摘要:
The method for manufacturing a liquid crystal display device includes carrier film feeding steps including feeding long carrier films from continuous rolls, respectively; peeling steps including folding back each of the carrier films at a front end part placed on a carrier film feed path so that the optical films are peeled off from the carrier films, respectively; and bonding steps including bonding the optical films to the viewer side and back side of a liquid crystal panel, wherein in the bonding steps, the optical films are bonded to the liquid crystal panel in such a manner that the number of times the optical film is bonded to the back side of the liquid crystal panel is greater than the number of times the optical film is bonded to the viewer side of the liquid crystal panel.
摘要:
Provided are a liquid crystal panel which contributes to reduction in thickness and is excellent in optical properties and a liquid crystal display apparatus. The liquid crystal panel of the present invention includes a liquid crystal cell, a first polarizer disposed on one side of the liquid crystal cell, a second polarizer disposed on another side of the liquid crystal cell, a first optical compensation layer and a first negative C plate disposed between the first polarizer and the liquid crystal cell, and a second negative C plate and a second optical compensation layer disposed between the liquid crystal cell and the second polarizer, in which the first optical compensation layer is disposed between the first polarizer and the first negative C plate, the second optical compensation layer is disposed between the second negative C plate and the second polarizer, the first and second optical compensation layers each include a coating layer functioning as a λ/4 plate, and each have a thickness of 0.3 to 3 μm, and the first and second negative C plates each include a coating layer, and each have a thickness of 0.5 to 10 μm.
摘要:
A method of manufacturing a polarizer is provided that makes it possible to manufacture a polarizer prevented from curling even when a liquid is brought into contact with a hydrophilic polymer film by being sprayed. A method of manufacturing a polarizer includes a swelling step A for swelling a hydrophilic polymer film 1 by bringing it into contact with a swelling liquid 2, a dyeing step B for dyeing the hydrophilic polymer film 1 by bringing it into contact with a dye liquid 3 containing a dichroic material, and a crosslinking/stretching step C for crosslinking the hydrophilic polymer film 1 by bringing it into contact with a crosslinking liquid 4 and further stretching it. In the method, the contact with the swelling liquid in the swelling step A is carried out in the gas phase by spraying the swelling liquid 2 onto both surfaces of the hydrophilic polymer film 1.
摘要:
The present invention provides a method of producing an elliptically polarizing plate including the steps of: forming a first birefringent layer on a surface of a transparent protective film; laminating a polarizer on a surface of the transparent protective film; forming a second birefringent layer on a surface of the first birefringent layer; and forming a third birefringent layer on a surface of the second birefringent layer. The first birefringent layer is arranged on the opposite side against the polarizer with respect to the transparent protective film. The step of forming the first birefringent layer includes the steps of: applying a liquid crystal material onto a substrate subjected to an alignment treatment; treating the applied liquid crystal material, so as to form the first birefringent layer on the substrate; and transferring the first birefringent layer onto a surface of the transparent protective film.
摘要:
The present invention provides a method of producing an elliptically polarizing plate including the steps of: forming a first birefringent layer on a surface of a transparent protective film; laminating a polarizer on a surface of the transparent protective film; forming a second birefringent layer on a surface of the first birefringent layer; and forming a third birefringent layer on a surface of the second birefringent layer. The first birefringent layer is arranged on the opposite side against the polarizer with respect to the transparent protective film. The step of forming the first birefringent layer includes the steps of: applying a liquid crystal material onto a substrate subjected to an alignment treatment; treating the applied liquid crystal material, so as to form the first birefringent layer on the substrate; and transferring the first birefringent layer onto a surface of the transparent protective film.
摘要:
A method of manufacturing a polarizer is provided that makes it possible to virtually simultaneously perform a contact of a hydrophilic polymer film with liquid and stretch of the hydrophilic polymer film in a width direction by a tenter method, or the like, using a small and simple manufacturing equipment. A method of manufacturing a polarizer includes a width direction stretching process for stretching a hydrophilic polymer film 1 in the width direction, which is continuously supplied, by gripping both ends in a width direction thereof with grip means 2 and moving the grip means 2 in a longitudinal direction of the film 1 as well as by bringing the film 1 into contact with liquid and also moving the grip means 2, which grips at least one of both ends in the width direction of the film 1, outwardly in the width direction of the film 1; and a dyeing process for dyeing the film 1 by a dichroic material. In the width direction stretching process, a contact with the liquid is carried out by at least one of spraying and coating of the liquid, and the width direction stretching process is carried out in at least one of the dyeing process and a process other than the dyeing process.
摘要:
A method of manufacturing a polarizer is provided that makes it possible to manufacture a polarizer prevented from curling even when a liquid is brought into contact with a hydrophilic polymer film by being sprayed. A method of manufacturing a polarizer includes a swelling step A for swelling a hydrophilic polymer film 1 by bringing it into contact with a swelling liquid 2, a dyeing step B for dyeing the hydrophilic polymer film 1 by bringing it into contact with a dye liquid 3 containing a dichroic material, and a crosslinking/stretching step C for crosslinking the hydrophilic polymer film 1 by bringing it into contact with a crosslinking liquid 4 and further stretching it. In the method, the contact with the swelling liquid in the swelling step A is carried out in the gas phase by spraying the swelling liquid 2 onto both surfaces of the hydrophilic polymer film 1.
摘要:
Provided are an elliptically polarizing plate that is excellent in contrast in an oblique direction and has a broadband and a wide viewing angle, and an image display device using the elliptically polarizing plate. The elliptically polarizing plate of the present invention includes in order: a polarizer; a protective layer; a first birefringent layer having a refractive index profile of nz>nx=ny; a second birefringent layer that functions as a λ/2 plate; and a third birefringent layer that functions as a λ/4 plate. A ratio Rth1/Rthp between an absolute value Rthp of a thickness direction retardation of the protective layer and an absolute value Rth1 of a thickness direction retardation of the first birefringent layer is preferably in a range of 1.1 to 4.
摘要:
Provided are a liquid crystal panel and a liquid crystal display apparatus each of which: contributes to a reduction in thickness; and is excellent in optical characteristics, and a method of producing the liquid crystal panel with extremely high production efficiency. A liquid crystal panel of the present invention has a first polarizer, a first protective layer, a first optical compensation layer, a first negative C plate, a liquid crystal cell, a second negative C plate, a second optical compensation layer, a second protective layer, and a second polarizer in the stated order. The first optical compensation layer is arranged between the first protective layer and the first negative C plate to be in close contact with the first protective layer without using any adhesive. The second optical compensation layer is arranged between the second negative C plate and the second protective layer to be in close contact with the second protective layer without using any adhesive. The first and second optical compensation layers are each a coating layer functioning as a λ/4 plate, and each have a thickness of 0.3 to 3 μm. The first and second negative C plates are each a coating layer, and each have a thickness of 0.5 to 10 μm.
摘要:
This invention provides a method for producing an optical film, the method comprising a rubbing treatment step of rubbing the surface of a lengthy plastic film F with a rubbing roll 4 obtained by winding a raised fabric 4a, an application step of applying a liquid crystalline molecule to the surface of the plastic film processed through said rubbing treatment step and a fixing step of fixing said applied liquid crystalline molecule. In the rubbing treatment step, the lengthy plastic film is supported and conveyed by a conveyer belt 3 having a metal surface, and plural backup rolls 5 which support the underside of the conveyer belt supporting the plastic film are disposed opposite to said rubbing roll, to set a rubbing strength RS defined by the following equation (1) to 2600 mm or more (more preferably 3400 mm or more).