Described are articles having an aminoplast resin photochromic coating prepared from an aminoplast resin, components(s) having hydroxyl functional groups and photochromic substances. The coatings exhibit a Fischer microhardness of from 45 to 180 Newtons per mm2 and desirable photochromic properties, i.e., the formation of darker activated colors and faster rates of photochromic activation and fade when irradiated with ultraviolet light. Also described are photochromic aminoplast resin articles.
摘要翻译:描述了具有由氨基塑料树脂,具有羟基官能团的组分和光致变色物质制备的氨基塑料树脂光致变色涂层的制品。 涂层表现出45至180牛顿/ mm 2的菲舍尔显微硬度和所需的光致变色性质,即形成更暗的活化颜色和较快的光致变色激活速率和用紫外线照射时的褪色。 还描述了光致变色氨基塑料树脂制品。
摘要:
Described are articles having an aminoplast resin photochromic coating prepared from an aminoplast resin, component(s) having at least two different functional groups and photochromic substances. The coatings exhibit a Fischer microhardness of from 45 to 180 Newtons per mm2 and desirable photochromic properties, i.e., the formation of darker activated colors and faster rates of photochromic activation and fade when irradiated with ultraviolet light. Also described are photochromic aminoplast resin articles.
摘要翻译:描述了具有由氨基塑料树脂,具有至少两个不同官能团的组分和光致变色物质制备的氨基塑料树脂光致变色涂层的制品。 涂层表现出45至180牛顿/ mm 2的菲舍尔显微硬度和所需的光致变色性质,即形成更暗的活化颜色和较快的光致变色激活速率和用紫外线照射时的褪色。 还描述了光致变色氨基塑料树脂制品。
摘要:
Described are articles having a polyanhydride photochromic coating. The coatings exhibit a Fischer microhardness of from 50 to 130 Newtons per mm2 and desirable photochromic properties, i.e., the formation of darker activated colors and faster rates of photochromic activation and fade when irradiated with ultraviolet light. Also described are polyanhydride photochromic articles.
摘要翻译:描述了具有聚酐光致变色涂层的制品。 涂层表现出的Fischer显微硬度为50至130牛顿/ mm 2,并且具有所需的光致变色性质,即形成更暗的活化颜色,并且当用紫外光照射时,光致变色激活速率和较快的速度。 还描述了聚酐光致变色制品。
摘要:
Described are photochromic epoxy resin coatings that meet commercially acceptable “cosmetic” standards for optical coatings. Also described are articles having such coatings. The coatings exhibit a Fischer microhardness of from 50 to 150 Newtons per mm2 and desirable photochromic properties, i.e., the formation of darker activated colors and faster rates of photochromic activation and fade when irradiated with ultraviolet light.
摘要:
Described are articles having an alkoxyacrylamide photochromic coating. The coatings exhibit a Fischer microhardness of from 50 to 130 Newtons per mm.sup.2 and desirable photochromic properties, i.e., the formation of darker activated colors and faster rates of photochromic activation and fade when irradiated with ultraviolet light. Also described are alkoxyacrylamide photochromic articles.
摘要翻译:描述了具有烷氧基丙烯酰胺光致变色涂层的制品。 涂层表现出的Fischer显微硬度为50至130牛顿/ mm 2,并且具有期望的光致变色性质,即形成更暗的活化颜色,并且当用紫外光照射时,光致变色活化速度更快,而且褪色。 还描述了烷氧基丙烯酰胺光致变色制品。
摘要:
Described is a polymerizable composition of a photochromic amount of at least one photochromic compound, at least one material having at least one carbonate group and at least one hydroxyl group, and at least one monoisocyanate containing material having at least one unsaturated group. The polymerizable composition optionally contains copolymerizable monomers. Also described are photochromic polymerizates, e.g., photochromic optical elements such as ophthalmic lenses, prepared from the polymerizable composition of the present invention.
摘要:
Described is a photochromic article that includes a substrate and at least a partial coating of an at least partially cured polymerizable composition of a photochromic amount of at least one photochromic compound, at least one material having at least one carbonate group and at least one hydroxyl group, and at least one monoisocyanate containing material having at least one unsaturated group. Also described are photochromic optical elements such as ophthalmic lenses, prepared from an optical element substrate coated with the photochromic polymerizable composition.
摘要:
Photochromic optical articles of improved resistance to light fatigue are provided by the use of a combination of hindered amine light stabilizer and asymmetric diaryloxalamide light stabilizer with a mixture of (1) photochromic material having a minima luminous transmission in the range of 560 to 630 nanometers and (2) photochromic material having a minima luminous transmission in the range of 430 to 520 nanometers.
摘要:
A process for incorporating by thermal diffusion a photochromic substance into a synthetic organic host material is described. In the process, a surface of the host material containing a coating of a resin composition of from about 5 to about 50 parts of hydroxy (C.sub.2 -C.sub.3) alkyl cellulose, e.g., hydroxy propyl cellulose, and from about 95 to about 50 parts of poly(vinylpyrrolidone), which resin composition contains a photochromic substance, is heated to diffuse at least a portion of the photochromic substance into the surface of the host material. Subsequently, the coating is removed by washing with warm soapy water. In a particular embodiment, the host material is a polymer prepared from diethylene glycol bis(allyl carbonate).
摘要:
Described is a method for imparting a photochromic response to a synthetic plastic article, e.g., an optical lens such as a sunglass lens prepared from an allyl diglycol carbonate monomer. The method described comprises depositing a thin uniform substantially dry film of a photochromic-bearing polymeric resin onto at least one planar surface of the synthetic plastic material, heating the plastic article and resin film substantially uniformly at temperatures near to but below the melting temperature of the photochromic substance for a time sufficient to transfer a photochromic amount of the photochromic material into the subsurface region of the plastic article, and thereafter removing the photochromic-lean resin film from the planar surface(s) of the plastic article.