High volume solids fluorocarbon coatings
    1.
    发明授权
    High volume solids fluorocarbon coatings 有权
    高体积固体碳氟涂料

    公开(公告)号:US06255398B1

    公开(公告)日:2001-07-03

    申请号:US09343004

    申请日:1999-06-29

    IPC分类号: C08L3304

    摘要: The invention provides thermosetting coating compositions in which acrylic copolymers are used as carriers for fluorocarbon resins. The compositions have a combination of high fluorocarbon content, high solids content, and a low viscosity suitable for coil coating. Thus, the solids are borne in organic solvent systems which permit minimization of the viscosity and a moderate evaporation rate. The solvent system has a &dgr;H of from 1.7 to 2.6 (calories/cubic centimeter)½ and a &dgr;V of from 8 to 9.5 (calories/cubic centimeter)½ and is exemplified by a mixture of 4 or more of the following solvents: aliphatic ketones having from 4 to 10 carbon atoms, alkyl esters having a total of from 5 to 7 carbon atoms, aromatic acid esters having from 8 to 12 carbon atoms, lactones, and aromatic solvents. The acrylic polymer is comprised of (a) acrylic esters having no additional functionality, (b) acrylic esters having additional functionality by which the acrylic polymer may be cross-linked, and (c) an acryloxyalkyl oxazolidine.

    摘要翻译: 本发明提供热固性涂料组合物,其中使用丙烯酸共聚物作为碳氟树脂的载体。 组合物具有高碳氟含量,高固体含量和适用于卷材涂层的低粘度的组合。 因此,固体承载在有机溶剂体系中,其允许最小化粘度和适度的蒸发速率。 溶剂系统的ΔH为1.7至2.6(卡路里/立方厘米)1/2,δV为8至9.5(卡路里/立方厘米)1/2,以4种或更多种以下溶剂的混合物为例:脂族酮 具有4至10个碳原子,具有总共5至7个碳原子的烷基酯,具有8至12个碳原子的芳族酸酯,内酯和芳族溶剂。 丙烯酸类聚合物由(a)不具有附加官能团的丙烯酸酯组成,(b)具有丙烯酸类聚合物可交联的附加官能团的丙烯酸酯,和(c)丙烯酰氧烷基恶唑烷。

    Metal roofing shingle stock and method for making it
    3.
    发明授权
    Metal roofing shingle stock and method for making it 失效
    金属屋顶瓦房屋及其制作方法

    公开(公告)号:US06485781B2

    公开(公告)日:2002-11-26

    申请号:US10087634

    申请日:2002-03-01

    IPC分类号: B05D112

    摘要: This invention relates to a method for embedding a multiplicity of discrete masses of material in a resinous coating on a sheet of metal in a coil coating system. The sheet is coated, the masses are embedded in the wet resinous coating, and the coating is dried in a one-pass system. The resinous coating and the embedded masses are preferably resistant to ultra-violet radiation. The wet resinous coating, therefore, is preferably a liquid fluorocarbon resin. The discrete masses comprise pigmented particulate minerals and resins in the form of granules, beads, vesiculated beads, pellets, flakes, platelets, cylinders, coating powders, and coating powder precursor chips. The minerals include glass, quartz, mica, pebbles, and ceramics. The particulate resins include polyesters, acrylics, nylons, polyurethanes, polycarbonates, solid fluorocarbon resins, and solid mixtures of a fluorocarbon resin and an acrylate or methacrylate polymer or copolymer. Sheet metal decorated in such a manner is useful as stock in the manufacture of metal roofing shingles simulating the appearance of traditional asphalt shingles.

    摘要翻译: 本发明涉及一种用于在线圈涂覆系统中将多个离散质量的材料嵌入树脂涂层的金属片上的方法。 将该片材进行涂布,将质量嵌入湿树脂涂层中,并且涂层在一次通过系统中干燥。 树脂涂层和嵌入块优选耐紫外线辐射。 因此,湿树脂涂料优选为液体氟碳树脂。 离散的质量包括着色颗粒矿物和颗粒形式的颗粒,珠粒,泡状珠粒,颗粒,薄片,血小板,圆柱体,涂层粉末和涂层粉末前体碎片。 矿物包括玻璃,石英,云母,鹅卵石和陶瓷。 颗粒状树脂包括聚酯,丙烯酸树脂,尼龙,聚氨酯,聚碳酸酯,固体氟碳树脂,以及氟碳树脂和丙烯酸酯或甲基丙烯酸酯聚合物或共聚物的固体混合物。 以这种方式装饰的钣金在用于模拟传统沥青瓦的外观的金属屋顶瓦的制造中是有用的。

    Metal roofing shingle stock and method for making it
    4.
    发明授权
    Metal roofing shingle stock and method for making it 失效
    金属屋顶瓦房屋及其制作方法

    公开(公告)号:US06540829B2

    公开(公告)日:2003-04-01

    申请号:US10087636

    申请日:2002-03-01

    IPC分类号: B05C1904

    摘要: A coil coating system for embedding discrete masses of material in a resinous coating on sheet metal as it is pulled from a dispensing coil through a series of rollers, said system comprising a paint pan, a roller rotating in the pan and picking up said resinous coating composition and transferring it to an applicator roller; thenceforth to the moving sheet metal, an oven, and a sprayer that can heat thermoplastic resin particles to a molten or plastic state and spray the particles to the moving sheet metal.

    摘要翻译: 一种线圈涂覆系统,用于在通过一系列辊从分配线圈拉出时将分散质量的材料嵌入到金属板上的树脂涂层中,所述系统包括油漆盘,在锅中旋转的辊和拾取所述树脂涂层 组合并将其转移到施加辊; 从而可移动的金属板,烘箱和喷雾器,其可以将热塑性树脂颗粒加热到熔融或塑性状态并将颗粒喷射到移动的金属板上。

    Non-blistering thick film coating compositions and method for providing
non-blistering thick film coatings on metal surfaces
    5.
    发明授权
    Non-blistering thick film coating compositions and method for providing non-blistering thick film coatings on metal surfaces 失效
    非起泡厚膜涂料组合物和在金属表面上提供非起泡厚膜涂层的方法

    公开(公告)号:US5688598A

    公开(公告)日:1997-11-18

    申请号:US672280

    申请日:1996-06-28

    摘要: A thermosetting, organic solvent-based, primer coating composition for protecting metal surfaces which includes a solvent solution of: (a) a hydroxy-functional polyester resin; (b) a thermosetting acrylic resin; (c) a hydroxy-terminal polybutadiene resin, a hydroxy-terminal epoxidized polybutadiene resin, or mixtures thereof; (d) a blocked isocyanate crosslinker including at least one dimethyl pyrazole blocked isocyanate; (e) an aminoplast crosslinker including at least one melamine-formaldehyde condensate; (f) a catalyst; and, (g) a pigment. The primer exhibits excellent flexibility after curing to allow the primer to be coil coated onto metals as a thicker film and to have the metal subsequently formed without film fracture or loss of adhesion. The primer also has improved solvent release properties during curing to allow volatiles to readily escape therefrom, which facilitates coil coating of the primer onto metals as thicker films that, when cured into thick film hardened surface finishes, do not exhibit the typical blisters, craters, pops, voids and other surface defects. The primer can be cured as well at reduced temperatures which contributes to the reduction in surface defects. A fluorocarbon topcoat is usually coil coated and cured over the non-blistering primer coating, to yield a composite coated metal substrate having a surface finish that is free of blisters, craters, pops, and voids, and other surface defects.

    摘要翻译: 一种用于保护金属表面的热固性有机溶剂型底漆涂料组合物,其包括以下溶剂溶液:(a)羟基官能聚酯树脂; (b)热固性丙烯酸树脂; (c)羟基末端聚丁二烯树脂,羟基末端环氧化聚丁二烯树脂或其混合物; (d)包含至少一个二甲基吡唑封端异氰酸酯的封端异氰酸酯交联剂; (e)包含至少一种三聚氰胺 - 甲醛缩合物的氨基塑料交联剂; (f)催化剂; 和(g)颜料。 该底漆在固化后显示出优异的柔韧性,以使底漆作为更厚的膜被卷绕在金属上,并且随后形成金属,而不会发生膜断裂或粘合丧失。 该底漆还具有改善的固化过程中的溶剂释放性能,以使挥发物容易从其中逸出,这有利于底漆在金属上卷绕涂层,因为当固化成厚膜硬化表面处理时,较薄的膜不会出现典型的起泡, 弹出,空隙等表面缺陷。 底漆也可以在降低的温度下固化,这有助于减少表面缺陷。 氟碳面漆通常在非起泡底漆涂层上卷曲涂覆并固化,得到具有表面光洁度的复合涂覆金属基材,其表面没有水泡,凹坑,气泡和空隙以及其它表面缺陷。