Fuel-barrier polyamide resin and multilayer shaped article
    1.
    发明授权
    Fuel-barrier polyamide resin and multilayer shaped article 有权
    燃料阻隔聚酰胺树脂和多层成型制品

    公开(公告)号:US07053172B2

    公开(公告)日:2006-05-30

    申请号:US10837699

    申请日:2004-05-04

    IPC分类号: C08G69/08 B32B27/00

    摘要: The fuel-barrier polyamide resin of the present invention is a product of the polycondensation of a diamine component comprising 70 mol % or higher of m-xylylenediamine and a dicarboxylic acid component comprising 70 mol % or higher of a mixed dicarboxylic acid which comprises a C4 to C20 α,ω-linear aliphatic dicarboxylic acid and at least one dicarboxylic acid selected from the group consisting of isophthalic acid and naphthalenedicarboxylic acid in a molar ratio of 30:70 to 95:5. The polyamide resin is excellent in not only fuel-barrier property and heat resistance, but also moldability and recyclability, and therefore suitably used as a barrier material of fuel containers.

    摘要翻译: 本发明的燃料阻隔性聚酰胺树脂是包含70摩尔%以上的间苯二甲胺的二胺成分和含有70摩尔%以上的混合二羧酸的二羧酸成分的缩聚物的产物,其包含C 4〜20%,ω-直链脂肪族二羧酸和选自间苯二甲酸和萘二甲酸的至少一种二羧酸,摩尔比为30: 70至95:5。 聚酰胺树脂不仅具有优异的燃料阻隔性和耐热性,而且还具有成型性和再循环性,因此适合用作燃料容器的阻隔材料。

    MULTI-LAYERED BOTTLE
    2.
    发明申请
    MULTI-LAYERED BOTTLE 有权
    多层瓶

    公开(公告)号:US20090120900A1

    公开(公告)日:2009-05-14

    申请号:US11994660

    申请日:2006-07-06

    IPC分类号: B65D90/02

    摘要: There is provided a multilayer bottle comprising a barrel portion including an outermost layer, an innermost layer and at least one barrier layer interposed between the outermost layer and the innermost layer, which satisfies the requirements represented by the following formulae (1) to (3) at the same time: OTR≦0.2 cc·mm/(m2·day·atm)  (1) where OTR represents an average oxygen transmission rate of the barrier layer of the barrel portion; 20≦(Average degree of orientation of barrier layer of barrel portion)≦45; and  (2) 0≦b/a≦100≦200  (3) where “a” represents an average thickness (μm) of the barrier layer of the barrel portion; and “b” represents an average thickness (μm) of the barrier layer of a bottom portion of the bottle. The multilayer bottle is free from delamination owing to impact upon dropping even when the bottle is formed with irregularities and bends and therefore exhibits a large freedom of design choice.

    摘要翻译: 提供了一种多层瓶,其包括筒状部分,其包括最外层,最内层和插入在最外层和最内层之间的至少一个阻挡层,其满足由下式(1)至(3)表示的要求, 同时:<?in-line-formula description =“In-line Formulas”end =“lead”?> OTR <= 0.2 cc.mm/(m2.day.atm)(1)<?in-line -formulae description =“In-line Formulas”end =“tail”?>其中OTR表示筒部分的阻挡层的平均氧气透过率; <?in-line-formula description =“在线公式”end =“lead”?> 20 <=(筒部阻挡层的平均取向度)<= 45; 和(2)<?in-line-formula description =“In-line Formulas”end =“tail”?> <?in-line-formula description =“In-line Formulas”end =“lead”?> 0 < = b / a <= 100 <= 200(3)<?in-line-formula description =“In-line Formulas”end =“tail”?>其中“a”表示阻挡层的平均厚度(mum) 的桶部分; “b”表示瓶的底部的阻挡层的平均厚度(mum)。 即使当瓶形成不规则和弯曲时,多层瓶也不会因为落下的冲击而脱层,因此表现出大的设计自由度。

    Multilayer Bottle
    3.
    发明申请
    Multilayer Bottle 有权
    多层瓶

    公开(公告)号:US20090277858A1

    公开(公告)日:2009-11-12

    申请号:US12158504

    申请日:2006-12-21

    IPC分类号: B65D23/00

    摘要: There is provided a multilayer bottle including an outermost layer and an innermost layer which are each made of a thermoplastic polyester resin, and at least one barrier layer interposed between the outermost layer and the innermost layer. The barrier layer contains at least two components including a polyamide obtained by polycondensing a diamine component containing m-xylylenediamine as a main component with a dicarboxylic acid component containing an α,ω-linear aliphatic dicarboxylic acid as a main component, and a thermoplastic resin having a lower molecular weight than that of the polyamide. The multilayer bottle hardly suffers from delamination upon impact or dropping and, therefore, is not required to have a shape with less irregularities or less bends for preventing the delamination, and further has a large freedom of design choice.

    摘要翻译: 提供了包括由热塑性聚酯树脂制成的最外层和最内层的多层瓶,以及插入在最外层和最内层之间的至少一个阻挡层。 阻挡层含有至少两种成分,包括通过将含有间苯二甲胺作为主要成分的二胺成分与含有α,ω-直链脂族二羧酸为主要成分的二羧酸成分缩聚得到的聚酰胺,以及具有 比聚酰胺低的分子量。 多层瓶几乎不会在冲击或滴落时发生分层,因此不需要具有较少的不规则形状或较少弯曲的形状以防止分层,并且还具有大的设计选择自由度。

    Multi-layered bottle
    4.
    发明授权
    Multi-layered bottle 有权
    多层瓶

    公开(公告)号:US08124204B2

    公开(公告)日:2012-02-28

    申请号:US11994660

    申请日:2006-07-06

    IPC分类号: B32B27/08 B32B27/34 B32B27/36

    摘要: There is provided a multilayer bottle comprising a barrel portion including an outermost layer, an innermost layer and at least one barrier layer interposed between the outermost layer and the innermost layer, which satisfies the requirements represented by the following formulae (1) to (3) at the same time: OTR≦0.2 cc·mm/(m2·day·atm)  (1) where OTR represents an average oxygen transmission rate of the barrier layer of the barrel portion; 20≦(Average degree of orientation of barrier layer of barrel portion)≦45; and  (2) 0≦b/a×100≦200  (3) where “a” represents an average thickness (μm) of the barrier layer of the barrel portion; and “b” represents an average thickness (μm) of the barrier layer of a bottom portion of the bottle. The multilayer bottle is free from delamination owing to impact upon dropping even when the bottle is formed with irregularities and bends and therefore exhibits a large freedom of design choice.

    摘要翻译: 提供了一种多层瓶,其包括筒状部分,其包括最外层,最内层和插入在最外层和最内层之间的至少一个阻挡层,其满足由下式(1)至(3)表示的要求, 同时:OTR&nlE; 0.2cc·mm /(m2·day·atm)(1)其中OTR表示筒部的阻挡层的平均氧气透过率; 20&nlE;(桶部分的阻挡层的平均取向度)&nlE; 45; 和(2)0&nlE; b / a×100&nlE; 200(3)其中“a”表示筒部的阻挡层的平均厚度(μm) “b”表示瓶的底部的阻挡层的平均厚度(μm)。 即使当瓶形成不规则和弯曲时,多层瓶也不会因为落下的冲击而脱层,因此表现出大的设计自由度。

    Multilayer bottle
    5.
    发明授权
    Multilayer bottle 有权
    多层瓶

    公开(公告)号:US07927678B2

    公开(公告)日:2011-04-19

    申请号:US12158504

    申请日:2006-12-21

    IPC分类号: B32B27/08

    摘要: There is provided a multilayer bottle including an outermost layer and an innermost layer which are each made of a thermoplastic polyester resin, and at least one barrier layer interposed between the outermost layer and the innermost layer. The barrier layer contains at least two components including a polyamide obtained by polycondensing a diamine component containing m-xylylenediamine as a main component with a dicarboxylic acid component containing an α,ω-linear aliphatic dicarboxylic acid as a main component, and a thermoplastic resin having a lower molecular weight than that of the polyamide. The multilayer bottle hardly suffers from delamination upon impact or dropping and, therefore, is not required to have a shape with less irregularities or less bends for preventing the delamination, and further has a large freedom of design choice.

    摘要翻译: 提供了包括由热塑性聚酯树脂制成的最外层和最内层的多层瓶,以及插入在最外层和最内层之间的至少一个阻挡层。 阻隔层含有至少两种成分,包括通过使含有间苯二甲胺作为主要成分的二胺组分与含有α,ω-线性脂族二羧酸作为主要成分的二羧酸组分缩聚获得的聚酰胺,以及具有 比聚酰胺低的分子量。 多层瓶几乎不会在冲击或滴落时发生分层,因此不需要具有较少的不规则形状或较少弯曲的形状以防止分层,并且还具有大的设计选择自由度。

    Fuel barrier thermoplastic resin composition and shaped article
    8.
    发明授权
    Fuel barrier thermoplastic resin composition and shaped article 有权
    燃料阻隔热塑性树脂组合物和成型制品

    公开(公告)号:US07323513B2

    公开(公告)日:2008-01-29

    申请号:US11017714

    申请日:2004-12-22

    IPC分类号: C08L77/04

    摘要: The thermoplastic resin composition of the invention comprises (A) 50 to 97% by weight of a polyolefin, (B) 2 to 45% by weight of a polyamide resin comprising a diamine component and a dicarboxylic acid component and (C) 1 to 45% by weight of a modified polyolefin and/or styrene copolymer. The polyamide resin is specified by that at least 70 mol % of the diamine component is a constitutional unit derived from m-xylylenediamine and at least 70 mol % of the dicarboxylic acid component is a constitutional unit derived from a C4-C20 straight-chain α,ω-aliphatic dicarboxylic acid and isophthalic acid in a molar ratio of 3:7 to 10:0. With such a chemical component, the thermoplastic resin composition exhibits excellent fuel barrier properties, heat resistance and moldability.