    摘要: Weld metals and methods for welding ferritic steels are provided. The weld metals have high strength and high ductile tearing resistance and are suitable for use in strain based pipelines. The weld metal contains retained austenite and has a cellular microstructure with cell walls containing lath martensite and cell interiors containing degenerate upper bainite. The weld metals are comprised of between 0.02 and 0.12 wt % carbon, between 7.50 and 14.50 wt % nickel, not greater than about 1.00 wt % manganese, not greater than about 0.30 wt % silicon, not greater than about 150 ppm oxygen, not greater than about 100 ppm sulfur, not greater than about 75 ppm phosphorus, and the balance essentially iron. Other elements may be added to enhance the properties of the weld metal. The weld metals are applied using a power source with current waveform control which produces a smooth, controlled welding arc and weld pool in the absence of CO2 or oxygen in the shielding gas.

    摘要翻译: 提供焊接金属和焊接铁素体钢的方法。 焊接金属具有高强度和高延展性抗撕裂性,适用于基于应变的管道。 焊缝金属含有残余奥氏体,并具有细胞结构,其中包含板条马氏体的细胞壁和含有退化的上贝氏体的细胞内部。 焊接金属包括0.02至0.12重量%的碳,7.50至14.50重量%的镍,不大于约1.00重量%的锰,不大于约0.30重量%的硅,不大于约150ppm的氧,不大于 大于约100ppm的硫,不大于约75ppm的磷,余量基本上是铁。 可以添加其它元素以增强焊接金属的性能。 使用具有电流波形控制的电源施加焊接金属,其在保护气体中不存在CO 2或氧的情况下产生平滑的,受控制的焊接电弧和焊接池。