摘要:
There is provided an oxide dispersion-strengthened nickel alloy which has a hot working property, a structure stability at high temperature, improved creep characteristics at high temperature and improved heat resistant fatigue characteristics. The oxide dispersion-strengthened alloy is composed of an oxide containing one or more kinds of elements in an amount of 2 wt % or less selected from the group composed of titanium, zirconium and hafnium, chromium in an amount of 15-35 wt %, carbon in an amount of 0.01-0.4 wt % and Y.sub.2 O.sub.3 in an amount of 0.3-2.0 wt %, and the balance of substantially nickel, wherein Y.sub.2 O.sub.3 is dispersed as particles in the matrix of the nickel alloy containing one or more kinds of elements selected from the group composed of titanium, zirconium and hafnium, chromium and carbon. The elements of equipment such as the nozzle guide vane of a gas turbine, the liner and transition piece of a combustor, and the like are composed of the oxide dispersion-strengthened alloy of the present invention so that they can be used at high temperature.
摘要翻译:提供了具有热加工性,高温结构稳定性,高温下蠕变特性提高,耐热疲劳特性提高的氧化物分散强化镍合金。 氧化物分散强化合金由含有选自钛,锆和铪组成的组中的2重量%以下的1种以上的元素的氧化物,15〜35重量%的铬, 0.01-0.4重量%的碳和0.3-2.0重量%的Y 2 O 3,余量基本上为镍,其中Y 2 O 3作为颗粒分散在含有选择的一种或多种元素的镍合金基质中 由钛,锆和铪组成的组,铬和碳组成。 燃气轮机的喷嘴引导叶片,燃烧器的衬套和过渡件等设备的元件由本发明的氧化物分散强化合金构成,从而可以在高温下使用。
摘要:
A high-temperature member for use in a gas turbine, the member being formed from a new wear-resistant alloy having good wear resistance as well as good ductility, is disclosed. The member was developed to prevent wear and damage that occur due to vibration while the turbine is running. The high-temperature member for use in a gas turbine is formed from a new cobalt-based wear-resistant alloy which is composed of a cobalt-chromium matrix and refractory metals, with the content of hard particles (such as carbide) reduced. The refractory metals promote work hardening, thereby improving wear resistance. The reduced content of hard particles contributes to good ductility.
摘要:
A high-temperature member for use in a gas turbine is formed from a cobalt-based alloy comprising 15-35 wt % of chromium; 0.02-1.5 wt % of silicon; 0.01-0.2 wt % of carbon; at least one kind of metal selected from the group consisting of niobium, tungsten, tantalum and rhenium, the total content of these four metals being controlled not to exceed 10% by atomic ratio of the entirety of the alloy excluding carbon; and at least one metal selected from the group consisting of nickel, manganese and iron, the total content of these metals being within a range of 1-9 wt %, the total content of nickel being controlled not to exceed 5 wt %, and the cobalt-based alloy having both of excellent resistance due to work hardening of the matrix and excellent ductility under room temperature. Then, in order to improve the high-temperature wear resistance, a pre-hardened layer is formed in the surface portion of the member by shot peening
摘要:
A water atomized Fe powder for a magnetic compact reduced in deformation resistance during molding and annealing temperature for removing strains is provided. A compact having improved magnetic properties is also provided. The water atomized powder containing at least one element selected from Nb, Ta, Ti, Zr and V in an amount of 0.001-0.03 atom % is soft magnetic and has a precipitation in the matrix, which is composed of at least one element selected from Nb, Ta, Ti, Zr and V and oxygen as a main component and has an average size of 0.02-0.5 μm. Disclosed is a method for manufacturing a soft magnetic powder includes adding at least one element selected from Nb, Ta, Ti, Zr and V, and annealing in a hydrogen-containing reduction atmosphere. This method decrease gaseous impurities, particularly oxygen, and defuse it, to improve the magnetic properties of the powder and compact.