymerisation and the total oligomer content of the moulding compositions is .ltoreq.0.6 wt. %.
摘要翻译:含有A)5-95重量份的芳族聚碳酸酯的热塑性聚碳酸酯/接枝聚合物模塑组合物,B)1至50重量份的至少一种苯乙烯,α-甲基苯乙烯,丙烯腈,N-甲基苯乙烯的共聚物或三元共聚物, 取代的马来酰亚胺或其混合物,C)1至50重量份的至少一种C.1的接枝聚合物)C至5重量份的苯乙烯,α-甲基苯乙烯,丙烯腈,N-取代的马来酰亚胺或其混合物,在C .2)95至10重量份的玻璃化转变温度为0℃的橡胶和D)1至25重量份(每100重量份A + B + C)至少一种添加剂 选自阻燃剂,润滑剂,抗静电剂,脱模剂或其混合物,其特征在于组分B)通过本体,溶液或悬浮液聚合制备,并且具有低聚物含量为1重量%。 %,组分C)通过乳液聚合制备,并且模塑组合物的总低聚物含量为0.6重量%。 %。