Glass for substrate, and glass substrate
    1.
    发明授权
    Glass for substrate, and glass substrate 有权
    玻璃基板和玻璃基板

    公开(公告)号:US08580411B2

    公开(公告)日:2013-11-12

    申请号:US13271322

    申请日:2011-10-12

    IPC分类号: G11B5/73 C03C3/083

    摘要: To provide glass to be used for a substrate which is, as a substrate, less susceptible to surface roughening even if subjected to cleaning by means of a strongly acidic solution.Glass for a substrate, which comprises, as represented by mol % based on the following oxides, from 62.5 to 69% of SiO2, from 9 to 15.5% of Al2O3, from 8 to 16 of Li2O, from 0 to 8% of Na2O, from 0 to 7% of K2O and from 0 to 3.5% of ZrO2, provided that SiO2—Al2O3 is at least 53.3%, Li2O+Na2O+K2O is from 17 to 24%, and the total of contents of the above six components is at least 97%.

    摘要翻译: 为了提供用作基板的玻璃,作为基板,即使经受强酸溶液的清洗也不太容易受到表面粗糙化的影响。 用于底物的玻璃,其以由以下氧化物的摩尔%表示,为62.5至69%的SiO 2,9至15.5%的Al 2 O 3,8至16的Li 2 O,0至8%的Na 2 O, 0〜7%的K 2 O和0〜3.5%的ZrO 2,只要SiO 2 -Al 2 O 3为至少53.3%,Li 2 O + Na 2 O + K 2 O为17〜24%,上述6种成分的总和为 至少97%。

    Glass substrate for information recording medium and magnetic disk
    3.
    发明授权
    Glass substrate for information recording medium and magnetic disk 有权
    用于信息记录介质和磁盘的玻璃基板

    公开(公告)号:US08349476B2

    公开(公告)日:2013-01-08

    申请号:US12909221

    申请日:2010-10-21

    CPC分类号: G11B5/7315 C03C3/083

    摘要: To provide a process to improve acid resistance of a glass substrate for an information recording medium. A process for producing the glass substrate for an information recording medium, includes processing a glass formed into a plate by a float process, a down-draw method or a press method, wherein, in cooling the glass at the last step the glass has a temperature of at least its strain point, the time during which the glass temperature is at least its strain point and at most a temperature where the glass viscosity is 1010dPa·s is at least 13 minutes.

    摘要翻译: 提供一种提高信息记录介质的玻璃基板耐酸性的方法。 一种用于信息记录介质的玻璃基板的制造方法,其特征在于,包括通过浮法加工形成板的玻璃,下拉法或压制法,其中,在最后一步冷却玻璃时,玻璃具有 至少其应变点的温度,玻璃温度至少为其应变点的时间,以及至多玻璃粘度为1010dPa·s的温度为至少13分钟。

    Glass for information recording medium substrate, glass substrate for information recording medium and magnetic disk
    4.
    发明授权
    Glass for information recording medium substrate, glass substrate for information recording medium and magnetic disk 有权
    用于信息记录介质基板的玻璃,用于信息记录介质的玻璃基板和磁盘

    公开(公告)号:US08168313B2

    公开(公告)日:2012-05-01

    申请号:US12724570

    申请日:2010-03-16

    IPC分类号: G11B5/73 C03C3/085 C03C3/087

    摘要: A glass for an information recording medium substrate, which comprises, as represented by mol % based on the following oxides, from 61 to 72% of SiO2, from 3 to 11% of Al2O3, from 0 to 14.3% of Li2O, from 0 to 22% of Na2O, from 0 to 22% of K2O, from 4 to 13% of MgO, from 0 to 6% of TiO2 and from 0 to 5% of ZrO2, provided that the total content of Li2O, Na2O and K2O (R2O) is from 10 to 22%, and (a) the ratio of the content of Li2O to R2O (Li2O/R2O) is at most 0.52, (b) the ratio of the content of Na2O to R2O (Na2O/R2O) is at least 0.35, or (c) the ratio of the content of K2O to R2O (K2O/R2O) is at least 0.45.

    摘要翻译: 一种用于信息记录介质基材的玻璃,其以以下氧化物的摩尔%表示,SiO 2为61至72%,Al 2 O 3为3至11%,Li 2 O 0至14.3%,为0至 22%的Na2O,0〜22%的K2O,4〜13%的MgO,0〜6%的TiO2和0〜5%的ZrO2,条件是Li2O,Na2O和K2O(R2O)的总含量 )为10〜22%,(a)Li 2 O与R 2 O(Li 2 O / R 2 O)的含量比例为0.52以下,(b)Na2O与R2O的含量比(Na2O / R2O)为 至少0.35,或(c)K2O与R2O(K2O / R2O)的含量之比至少为0.45。

    Process for producing glass substrate for information recording medium
    6.
    发明授权
    Process for producing glass substrate for information recording medium 有权
    信息记录媒体用玻璃基板的制造方法

    公开(公告)号:US08402790B2

    公开(公告)日:2013-03-26

    申请号:US12909423

    申请日:2010-10-21

    IPC分类号: G11B5/84 C03B25/00 G11B5/62

    摘要: To provide a process to improve acid resistance of a glass substrate for an information recording medium.A process for producing a glass substrate for an information recording medium, comprising processing a glass formed into a plate by a float process, a down-draw method or a press method, wherein, in cooling of the glass in the last step where the glass has a temperature of at least its strain point, the time during which the glass temperature is at least its strain point and at most a temperature where the glass viscosity is 1010 dPa·s is at least 13 minutes.

    摘要翻译: 提供一种提高信息记录介质的玻璃基板耐酸性的方法。 一种用于信息记录介质的玻璃基板的制造方法,其特征在于,包括通过浮法加工形成为板的玻璃,下拉法或压制法,其中在玻璃的最后工序中,玻璃的冷却 具有至少应变点的温度,玻璃温度至少为其应变点的时间和玻璃粘度为1010dPa·s以下的温度为至少13分钟。

    GLASS SUBSTRATE FOR INFORMATION RECORDING MEDIUM AND MAGNETIC DISK
    7.
    发明申请
    GLASS SUBSTRATE FOR INFORMATION RECORDING MEDIUM AND MAGNETIC DISK 有权
    用于信息记录介质和磁盘的玻璃基板

    公开(公告)号:US20110123833A1

    公开(公告)日:2011-05-26

    申请号:US12909221

    申请日:2010-10-21

    IPC分类号: G11B5/706

    CPC分类号: G11B5/7315 C03C3/083

    摘要: To provide a glass for an information recording medium substrate, which is excellent in weather resistance.A glass substrate for an information recording medium, which is made of an alkali aluminosilicate glass, wherein the difference obtained by subtracting the glass transition temperature Tg from the fictive temperature Tf, i.e. Tf−Tg, is at most 5° C. The glass substrate for an information recording medium, which comprises, as represented by mol % based on the following oxides, from 64 to 67% of SiO2, from 8 to 10% of Al2O3, from 10 to 13% of Li2O, from 9 to 12% of Na2O, from 0 to 2% of K2O and from 2 to 4% of ZrO2, provided that the total content of Li2O, Na2O and K2O, i.e. Li2O+Na2O+K2O, is from 21 to 25%.

    摘要翻译: 提供耐候性优异的信息记录介质基板用玻璃。 用于由铝硅酸铝玻璃制成的信息记录介质的玻璃基板,其中通过从假想温度Tf(即Tf-Tg)减去玻璃化转变温度Tg得到的差值为至多5℃。玻璃基板 对于信息记录介质,其包含以下列氧化物的摩尔%表示:SiO 2 64%〜67%,Al 2 O 3 8〜10%,Li 2 O 10〜13%,Li 2 O 9〜12% Na 2 O,0〜2%的K 2 O和2〜4%的ZrO 2,条件是Li 2 O,Na 2 O和K 2 O(即Li 2 O + Na 2 O + K 2 O)的总含量为21〜25%。

    Vehicle door control apparatus and vehicle door control method
    8.
    发明授权
    Vehicle door control apparatus and vehicle door control method 有权
    车门控制装置和车门控制方法

    公开(公告)号:US09193331B2

    公开(公告)日:2015-11-24

    申请号:US13825127

    申请日:2012-02-07

    申请人: Jun Endo

    发明人: Jun Endo

    摘要: A vehicle door control apparatus is provided with an authentication unit, a detection unit and a control unit. The authentication unit authenticates an ID information outputted from a mobile device carried by a user. The detection unit detects an object around a door. The control unit performs an opening operation of the door at least when both a first condition and a second condition are satisfied. In the first condition, the authentication unit authenticates the ID information. In the second condition, the detection unit detects that the object is separated from a predetermined determination area after the object is continuously located in the determination area over a predetermined time.

    摘要翻译: 车门控制装置设有认证单元,检测单元和控制单元。 认证单元认证由用户承载的移动设备输出的ID信息。 检测单元检测门周围的物体。 至少当满足第一条件和第二条件时,控制单元执行门的打开操作。 在第一条件下,认证单元认证该ID信息。 在第二条件下,检测单元在预定时间之后,在物体连续地位于确定区域中之后,检测出物体与预定的确定区域分离。

    Organic electroluminescent element
    10.
    发明授权
    Organic electroluminescent element 有权
    有机电致发光元件

    公开(公告)号:US08604466B2

    公开(公告)日:2013-12-10

    申请号:US13258693

    申请日:2010-03-23

    IPC分类号: H01L35/24

    摘要: Provided is an organic electroluminescence device that has solved the conventional problems, and is thermally and chemically stable, has high efficiency with which an electron is injected from a cathode layer or an intermediate conductive layer to a light emitting layer, provides high luminous efficiency at a low voltage, and can maintain a long lifetime. Specifically, the organic electroluminescence device is an organic electroluminescence device, including: two electrode layers and optionally one or more intermediate conductive layers; a light emitting layer between the electrode layers, or between one of the electrode layers and the intermediate conductive layer and/or between the intermediate conductive layers; and an electron injection region formed of one or two or more layers between the light emitting layer and the cathode layer and/or between the light emitting layer and the intermediate conductive layer, in which at least one layer in the electron injection region contains at least one kind selected from the group consisting of an oxide of a transition metal belonging to any one of Groups 5 to 8 of the periodic table, a nitrogen-containing heterocyclic derivative, and a chalcogenide, and further contains a compound represented by the formula: MxAOy (in the formula, M represents Li, Na, K, Rb, or Cs, A represents Zr, V, Nb, Ta, Si, or Ge, x represents 1 or 2, and y represents an integer of 1 to 4).

    摘要翻译: 本发明提供了一种有机电致发光器件,其解决了常规问题,并且是化学稳定的,具有从阴极层或中间导电层向发光层注入电子的高效率,在 低电压,可以保持长寿命。 具体地说,有机电致发光元件是有机电致发光器件,包括:两个电极层和可选的一个或多个中间导电层; 电极层之间或者电极层和中间导电层之间和/或中间导电层之间的发光层; 以及在所述发光层和所述阴极层之间和/或所述发光层与所述中间导电层之间由一层或两层以上形成的电子注入区域,其中所述电子注入区域中的至少一层至少含有 选自属于周期表第5至8族中的任何一种的过渡金属的氧化物,含氮杂环衍生物和硫族化物的一种,并且还包含由下式表示的化合物:MxAOy (式中,M表示Li,Na,K,Rb或Cs,A表示Zr,V,Nb,Ta,Si或Ge,x表示1或2,y表示1〜4的整数。