摘要:
Resins which are the copolymers of an alpha-olefin, a cyclic olefin, and an aromatic-group-containing monomer are provided. The cyclic olefins retain their cyclic structures and the aromatic-group-containing monomers retain their aromatic structures after copolymerization into the resin product. Methods for production of the new resins in the presence of a metallocene catalyst system are also provided. New adhesive compositions containing the resin and articles using the new adhesive compositions are also part of the invention.
摘要:
Novel tackifier resins having a M.sub.n of 5,000 or less and a T.sub.g of 0.degree. C. or above are produced by combining a metallocene catalyst with an alpha-olefin and a cyclic monomer. New adhesives are produced by blending the novel tackifier with a base polymer.
摘要:
This invention relates to an adhesive comprising a polymer composition comprising at least 50 mol % of one or more C3 to C40 olefins where the polymer composition has (a) a Dot T-Peel of 1 Newton or more on Kraft paper; (b) an Mw of at least 7000 to 80,000; (c) a branching index (g′) of from 0.4 to 0.90 measured at the Mz of the polymer composition; (d) a heat of fusion of 1 to 70 J/g; and (e) a heptane insoluble fraction of 70 weight % or less, based upon the weight of the polymer composition, where the heptane insoluble fraction has branching index g′ of 0.9 or less as measured at the Mz of the polymer composition.
摘要:
Disclosed is a process for producing branched polymers including at least 50 mol % C3–C40 olefins. The process may include: (1) feeding a first catalyst, an activator, and one or more C2–C40 olefins into a first reaction zone at a temperature of greater than 70° C. and a residence time of 120 minutes or less to produce a product; (2) feeding the product a second catalyst, and an activator into a second reaction zone at a temperature of greater than 70° C., and a residence time of 120 minutes or less. One of the catalysts should be chosen to produce a polymer having a weight average molecular weight of 100,000 or less and a crystallinity of 20% or less. The other catalyst should be chosen to producing a polymer having a weight average molecular weight of 100,000 or less and a crystallinity of 20% or more.
摘要:
This invention relates to a composition comprising a functionalized C3 to C40 olefin polymer comprising at least 50 mol % of one or more C3 to C40 olefins, and where the olefin polymer, prior to functionalization, has: a Dot T-Peel of 1 Newton or more on Kraft paper; an Mw of 10,000 to 100,000; and a branching index (g′) of 0.98 or less measured at the Mz of the polymer when the polymer has an Mw of 10,000 to 60,000, or a branching index of 0.95 or less measured at the Mz of the polymer when the polymer has an Mw of 10,000 to 100,000; and where the C3 to C40 olefin polymer comprises at least 0.001 wt % of a functional group. This invention further relates to blends of such functionalized polymers with other polymers including non-functionalized C3 to C40 olefin polymers as described above.
摘要:
This invention relates to a polymer comprising one or more C3 to C40 olefins, optionally one or more diolefins, and less than 15 mole % of ethylene, where the polymer has: a) a Dot T-Peel of 1 Newton or more; and b) a branching index (g′) of 0.95 or less measured at the Mz of the polymer; c) an Mw of 100,000 or less. This invention also relates a polymer comprising one or more C3 to C40 olefins where the polymer has: a) a Dot T-Peel of 1 Newton or more on Kraft paper; b) a branching index (g′) of 0.95 or less measured at the Mz of the polymer; c) a Mw of 10,000 to 100,000; and d) a heat of fusion of 1 to 70 J/g. This invention also relates a polymer comprising one or more C3 to C40 olefins where the polymer has: a) a Dot T-Peel of 1 Newton or more on Kraft paper; b) a branching index (g′) of 0.98 or less measured at the Mz of the polymer; c) a Mw of 10,000 to 60,000; d) a heat of fusion of 1 to 50 J/g. This invention also relates to a homopolypropylene or a copolymer of propylene and up to 5 mole % ethylene having: a) an isotactic run length of 1 to 30 (isotactic run length “IRL” is defined to be the percent of mmmm pentad divided by 0.5×percent of mmmr pentad) as determined by Carbon 13 NMR, preferably 3 to 25, more preferably 4 to 20, b) a percent of r dyad of greater than 20%, preferably from 20 to 70% as determined by Carbon 13 NMR, and c) a heat of fusion of 70 J/g or less, preferably 60 J/g or less, more preferably between 1 and 55 J/g, more preferably between 4 and 50 J/g. This invention further relates to a process to produce an olefin polymer comprising: 1) selecting a first catalyst component capable of producing a polymer having an Mw of 100,000 or less and a crystallinity of 5% or less at selected polymerization conditions; 2) selecting a second catalyst component capable of producing polymer having an Mw of 100,000 or less and a crystallinity of 20% or more at the selected polymerization conditions; 3) contacting the catalyst components in the presence of one or more activators with one or more C3 to C40 olefins, at the selected polymerization conditions in a reaction zone; 4) obtaining the polymer. This invention further relates to a continuous process to produce a branched olefin polymer comprising: 1) selecting a first catalyst component capable of producing a polymer having an Mw of 100,000 or less and a crystallinity of 5% or less under selected polymerization conditions; 2) selecting a second catalyst component capable of producing polymer having an Mw of 100,000 or less and a crystallinity of 20% or more at the selected polymerization conditions; 3) contacting the catalyst components in the presence of one or more activators with one or more C3 to C40 olefins, and, optionally one or more diolefins; 4) at a temperature of greater than 100° C.; 5) at a residence time of 120 minutes or less; 6) wherein the ratio of the first catalyst to the second catalyst is from 1:1 to 50:1; 7) wherein the activity of the catalyst components is at least 100 kilograms of polymer per gram of the catalyst components; and wherein at least 20% of the olefins are converted to polymer.
摘要:
The present invention describes polymer comprising one or more C3 to C40 olefins and having a Mw of 100,000 or less and a Dot T-Peel of 1 Newton or more. The polymer may have a branching index (g′) of 0.95 or less measured at the Mz of the polymer, and a heat of fusion of 1 to 70 J/g. Also described are polymers of homopolypropylene or a copolymer of propylene and up to 5 mole % ethylene having: an isotactic run length of 1 to 30 as determined by Carbon 13 NMR and a percent of r dyad of greater than 20%, preferably from 20 to 70% as determined by Carbon 13 NMR. Also described are methods of making these and other polymers.
摘要:
Embodiments of the present invention relate to article comprising 1) a functionalized component, 2) tackifier, and 3) an olefin polymer comprising one or more C3 to C40 olefins, optionally one or more diolefins, and less than 5 mole % of ethylene having a Dot T-Peel of 1 Newton or more, a branching index (g′) of 0.95 or less measured at the Mz of the polymer; and an Mw of 100,000 or less; where the functional component is selected from the group consisting of functionalized polymers, functionalized oligomers and beta nucleating agents; and where the Gardner color of the adhesive does not change by more than 7 Gardner units when the adhesive has been heat aged at 180° C. for 48 hours as compared to the Gardner color of the unaged composition.
摘要:
Disclosed herein is an adhesive composition comprising a blend functionalized with a functional group, wherein the blend comprises a C3 to C40 olefin polymer and an additive, the C3 to C40 olefin polymer comprising at least 50 mol % of one or more C3 to C40 olefins, and where the C3 to C40 olefin polymer has: a Dot T-Peel of 1 Newton or more on Kraft paper; an Mw of 10,000 to 100,000; and a branching index (g′) of 0.98 or less measured at the Mz of the polymer when the polymer has an Mw of 10,000 to 60,000, or a branching index (g′) of 0.95 or less measured at the Mz of the polymer when the polymer has an Mw of 10,000 to 100,000. A process of producing the adhesive composition, as well as methods of utilizing the adhesive composition are also disclosed.
摘要:
This invention relates to a composition comprising a functionalized C3 to C40 olefin polymer comprising at least 50 mol % of one or more C3 to C40 olefins, and where the olefin polymer, prior to functionalization, has: a Dot T-Peel of 1 Newton or more on Kraft paper; an Mw of 10,000 to 100,000; and a branching index (g′) of 0.98 or less measured at the Mz of the polymer when the polymer has an Mw of 10,000 to 60,000, or a branching index of 0.95 or less measured at the Mz of the polymer when the polymer has an Mw of 10,000 to 100,000; and where the C3 to C40 olefin polymer comprises at least 0.001 wt % of a functional group. This invention further relates to blends of such functionalized polymers with other polymers including non-functionalized C3 to C40 olefin polymers as described above.