POLYETHYLENE YARN, METHOD FOR MANUFACTURING THE SAME, AND SKIN COOLING FABRIC COMPRISING THE SAME

    公开(公告)号:US20220205145A1

    公开(公告)日:2022-06-30

    申请号:US17602704

    申请日:2019-12-27

    IPC分类号: D02G3/44 D01D5/088 D01F6/04

    摘要: Disclosed is a polyethylene yarn capable of providing a user with a soft tactile sensation as well as a cooling feeling or a cooling sensation, and also having improved weavability that enables the manufacture of a skin cooling fabrics having excellent pilling resistance, abrasion resistance, cuttability, and sewability, a method for manufacturing the same, and a skin cooling fabric including the same. In a strength-elongation curve of the polyethylene yarn obtained by measuring at ambient temperature, (i) elongation at strength of 1 g/d is 0.5 to 3%, (ii) elongation at strength of 3 g/d is 5.5 to 10%, and (iii) a difference between elongation at strength of 4 g/d and elongation at maximum strength is 5.5 to 25%, and the polyethylene yarn has toughness of 55 to 120 J/m3 at ambient temperature.

    DRAWN POLYETHYLENE TEREPHTHALATE FIBER, PET TIRE CORD, AND TIRE COMPRISING THEREOF
    5.
    发明申请
    DRAWN POLYETHYLENE TEREPHTHALATE FIBER, PET TIRE CORD, AND TIRE COMPRISING THEREOF 审中-公开
    拉伸聚乙烯纤维,PET轮胎和包括其的轮胎

    公开(公告)号:US20140299246A1

    公开(公告)日:2014-10-09

    申请号:US14078047

    申请日:2013-11-12

    IPC分类号: C08G63/183 B60C9/00

    摘要: The present invention relates to a drawn PET fiber that can provide a cap ply cord and the like showing more improved modulus and good dimensional stability, a PET tire cord, and a tire including the same. The drawn PET fiber may be a fiber including 90 mol % or more of PET, of which the crystallinity is 53% or more, the amorphous orientation factor (AOF) is 0.15 or less, and the birefringence index is 0.14 to 0.16, after heat-treating the same at 230° C. for 1 minute under the initial load of 20g/1000d.