Abstract: A carrier for ligand immobilization obtained by shrinking polysaccharide porous beads not less than 10% by a shrinkage rate defined by the following formula, and crosslinking the polysaccharide porous beads: Shrinkage rate (%)=(1−V2/V1)×100 (wherein, V1 indicates the gel volume of polysaccharide porous beads before shrinkage, and V2 indicates the gel volume of polysaccharide porous beads after shrinkage).
-
公开(公告)号:US10040053B2
公开(公告)日:2018-08-07
申请号:US15029293
申请日:2014-10-14
Applicant: KANEKA CORPORATION
Inventor: Kento Kanaya , Yoshikazu Kawai , Takahiro Okubo , Ken-ichiro Morio
IPC: B01J20/24 , B01J20/285 , B01D15/00 , B01J20/32 , C02F1/28 , C12P19/14 , B01J20/26 , B01J20/30 , B01J20/28 , C08J9/00 , B01J20/00 , B01J39/00 , C02F1/42 , C02F1/52 , B01D21/01 , C07K1/22 , C08J9/26 , G01N30/52 , B01J20/286
Abstract: The objective of the present invention is to provide to a method for easily producing high-performance porous cellulose beads having high mechanical strength. Also, the objective of the present invention is to provide an adsorbent produced from the high-performance porous cellulose beads. According to the present invention, high-performance porous cellulose beads can be easily produced from porous cellulose beads, and an adsorbent having high strength and high adsorption amount can be easily produced from the high-performance porous cellulose beads.
-
公开(公告)号:US10221211B2
公开(公告)日:2019-03-05
申请号:US15025152
申请日:2014-09-26
Applicant: KANEKA CORPORATION
Inventor: Takahiro Okubo , Yoshikazu Kawai , Masaru Hirano , Fuminori Konoike , Keiichi Karasugi , Tatsuya Honda
IPC: B01D15/38 , C07K1/22 , B01J20/24 , C08B1/08 , C08B15/08 , C08B15/10 , C08B3/06 , C08B15/00 , C08B16/00 , C08L1/02 , C08L1/04 , C08L1/12 , B01J20/286 , B01J20/32 , B01J20/28 , C08J3/16 , B01J20/26 , B01J20/285 , B01J20/30 , C07K16/00 , C08J9/00
Abstract: A process for producing porous cellulose beads of the present invention is characterized by comprising the steps of: a) mixing an alkali aqueous solution and cellulose to prepare cellulose micro dispersion at low temperature, b) adding water to the cellulose micro dispersion to prepare cellulose slurry, and d) bringing the cellulose slurry into contact with coagulation solvent. A carrier for ligand immobilization of the present invention is characterized by being by shrinking polysaccharide porous beads not less than 10% by a shrinkage rate defined by the following formula, and crosslinking the polysaccharide porous beads: Shrinkage rate (%)=(1−V2/V1)×100 (wherein, V1 indicates the gel volume of polysaccharide porous beads before shrinkage, and V2 indicates the gel volume of polysaccharide porous beads after shrinkage).
-
-