摘要:
An induction coil for inductive heating of at least one metallic component having at least one lateral face and at least one face to be heated is provided. The induction coil includes a meandering pattern section shaped around the at least one component in such a way that the section extends over at least a partial area of the at least one lateral face of the at least one component to be heated in the area of the at least one face to be heated. A device and method for inductive heating of at least one metallic component are also provided.
摘要:
A method for welding two components is disclosed. In an embodiment, the method includes the following process steps. The two components are positioned such that the joining surfaces are opposite each other, at a short distance from each other. A high-frequency electrical current is conducted through the two components, heating the components at least in the region of the joining surfaces. The two components are pressed against each other such that the two joining surfaces are welded together.
摘要:
A method for joining at least two components by inductive high-frequency pressure welding is disclosed. The first component has a first material structure with a first hardness and the second component has a second material structure with a second hardness which is smaller than the first hardness. Both components are inductively heated in the region of the joining surfaces and are subsequently pressed together by a compressive force. The joining surface of the first component with the first hardness, which is greater than the second hardness of the second component, is pre-contoured in a spherical, conical or convex manner prior to joining the two components.
摘要:
A method for joining at least two components by inductive high-frequency pressure welding is disclosed. The first component has a first material structure with a first hardness and the second component has a second material structure with a second hardness which is smaller than the first hardness. Both components are inductively heated in the region of the joining surfaces and are subsequently pressed together by a compressive force. The joining surface of the first component with the first hardness, which is greater than the second hardness of the second component, is pre-contoured in a spherical, conical or convex manner prior to joining the two components.
摘要:
The present technology concerns one or more methods for joining of metal components especially components of a gas turbine, in which joining of the corresponding joining surfaces of the components occurs by means of an inductive low or high-frequency pressure welding and in which, before heating and joining of the components by means of inductive low or high-frequency pressure welding, sputter etching of the joining surfaces is carried out. The present technology also concerns a device for execution of an inductive low or high-frequency pressure welding method for joining the metal components, especially components of a gas turbine, with at least one induction generator and at least one inductor, as well as a component produced with the method according to the present technology.
摘要:
A method and apparatus for the detection of flaws, in particular of fissures, in metal components, is disclosed. A pulsed high-frequency magnetic field is coupled to the component. The temperature distribution of thermal energy generated by eddy currents during the application of a magnetic field pulse is detected.
摘要:
The invention relates to a method and device for generatively producing components, said device comprising a radiation device for selectively radiating a powder bed, and an induction device for inductively heating the component produced by radiating the powder bed, Said induction device comprising at least one voltage source which can simultaneously produce alternating voltages with at least two different frequencies.
摘要:
The invention relates to a method for joining two components (10, 12) made of a metal material, which are connected on two mutually associated joining surfaces (14, 16) by means of a joined connection, wherein at least one of the components (10) is strengthened in at least a partial region of the joining surface (14) thereof prior to joining. The invention further relates to a joined connection of two components (10, 12) made of a metal material.
摘要:
The invention relates to a method for joining two components (10, 12) made of a metal material, which are connected on two mutually associated joining surfaces (14, 16) by means of a joined connection, wherein at least one of the components (10) is strengthened in at least a partial region of the joining surface (14) thereof prior to joining. The invention further relates to a joined connection of two components (10, 12) made of a metal material.
摘要:
The invention relates to a method of nondestructive and contactless testing of components (3), wherein ultrasonic waves (6) are irradiated onto the surface of the component (3) at a predefinable, non-perpendicular angle of incidence (9) using an ultrasonic transmission sound transducer (1) arranged spaced apart from the surface of the component (3) and the intensity of the ultrasonic waves (7) reflected from the surface of the component (3) is detected with time resolution and/or frequency resolution by the antenna array elements (2n) of an ultrasonic antenna array (2) configured for detecting ultrasonic waves (7) and the phase shift of the ultrasonic waves guided at the surface of the test body is determined therefrom with respect to the ultrasonic waves (7) directly reflected at the surface of the component (3).