摘要:
A fast-setting, bioresorbable calcium phosphate cement is prepared by a process which can be carried out with a heat treatment up to 1000° C. on a mixture of a wetting solution and a calcium phosphate powder having a Ca to P molar ratio of 0.5–2.5. The wetting solution suitable for use in the process of the present invention includes water, an organic solvent, an acidic and basic solution. A setting solution for mixing with the heated powder to form the fast-setting, bioresorbable calcium phosphate cement may be water, an acidic or basic solution according to the process of the present invention.
摘要:
A process for preparing a paste from calcium phosphate cement includes a) mixing an aqueous acidic solution and powder containing at least one of tricalcium phosphate and tetracalcium phosphate; and b) mixing the resulting mixture from step a) and an aqueous basic solution to form a paste. The calcium phosphate cement paste is useful in dental and bone prosthesis.
摘要:
A fast-setting, bioresorbable calcium phosphate cement is prepared by a process which can be carried out with a heat treatment up to 1000° C. on a mixture of a wetting solution and a calcium phosphate powder having a Ca to P molar ratio of 0.5-2.5. The wetting solution suitable for use in the process of the present invention includes water, an organic solvent, an acidic and basic solution. A setting solution for mixing with the heated powder to form the fast-setting, bioresorbable calcium phosphate cement may be water, an acidic or basic solution according to the process of the present invention.
摘要:
A method of shortening a working and setting time of a CPC paste without using additives or sacrificing its strength, which includes heating CPC powder so that the CPC powder is maintained at a temperature of 50-400° C. for a period of time which is greater than one minute.
摘要:
A method for increasing working time/setting time of monolithic tetracalcium phosphate (TTCP) cement paste formed by mixing a TTCP powder with an aqueous solution, which includes heating the TTCP powder, prior to the mixing, so that the TTCP powder is maintained at a temperature of 50-350° C. for a period of time which is greater than one minute, and that a TTCP cement paste formed by mixing the resulting heated TTCP powder with the aqueous solution has a prolonged working time in comparison with that formed by mixing TTCP powder that has not been subjected to such heating with the aqueous solution.
摘要:
A tetracalcium phosphate (TTCP) particle for use in preparing a fast-setting, bioresorbable calcium phosphate cement is disclosed. The TTCP particle has a basic calcium phosphate whiskers on a surface thereof; the basic calcium phosphate whiskers having a Ca/P molar ratio greater than 1.33, and having a length up to about 5000 nm and a width up to about 500 nm. The basic calcium phosphate whiskers are substantially free of a hydroxyapatite phase and mainly composed of TTCP phase.
摘要:
A tetracalcium phosphate (TTCP) particle for use in preparing a fast-setting, bioresorbable calcium phosphate cement is disclosed. The TTCP particle has a basic calcium phosphate whiskers or fine crystals on a surface thereof; the basic calcium phosphate whiskers or fine crystals having a Ca/P molar ratio greater than 1.33, and having a length up to about 5000 nm and a width up to about 500 nm.
摘要:
A fast-setting, bioresorbable calcium phosphate cement is prepared by a process which can be carried out with a heat treatment up to 1000° C. on a mixture of a wetting solution and a calcium phosphate powder having a Ca to P molar ratio of 0.5-2.5. The wetting solution suitable for use in the process of the present invention includes water, an organic solvent, an acidic and basic solution. A setting solution for mixing with the heated powder to form the fast-setting, bioresorbable calcium phosphate cement may be water, an acidic or basic solution according to the process of the present invention.
摘要:
A fast-setting, bioresorbable calcium phosphate cement is prepared by a process which can be carried out with a heat treatment up to 1000° C. on a mixture of a wetting solution and a calcium phosphate powder having a Ca to P molar ratio of 0.5–2.5. The wetting solution suitable for use in the process of the present invention includes water, an organic solvent, an acidic and basic solution. A setting solution for mixing with the heated powder to form the fast-setting, bioresorbable calcium phosphate cement may be water, an acidic or basic solution according to the process of the present invention.
摘要:
A fast-setting, bioresorbable calcium phosphate cement is prepared by a process which can be carried out with a heat treatment up to 1000° C. on a mixture of a wetting solution and a calcium phosphate powder having a Ca to P molar ratio of 0.5-2.5. The wetting solution suitable for use in the process of the present invention includes water, an organic solvent, an acidic and basic solution. A setting solution for mixing with the heated powder to form the fast-setting, bioresorbable calcium phosphate cement may be water, an acidic or basic solution according to the process of the present invention.