摘要:
An object of the present invention is to provide nickel cobalt manganese composite hydroxide particles having a small particle diameter and a uniform particle size distribution, and a method for producing the same.[Solution]A method for producing a nickel cobalt manganese composite hydroxide by a crystallization reaction is provided. The method includes: a nucleation step of performing nucleation by controlling a pH of an aqueous solution for nucleation including metal compounds containing nickel, cobalt and manganese, and an ammonium ion donor to 12.0 to 14.0 in terms of the pH as measured at a liquid temperature of 25° C. as a standard; and a particle growth step of growing nuclei by controlling a pH of an aqueous solution for particle growth containing nuclei formed in the nucleation step to 10.5 to 12.0 in terms of the pH as measured at a liquid temperature of 25° C. as a standard.
摘要:
An object of the present invention is to provide nickel cobalt manganese composite hydroxide particles having a small particle diameter and a uniform particle size distribution, and a method for producing the same.[Solution]A method for producing a nickel cobalt manganese composite hydroxide by a crystallization reaction is provided. The method includes: a nucleation step of performing nucleation by controlling a pH of an aqueous solution for nucleation including metal compounds containing nickel, cobalt and manganese, and an ammonium ion donor to 12.0 to 14.0 in terms of the pH as measured at a liquid temperature of 25° C. as a standard; and a particle growth step of growing nuclei by controlling a pH of an aqueous solution for particle growth containing nuclei formed in the nucleation step to 10.5 to 12.0 in terms of the pH as measured at a liquid temperature of 25° C. as a standard.
摘要:
Active material particles are provided that exhibit performance suitable for increasing the output of a lithium secondary battery and little deterioration due to charge-discharge cycling. The active material particles provided by the present invention have a hollow structure having secondary particles including an aggregate of a plurality of primary particles of a lithium transition metal oxide, and a hollow portion formed inside the secondary particles, and through holes that penetrates to the hollow portion from the outside are formed in the secondary particles. BET specific surface area of the active material particles is 0.5 to 1.9 m2/g.
摘要:
Active material particles are provided that exhibit performance suitable for increasing the output of a lithium secondary battery and little deterioration due to charge-discharge cycling. The active material particles provided by the present invention have a hollow structure having secondary particles including an aggregate of a plurality of primary particles of a lithium transition metal oxide, and a hollow portion formed inside the secondary particles, and through holes that penetrates to the hollow portion from the outside are formed in the secondary particles. BET specific surface area of the active material particles is 0.5 to 1.9 m2/g.
摘要:
Active material particles are provided that exhibit performance suitable for increasing the output of a lithium secondary battery and little deterioration due to charge-discharge cycling. The active material particles provided by the present invention have a hollow structure having secondary particles including an aggregate of a plurality of primary particles of a lithium transition metal oxide, and a hollow portion formed inside the secondary particles, and through holes that penetrates to the hollow portion from the outside are formed in the secondary particles. BET specific surface area of the active material particles is 0.5 to 1.9 m2/g.
摘要:
Provided are nickel manganese composite hydroxide particles having a small and uniform particle size and having a double structure which enables to obtain a cathode active material having a hollow structure, and a manufacturing method thereof. When obtaining the nickel manganese composite hydroxide by a reaction crystallization, using an aqueous solution for nucleation, which includes at least a metallic compound that contains nickel, a metallic compound that contains manganese and an ammonium ion donor and controlling the pH value that is measured at a standard solution temperature of 25° C. is 10.5 to 12.0, nucleation is performed in an oxidizing atmosphere in which the oxygen concentration is greater than 1% by volume, and then nuclei are grown by switching the atmosphere from the oxidizing atmosphere to a mixed atmosphere of oxygen and inert gas in which the oxygen concentration is 1% by volume or less.
摘要:
Provided are nickel manganese composite hydroxide particles having a small and uniform particle size and having a double structure which enables to obtain a cathode active material having a hollow structure, and a manufacturing method thereof. When obtaining the nickel manganese composite hydroxide by a reaction crystallization, using an aqueous solution for nucleation, which includes at least a metallic compound that contains nickel, a metallic compound that contains manganese and an ammonium ion donor and controlling the pH value that is measured at a standard solution temperature of 25° C. is 10.5 to 12.0, nucleation is performed in an oxidizing atmosphere in which the oxygen concentration is greater than 1% by volume, and then nuclei are grown by switching the atmosphere from the oxidizing atmosphere to a mixed atmosphere of oxygen and inert gas in which the oxygen concentration is 1% by volume or less.
摘要:
The present invention provides a cathode active material for a nonaqueous electrolyte secondary battery with a high capacity, high stability and excellent output characteristics and a method for producing the same, and a nonaqueous electrolyte secondary battery using the cathode active material.The cathode active material for a nonaqueous electrolyte secondary battery is represented by a general formula: LitNi1.x.y.zCoxAlyTizO2 wherein 0.98≦t≦1.10, 0
摘要翻译:本发明提供一种具有高容量,高稳定性和优异的输出特性的非水电解质二次电池用正极活性物质及其制造方法以及使用该正极活性物质的非水电解质二次电池。 用于非水电解质二次电池的阴极活性材料由以下通式表示:LitNi1.x.y.zCoxAlyTizO2其中0.98 @ t @ 1.10,0
摘要:
A method for producing nickel composite hydroxide particles may include: a first step of producing nuclei including primary particles by controlling the pH of an aqueous solution for nucleation, the aqueous solution for nucleation containing a metal compound having an atomic ratio of metals corresponding to an atomic ratio of metals in the nickel composite hydroxide particles and substantially not containing a metal complex ion-forming agent; and a second step of forming, on an outer surface of each of the nuclei, an outer shell portion including platy primary particles larger than primary particles of the nuclei by controlling the pH of an aqueous solution for particle growth containing the nuclei obtained in the nucleation step.
摘要:
Disclosed are: nickel complex hydroxide particles that have small and uniform particle diameters; and a method by which the nickel complex hydroxide particles can be produced. Specifically disclosed is a method for producing a nickel complex hydroxide by a crystallization reaction, which comprises: a nucleation step in which nucleation is carried out, while controlling an aqueous solution for nucleation containing an ammonium ion supplying material and a metal compound that contains nickel to have a pH of 12.0-13.4 at a liquid temperature of 25° C.; and a particle growth step in which nuclei are grown, while controlling an aqueous solution for particle growth containing the nuclei, which have been formed in the nucleation step, to have a pH of 10.5-12.0 at a liquid temperature of 25° C. In this connection, the pH in the particle growth step is controlled to be less than the pH in the nucleation step.