Process for preparing polymer by using copper compound
    1.
    发明授权
    Process for preparing polymer by using copper compound 失效
    使用铜化合物制备聚合物的方法

    公开(公告)号:US06433130B1

    公开(公告)日:2002-08-13

    申请号:US09780340

    申请日:2001-02-12

    IPC分类号: C08F608

    摘要: The present inventors has its objects to provide a polymerization catalyst component, a copper compound which can easily be synthesized and is stable. The present invention is related to a method of producing a polymer which comprises using a copper compound represented by the general formula CuXn, LCuXn or L(L′)CnXn (wherein L and L′ each represents a ligand, X represents a halogen atom or an alkoxy, thioxy, allyloxy, amino, secondary amino, tertiary amino, cyano, nitro, alkyl or allyl group, and n represents an integer of 0 to 2) as a catalyst and/or polymerization initiator in polymerizing a vinyl monomer whose polarity value e, when expressed in terms of absolute value, is not more than 1.5.

    摘要翻译: 本发明人的目的是提供一种聚合催化剂组分,一种易于合成和稳定的铜化合物。本发明涉及一种制备聚合物的方法,该方法包括使用由通式CuXn表示的铜化合物, LCuXn或L(L')CnXn(其中L和L'各自表示配体,X表示卤素原子或烷氧基,硫代羟基,烯丙氧基,氨基,仲氨基,叔氨基,氰基,硝基,烷基或烯丙基, n表示0〜2的整数)作为催化剂的聚合引发剂和/或聚合引发剂,其极性值e以绝对值表示时不超过1.5。

    Expandable polyolefin resin compositions
    2.
    发明授权
    Expandable polyolefin resin compositions 失效
    可发性聚烯烃树脂组合物

    公开(公告)号:US5304580A

    公开(公告)日:1994-04-19

    申请号:US903585

    申请日:1992-06-25

    摘要: The invention provides an expandable polyolefin resin composition comprising (a) 40 to 100 wt. % of a polypropylene resin having a melt index of 0.5 to 12, (b) 0 to 60 wt. % of a polyethylene resin having a melt index of 2 to 50 (c) 0.5 to 10 parts by weight of the di(meth)acrylate of an aliphatic dihydric alcohol having a methylene group with 2 to 18 carbon atoms between the (meth)acryloyloxy groups at both ends per 100 parts by weight of the combination of the resins (a) and (b), and (d) 1 to 50 parts by weight of a thermally decomposable blowing agent. Preferably the composition further comprises (e) 0.5 to 5 parts by weight of a monofunctional monomer. When uniformly crosslinked, the composition affords an expandable polyolefin resin composition suited to production of a crosslinked polyolefin resin foam excellent in heat resistance, toughness and moldability of formability and appearing homogeneous.

    摘要翻译: 本发明提供一种可发性聚烯烃树脂组合物,其包含(a)40至100wt。 熔体指数为0.5〜12的聚丙烯树脂的%,(b)0〜60重量% 熔融指数为2〜50(c)的聚乙烯树脂的%(c)在(甲基)丙烯酰氧基(甲基)丙烯酰氧基中具有2〜18个碳原子的亚甲基的脂肪族二元醇的二(甲基)丙烯酸酯0.5〜10重量份 (a)和(b)的组合相对于100重量份的两端,和(d)1〜50重量份的热分解发泡剂。 优选地,组合物还包含(e)0.5至5重量份的单官能单体。 当均匀交联时,该组合物提供了适用于生产耐热性,韧性和成型性优异且呈均匀的交联聚烯烃树脂发泡体的可发性聚烯烃树脂组合物。

    Plastic foam material composed of a polyolefin based resin composition
and method for making same
    3.
    发明授权
    Plastic foam material composed of a polyolefin based resin composition and method for making same 失效
    由聚烯烃类树脂组合物构成的塑料泡沫材料及其制造方法

    公开(公告)号:US5543438A

    公开(公告)日:1996-08-06

    申请号:US316566

    申请日:1994-09-30

    摘要: A plastic foam material composed of a polyolefin based resin composition, consists essentially of specified amounts of polypropylene based resins and polyethylene based resins, included from about 20 to about 65 weight percent of a cross linked portion. The cross linked portion consists of from about 55 to about 95 weight percent of a cross linked polypropylene and from about 5 to about 45 weight percent of cross linked polyethylene. The amount of cross-linkage can be determined by a xylene extraction technique. The plastic foam material may further include specified amounts of a cross-linking agent and specified amounts of an organic thermodecomposition foaming agent. The thermodecomposition foaming agent decomposes at sufficiently high temperatures to yield a plastic foam material, which exhibits superior adherence properties and fewer deformities of its surface exemplified by swelling, shrinkage and wrinkling of its surface. A method to produce the plastic foam material is also disclosed.

    摘要翻译: 由聚烯烃基树脂组合物组成的塑料泡沫材料基本上由特定量的聚丙烯基树脂和聚乙烯基树脂组成,包括约20至约65重量%的交联部分。 交联部分由约55至约95重量%的交联聚丙烯和约5至约45重量%的交联聚乙烯组成。 交联量可以通过二甲苯萃取技术测定。 塑料泡沫材料还可以包括指定量的交联剂和指定量的有机热分解发泡剂。 热分解发泡剂在足够高的温度下分解以产生塑料泡沫材料,其表现出优异的粘附性能和较少的表面形状,例如其表面的膨胀,收缩和起皱。 还公开了一种生产塑料泡沫材料的方法。

    Process for preparing impact-resistant polyamides
    5.
    发明授权
    Process for preparing impact-resistant polyamides 失效
    制备耐冲击聚酰胺的方法

    公开(公告)号:US4490520A

    公开(公告)日:1984-12-25

    申请号:US469579

    申请日:1983-02-24

    IPC分类号: C08G69/00 C08G69/18 C08G69/20

    CPC分类号: C08G69/20 C08G69/18

    摘要: A process for preparing polyamides having improved impact strength and elongation comprising polymerizing an -lactam in the presence of (1) an alkali catalyst and (2) the reaction product of (a) a polyfunctional co-catalyst such as a polyisocyanate and (b) a polyoxyalkalene amine. The polyamides of the present invention are particularly useful for making strong tough molded or cast articles.

    摘要翻译: 一种制备具有改善的冲击强度和伸长率的聚酰胺的方法,包括在(1)碱催化剂存在下聚合内酯,和(2)多官能助催化剂如多异氰酸酯和(b)的反应产物, 聚氧化烯胺。 本发明的聚酰胺特别可用于制造强韧的模制或铸造制品。