摘要:
A polybutylene naphthalate-based resin composition contains, relative to (A) 100 parts by wt of polybutylene naphthalate resin, (B) 40-150 parts by wt of polyester block copolymer, (C) 0.5-5 parts by wt of hydrolysis retarder, and (D) 0.5-5 parts by wt of inorganic multiporous filler.
摘要:
There are provided a polybutylene naphthalate-based resin composition containing polybutylene naphthalate resin, a polyester block copolymer, and magnesium hydroxide; and an electric wire using a polybutylene naphthalate-based resin composition, with an insulated coating layer formed on a conductor, by using a polybutylene naphthalate-based resin composition containing polybutylene naphthalate resin, a polyester block copolymer, and magnesium hydroxide as an insulating material.
摘要:
An insulated conductor includes a conductor, and an insulation covering the conductor and formed of a resin composition. The resin composition includes more than 60% by weight of polybutylene naphthalate resin. The resin composition further includes a hydrogenated block copolymer that a block copolymer including a styrene and a diene system compound is saturated by hydrogenation, and at least one of a polyolefin and a compound including a glycidyl group. A method for manufacturing the insulated conductor includes forming on the conductor the insulation including the resin composition by extrusion in a range of 290° C. to 310° C.
摘要:
An insulated wire uses a resin composition. The insulated wire includes a conductor; and an insulating material provided on the conductor, the insulating material includes a polyester resin in 100 parts by weight, a non-bromine flame retardant agent in 1-30 parts by weight, a polyorganosiloxane core-graft copolymer in 1-50 parts by weight, an inorganic porous filler in 0.1-50 parts by weight; and a hydrolysis resistance modifier in 0.05-10 parts by weight.
摘要:
A halogen-free flame-retardant resin composition includes 100 parts by, weight of base polymer of polyolefin resin, not less than 50 parts by weight and not more than 250 parts by weight of metal hydroxide, not less than 1 part by weight and not more than 50 parts by weight of calcium borate, not less than 1 part by weight and not more than 50 parts by weight of zinc stannate, and less than 30 seconds of burning time after removal of flame in a vertical flame test complying with CODE 895 OR 3rd edition, appendix 6 of the UIC standard.
摘要:
An exemplary method for producing a catalyst is provided where the catalyst includes a catalyst support on which a metallic compound is loaded. An impurity content of the catalyst can be in a range of approximately 0.01 mass % to 0.15 mass %. In particular, the exemplary method can include pre-treating the catalyst support to lower an impurity concentration of the catalyst support, and loading the metallic compound on the catalyst support after the pretreatment procedure.