摘要:
A thin magnetic element comprising a coil pattern formed on at least one side of a substrate and a thin magnetic film formed on the coil pattern, wherein, assuming that the thickness and width of a coil conductor constituting the coil pattern are t and a, respectively, an aspect ratio t/a of the coil conductor satisfies the relationship 0.035≦t/a≦0.35, and the thin magnetic film has a resistivity of 400 &mgr;&OHgr;cm or more.
摘要翻译:一种薄磁性元件,包括形成在衬底的至少一侧的线圈图案和形成在线圈图案上的薄磁膜,其中,假定构成线圈图案的线圈导体的厚度和宽度分别为t和a ,线圈导体的纵横比t / a满足关系0.035 <= t / a <= 0.35,薄磁膜的电阻率为400μΩEG·cm以上。
摘要:
A thin magnetic element which comprises a coil pattern formed on at least one side of a substrate and a thin magnetic film formed on the coil pattern, wherein:said thin magnetic film is for++med to a thickness of 0.5 .mu.m or greater but 8 .mu.m or smaller;and at least one of the following conditions, that is, assuming that the thickness and width of a coil conductor constituting the coil pattern are t and a, respectively, an aspect ratio t/a of the coil conductor satisfies the following relationship: 0.035.ltoreq.t/a.ltoreq.0.35;and assuming that the width of the conductor constituting the coil pattern is a and the distance between the mutually adjacent coil conductors in the coil pattern is b, the following relationship: 0.2.ltoreq.a/(a+b) is satisfied.
摘要:
A method for making a Fe-based soft magnetic alloy where an alloy melt is injected onto a moving cooling unit to form an amorphous alloy ribbon. The alloy melt contains Fe as a main component, B and at least one metallic element M selected from the group consisting of Ti, Zr, Hf, V, Nb, Ta, Mo and W, the composition of the alloy melt being selected such that the resulting amorphous alloy ribbon is characterized by a first crystallization temperature at which fine grain bcc Fe crystallites precipitate, and a second crystallization temperature at which a compound phase containing Fe--B and/or Fe--M precipitates. The amorphous alloy ribbon is then annealed at a temperature which is higher that the first crystallization temperature and less than the second crystallization temperature for an annealing time in the range of 0 minutes to 20 minutes.
摘要:
A soft magnetic alloy used as a radio frequency magnetic material and having high resistivity and high magnetic permeability in a high frequency band, and an inductor, a wave absorber and antenna each comprising the soft magnetic alloy. The soft magnetic alloy has a crystal phase containing Co as a main component and at least one element T selected as a primary component from Fe, Ni, Pd, Mn and Al, and having a face-centered cubic structure, a body-centered cubic structure or a mixture thereof having an average crystal grain size of 30 nm or less; and a ferromagnetic amorphous phase surrounding the crystal phase and containing at least one element M selected from Ti, Zr, Hf, Nb, Ta, Mo, W, Y and rare earth elements, O, N, C, B, at least one oxide of element M, Fe and element T.
摘要:
A hard magnetic alloy in accordance with the present invention is composed of at least element T selected from the group consisting of Fe, Co and Ni, at least one rare earth element R, and boron (B). The hard magnetic alloy has an absolute value of the temperature coefficient of magnetization of 0.15%/° C. or less and a coercive force of 1 kOe, when being used in a shape causing a permeance factor of 2 or more. A hard magnetic alloy compact in accordance with the present invention has a texture, in which at least a part or all of the texture comprises an amorphous phase or fine crystalline phase having an average crystal grain size of 100 nm or less, is subjected to crystallization or grain growth under stress, such that a mixed phase composed of a soft magnetic or semi-hard magnetic phase and a hard magnetic phase is formed in the texture, and anisotropy is imparted to the crystal axis of the hard magnetic phase.
摘要:
In a magnetic film forming method, a plurality of chips formed of Fe.sub.3 O.sub.4 and a plurality of chips formed of HfO.sub.2 are disposed on a target formed of Fe. The composition ratio of a Fe--Hf--O film can be set within a proper range by adjusting the numbers of the up said two kind of chips.
摘要翻译:在磁性膜形成方法中,由Fe 3 O 4形成的多个芯片和由HfO 2形成的多个芯片设置在由Fe形成的靶上。 通过调整上述两种芯片的数量,可以将Fe-Hf-O膜的组成比设定在适当的范围内。
摘要:
In a stepping motor having a stator provided with an electromagnet and a rotor composed of a hard magnetic alloy, the hard magnetic alloy comprises at least one element T of Fe and Co, at least one element R of rare earth elements and B, has a remanence ratio of at least 0.7, remanent magnetization (Ir) of at least 120 emu/g and coercive force (iHc) of at least 1 kOe and includes a fine crystalline phase having an average crystal grain size of 100 nm or less as a main phase. The hard magnetic alloy is solidified and compacted by making use of a softening phenomenon which arises when the amorphous phase contained in the structure of the hard magnetic alloy is crystallized. A method of manufacturing the hard magnetic alloy used to the stepping motor is also disclosed.
摘要:
A hard magnetic alloy in accordance with the present invention is composed of at least element T selected from the group consisting of Fe, Co and Ni, at least one rare earth element R, and boron (B). The hard magnetic alloy has an absolute value of the temperature coefficient of magnetization of 0.15%/° C. or less and a coercive force of 1 kOe, when being used in a shape causing a permeance factor of 2 or more. A hard magnetic alloy compact in accordance with the present invention has a texture, in which at least a part or all of the texture comprises an amorphous phase or fine crystalline phase having an average crystal grain size of 100 nm or less, is subjected to crystallization or grain growth under stress, such that a mixed phase composed of a soft magnetic or semi-hard magnetic phase and a hard magnetic phase is formed in the texture, and anisotropy is imparted to the crystal axis of the hard magnetic phase.
摘要:
A thin film magnetic head includes an upper core layer and a lower core layer which are made of an Fe—M—O alloy, an Fe—M—T—O alloy or an NI—Fe—X alloy so that the upper core layer has a high saturation magnetic flux density, low coercive force and high resistivity, and the lower core layer has a lower saturation magnetic flux density than the upper core layer, low coercive force, high resistivity, and a low magnetostriction constant. Also the lower core layer is formed so that the thickness gradually decreases toward both side ends, and a gap layer can be formed on the lower core layer to have a uniform thickness. Since the lower core layer is formed by sputtering, a material having excellent soft magnetic material can be used, thereby enabling recording at high frequency.
摘要:
A hard magnetic material contains Co as a main component, at least one element Q of P, C, Si and B, and Sm, and an amorphous phase and a fine crystalline phase. The texture of the hard magnetic material contains 50% by volume or more of fine crystalline phase having an average crystal grain size of 100 nm or less, and has a mixed phase state containing a soft magnetic phase and a hard magnetic phase. Further, anisotropy is imparted to the crystal axis of the hard magnetic phase.